# US 2016/0145104 A1 · Method for making lithium iron phosphate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0145104 A1
- Document ID: US20160145104A1
- Status: Published application
- Kind: A1
- Application number: 15/011,637
- Filed: 2016-01-31
- Published: 2016-05-26
- Earliest claimed: 2013-08-15
- Assignees: Jiangsu Huadong Institute of Li-Ion Battery Co., Ltd.; Tsinghua University
- Applicants: Jiangsu Huadong Institute of Li-ion Battery Co. Ltd.; Tsinghua University
- Inventors: XIANG-MING HE; LI WANG; FEI-FEI GAO; ZHONG-JIA DAI; XIAN-KUN HUANG; JI-XIAN WANG
- Web page: https://patentgrep.com/patent/US20160145104A1

## CPC

- C01B 25/45: containing plural metal, or metal and ammonium
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for making a lithium iron phosphate suitable for use as a cathode active material comprises providing a lithium ion source solution and an iron phosphate, the lithium ion source solution comprising an organic solvent and a lithium chemical compound dissolved in the organic solvent. The lithium ion source solution and the iron phosphate are mixed and the mixture heated at a first temperature under a normal pressure to form a precursor solution, the first temperature being in a range from about 40° C. to about 90° C. The precursor solution is placed in a solvothermal reaction reactor and heated at a second temperature to form the lithium iron phosphate particles, the second temperature being higher than the first temperature.

## Claims

### Claim 1

A method for making a lithium iron phosphate comprising:
providing a lithium ion source solution and an iron phosphate, wherein the lithium ion source solution comprises an organic solvent and a lithium chemical compound dissolved in the organic solvent;
mixing the lithium ion source solution and the iron phosphate to form a mixture;
heating the mixture at a first temperature under a normal pressure to form a precursor solution, wherein the first temperature is in a range from about 40° C. to about 90° C.; and
placing the precursor solution in a solvothermal reaction reactor and heating the precursor solution at a second temperature to form the lithium iron phosphate, wherein the second temperature is higher than the first temperature.

### Claim 2 (depends on 1)

The method of claim 1, further comprising a step of stirring the precursor solution after placing the precursor solution in the solvothermal reaction reactor.

### Claim 3 (depends on 2)

The method of claim 2, wherein a stirring velocity is in a range from about 30 revolutions per minute to about 100 revolutions per minute.

### Claim 4 (depends on 1)

The method of claim 1, wherein the organic solvent is a diol solvent, polyol solvent or polymer polyol solvent.

### Claim 5 (depends on 4)

The method of claim 4, wherein the organic solvent is selected from ethylene glycol, glycerol, diethylene glycol, triethylene glycol, tetraethylene glycol, 1,2,4-butanetriol (C4H10O3), polyethylene glycol, and any combination thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein a total concentration of the iron phosphate and the lithium chemical compound in the mixture is less than or equal to 1.5 mol/L.

### Claim 7 (depends on 1)

The method of claim 1, wherein a morphology of the iron phosphate is changed from a solid spherical structure to a hollow porous structure in the precursor solution.

### Claim 8 (depends on 1)

The method of claim 1, wherein a concentration of lithium ions in the lithium ion source solution is in a range from about 0.5 mol/L to about 0.7 mol/L.

### Claim 9 (depends on 1)

The method of claim 1, wherein a heating apparatus is provided and preheated to the first temperature, and then the mixture is placed in the heating apparatus to keep the first temperature.

### Claim 10 (depends on 1)

The method of claim 1, wherein the second temperature is in the range from about 120° C. to about 250° C.

### Claim 11 (depends on 1)

The method of claim 1, wherein a filling rate for the precursor solution in the solvothermal reaction reactor is about 60%˜80%.