# US 2016/0144577 A1 · Method for manufacturing a composite part from a preimpregnated material with a semi-crystalline matrix having an amorphous surface layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0144577 A1
- Document ID: US20160144577A1
- Status: Published application
- Kind: A1
- Application number: 14/950,838
- Filed: 2015-11-24
- Published: 2016-05-26
- Earliest claimed: 2014-11-24
- Assignees: Alenia Aermacchi S.p.A.
- Applicants: ALENIA AERMACCHI S.p.A.
- Inventors: Michele IANNONE
- Web page: https://patentgrep.com/patent/US20160144577A1

## CPC

- B29C 70/342: {using isostatic pressure}
- B29C 66/73771: {the to-be-joined area of at least one of the parts to be joined being amorphous}
- B29C 66/73773: {the to-be-joined area of at least one of the parts to be joined being semi-crystalline}
- B29C 70/0035: {comprising two or more matrix materials}
- B29C 70/44: using isostatic pressure, e.g. pressure difference-moulding, vacuum bag-moulding, autoclave-moulding or expanding rubber-moulding
- B29C 70/546: {Measures for feeding or distributing the matrix material in the reinforcing structure}
- B29D 99/0021: {provided with plain or filled structures, e.g. cores, placed between two or more plates or sheets, e.g. in a matrix}
- B29C 35/0227: {using pressure vessels, e.g. autoclaves, vulcanising pans (B29C35/065 takes precedence)}
- B29K 2071/00: Use of polyethers {, e.g. PEEK, i.e. polyether-etherketone or PEK, i.e. polyetherketone or derivatives thereof}, as moulding material
- B29K 2079/085: {Thermoplastic polyimides, e.g. polyesterimides, PEI, i.e. polyetherimides, or polyamideimides; Derivatives thereof}
- B29K 2105/253: {Preform}
- B29K 2307/04: Carbon
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A method for manufacturing a composite part includes preparing a stack of plies made of a starting material, applying a vacuum bag to the stack of plies, and subjecting the stack of plies to a temperature and pressure cycle in an autoclave. The starting material is a laminate material of resin matrix reinforced with a fiber material. The matrix has a core layer of semi-crystalline thermoplastic resin and a pair of outer layers of amorphous thermoplastic resin arranged on opposite sides of the core layer. The glass transition temperature of the amorphous thermoplastic resin is below the melting point of the semi-crystalline thermoplastic resin. The autoclave temperature cycle heating rapidly the stack of plies to a working temperature above the transition temperature, but below the melting point, keeping the stack of plies at the working temperature during a time period for compaction alone; and cooling the stack of plies.

## Claims

### Claim 1

A method for manufacturing a composite part, comprising the following steps:
preparing a stack of plies, said stack comprising a plurality of plies, each of the plurality of plies being made of a starting material;
applying a vacuum bag to the stack of plies, and applying vacuum within the vacuum bag; and
subjecting the stack of plies to a temperature and pressure cycle in an autoclave;
wherein said starting material is a laminate material comprising a resin matrix reinforced with a fiber material, wherein the matrix comprises a core layer of semi-crystalline thermoplastic resin having a melting point, and a pair of outer layers arranged on opposite sides of the core layer, each outer layer consisting of amorphous thermoplastic resin having a glass transition temperature, wherein the glass transition temperature of the amorphous thermoplastic resin is below the melting point of the semi-crystalline thermoplastic resin;
wherein adjacent plies of the plurality of plies make contact with each other by the respective outer layers of amorphous thermoplastic resin; and
wherein the temperature and pressure cycle in an autoclave comprises:
applying pressure in an increasing manner until a working pressure is reached, and rapidly heating the stack of plies until a working temperature which is above the glass transition temperature of the amorphous thermoplastic resin but below the melting point of the semi-crystalline thermoplastic resin is reached;
keeping the stack of plies at the working temperature during a time period for compaction alone; and
cooling the stack of plies and releasing the pressure after the temperature has dropped below the glass transition temperature of the amorphous thermoplastic resin.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the rate of increase of the temperature during heating of the temperature and pressure cycle is greater than 3° C./min.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the time period for compaction alone during the temperature and pressure cycle is shorter than 30 minutes.

### Claim 4 (depends on 1)

The method according to claim 1, wherein preparing the stack of plies comprises heat-welding at least some of the plies to one another at local points of the plies.

### Claim 5 (depends on 1)

The method according to claim 1, wherein said semi-crystalline thermoplastic resin is polyether ether ketone.

### Claim 6 (depends on 1)

The method according to claim 1, wherein said amorphous thermoplastic resin is poly(ether imide).

### Claim 7 (depends on 1)

The method according to claim 1, wherein said fiber material comprises carbon fibers.
