# US 2016/0145148 A1 · Glass body for pressure forming and method for manufacturing the same, and microfabricated glass body and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0145148 A1
- Document ID: US20160145148A1
- Status: Published application
- Kind: A1
- Application number: 15/013,287
- Filed: 2016-02-02
- Published: 2016-05-26
- Earliest claimed: 2013-08-29
- Assignees: Kobe University; Asahi Glass Company, Limited
- Applicants: Kobe University; Asahi Glass Company, Limited
- Inventors: Kenji IMAKITA; Minoru FUJII; Kenji KITAOKA
- Web page: https://patentgrep.com/patent/US20160145148A1

## CPC

- C03C 11/005: {obtained by leaching after a phase separation step}
- C03B 23/02: Re-forming glass sheets
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 23/00: Other surface treatment of glass not in the form of fibres or filaments
- C03B 2215/41: Profiled surfaces
- C03B 2215/414: Arrays of products, e.g. lenses
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

Provided are a glass body for pressure forming enabling press forming in a low-temperature range without the need of a special mold material, and a method for manufacturing the same. A glass body for pressure forming 1 having a porosified layer 1b formed by porosifying a surface thereof and having a Vickers hardness of 85 N/mm2 or less on the porosified surface. The porosified layer 1b can be manufactured by phase-separating the glass body by spinodal decomposition, acid-treating the phase-separated glass body and then treating the acid-treated glass body with alkali or hot water to porosify the surface of the glass body.

## Claims

### Claim 1

A glass body for pressure forming having a porosified surface, the glass body having a Vickers hardness of 85 N/mm2 or less on the porosified surface.

### Claim 2 (depends on 1)

The glass body for pressure forming according to claim 1,
wherein a depth of a layer of the porosified surface is 1 μm or more.

### Claim 3 (depends on 1)

The glass body for pressure forming according to claim 1,
wherein a shape of the glass body is a plate shape.

### Claim 4 (depends on 1)

The glass body for pressure forming according to claim 1,
wherein a transmittance at a wavelength of 400 nm to 800 nm of the glass body is 80% or more.

### Claim 5

A method for manufacturing a glass body for pressure forming, comprising:
phase-separating the glass material by spinodal decomposition; and
porosifying a surface of the glass material by acid-treating the phase-separated glass material and then treating the acid-treated glass material with alkali or hot water.

### Claim 6 (depends on 5)

The method for manufacturing a glass body for pressure forming according to claim 5,
wherein after the acid treatment, the alkali treatment is performed, and thereafter the hot water treatment is performed.

### Claim 7 (depends on 1)

A microfabricated glass body having a desired projecting and recessed shape formed by press-processing a surface of the glass body for pressure forming according to claim 1.

### Claim 8 (depends on 7)

The microfabricated glass body according to claim 7,
wherein a line width or one side of the projecting and recessed shape is 0.1 to 100 μm.

### Claim 9 (depends on 7)

The microfabricated glass body according to claim 7,
wherein the projecting and recessed shape formed on a surface of the microfabricated glass body has an optical function.

### Claim 10 (depends on 7)

The microfabricated glass body according to claim 7,
wherein the projecting and recessed shape formed on a surface of the microfabricated glass body has a physical function.

### Claim 11

A method for manufacturing a microfabricated glass body, comprising:
phase-separating a glass material by spinodal decomposition;
porosifying a surface of the glass material by acid-treating the phase-separated glass material and then treating the acid-treated glass material with alkali or hot water; and
pressing the porosified glass material by a forming die to transfer a projecting and recessed shape.

### Claim 12 (depends on 11)

The method for manufacturing a microfabricated glass body according to claim 11,
wherein a line width or one side of the projecting and recessed shape is 0.1 to 100 μm.

### Claim 13 (depends on 11)

The method for manufacturing a microfabricated glass body according to claim 11,
wherein the press of the porosified glass is performed at a temperature equal to or lower than a glass transition point (Tg) of the glass material.