# US 2016/0144537 A1 · Method for shaping a plate made of a sintered and restructured polytetrafluoroethylene and applications thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0144537 A1
- Document ID: US20160144537A1
- Status: Published application
- Kind: A1
- Application number: 14/905,127
- Filed: 2014-07-11
- Published: 2016-05-26
- Earliest claimed: 2013-07-15
- Assignees: Commissariat A L'energie Atomique Et Aux Energies Alternatives; Technetics Group France SAS
- Applicants: Commissariat à L'éNergie Atomique Et Aux éNergies Alternatives; Technetics Group France SAS
- Inventors: Laurent GUIMET; Sophie PARSY; Michel LEFRANCOIS
- Web page: https://patentgrep.com/patent/US20160144537A1

## CPC

- B29C 43/003: {characterised by the choice of material}
- B29C 43/006: {Pressing and sintering powders, granules or fibres}
- B29C 43/02: of articles of definite length, i.e. discrete articles {(B29C35/0227 takes precedence)}
- B29C 43/18: incorporating preformed parts or layers, e.g. compression moulding around inserts or for coating articles {(B29C43/206 takes precedence)}
- B29C 43/52: Heating or cooling
- F16K 7/12: with flat, dished, or bowl-shaped diaphragm
- B29C 2791/001: Shaping in several steps
- B29K 2027/18: PTFE, i.e. polytetrafluoroethylene {, e.g. ePTFE, i.e. expanded polytetrafluoroethylene}
- B29K 2105/256: {Sheets, plates, blanks or films}
- B29L 2031/755: {Membranes, diaphragms}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- F16K: VALVES; TAPS; COCKS; ACTUATING-FLOATS; DEVICES FOR VENTING OR AERATING {(devices for emptying and evacuating the excess liquid in valves or conduits F16L55/07)}
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

The invention relates to a method for shaping a plate made of a sintered and restructured polytetrafluoroethylene and to the applications thereof. This method comprises: heating the plate to a temperature θ1 at least equal to the melting temperature of a sintered polytetrafluoroethylene; and shaping the thereby heated plate by compression in a compression mold. Applications: manufacturing of notably diaphragms for diaphragm valves and pumps.

## Claims

### Claim 1

A method for shaping a plate made of a sintered and restructured polytetrafluoroethylene, comprising:
heating the plate to a temperature θ1 at least equal to a melting temperature of a sintered polytetrafluoroethylene; and
shaping the thereby heated plate by compression in a compression mold.

### Claim 2 (depends on 1)

The method of claim 1, wherein the heating of the plate is carried out outside the compression mold.

### Claim 3 (depends on 2)

The method of claim 2, comprising:
introducing the plate in an oven heated beforehand to the temperature θ1 and maintaining the plate in the thereby heated oven for 10 minutes to 60 minutes; and then
transferring the plate into the compression mold, the compression mold being heated beforehand to a temperature θ2 at least equal to 200° C. but less than the melting temperature of the sintered polytetrafluoroethylene, and compressing the plate in the thereby heated compression mold for 5 minutes to 30 minutes, under a pressure ranging from 50 MPa to 150 MPa.

### Claim 4 (depends on 1)

The method of claim 1, wherein the heating of the plate is carried out inside the compression mold.

### Claim 5 (depends on 4)

The method of claim 4, comprising:
introducing the plate in the compression mold, the compression mold being heated beforehand to the temperature θ1, and compressing the plate in the thereby heated compression mold under a pressure ranging from 50 MPa to 150 MPa; and then
cooling the compression mold and maintaining the plate under compression until the temperature of the compression mold is less than the melting temperature of the sintered PTFE.

### Claim 6

A method for manufacturing a film-shaped part made of a sintered and restructured polytetrafluoroethylene, the film-shaped part having at least one not planar portion, from a plate made of a sintered and restructured polytetrafluoroethylene, comprising:
heating the plate to a temperature θ1 at least equal to a melting temperature of a sintered polytetrafluoroethylene; and
shaping the thereby heated plate by compression in a compression mold, the compression mold comprising at least one not planar portion, and thereby obtaining the film-shaped part.

### Claim 7 (depends on 6)

The method of claim 6, wherein the part has a smaller thickness than a thickness of the plate.

### Claim 8 (depends on 6)

The method of claim 6, wherein the part comprises a planar or substantially planar peripheral portion and a dome-shaped central portion.

### Claim 9 (depends on 8)

The method of claim 8, wherein the peripheral portion of the part comprises two opposites faces and a ring-shaped bulge, coaxial with the dome, on at least one of the faces.

### Claim 10 (depends on 8)

The method of claim 8, wherein the part comprises a pin which is integrated to a top of the dome.

### Claim 11 (depends on 6)

The method of claim 6, comprising:
the compression mold is heated.
introducing the plate in an oven heated beforehand to the temperature θ1 and maintaining the plate in the thereby heated oven for 10 minutes to 60 minutes; and then
transferring the plate into the compression mold, the compression mold being heated beforehand to a temperature θ2 at least equal to 200° C. but less than the melting temperature of the sintered polytetrafluoroethylene, and compressing the plate in the thereby heated compression mold for 5 minutes to 30 minutes, under a pressure ranging from 50 MPa to 150 MPa.

### Claim 12 (depends on 6)

The method of claim 6, wherein:
the compression mold is
the plate is maintained under compression at least until the temperature of the compression mold attains 200° C.
introducing the plate in the compression mold, the compression mold being heated beforehand to the temperature θ1, and compressing the plate in the thereby heated compression mold under a pressure ranging from 50 MPa to 150 MPa; and then
cooling the compression mold and maintaining the plate under compression until the temperature of the compression mold is less than the melting temperature of the sintered PTFE.

### Claim 13

A film-shaped part made of a sintered and restructured polytetrafluoroethylene, the part having at least one not planar portion, which may be obtained by a method comprising:
heating a plate made of a sintered and restructured polytetrafluoroethylene to a temperature θ1 at least equal to a melting temperature of a sintered polytetrafluoroethylene; and
shaping the thereby heated plate by compression in a compression mold, the compression mold comprising at least one not planar portion, and thereby obtaining the film-shaped part.

### Claim 14 (depends on 13)

A diaphragm for a diaphragm valve or pump, which comprises at least one sintered and restructured polytetrafluoroethylene part of claim 13, the sintered and restructured polytetrafluoroethylene not comprising any reinforcement filler.

### Claim 15 (depends on 14)

The diaphragm of claim 14, which further comprises at least one part made of an elastomer, the part made of the sintered and restructured polytetrafluoroethylene and the part made of the elastomer being superposed.

### Claim 16 (depends on 14)

A diaphragm valve or pump, which comprises at least one diaphragm of claim 14.

### Claim 17 (depends on 11)

The method of claim 11, wherein:
the oven is heated beforehand to a temperature ranging from 365° C. to 375° C. and the plate is maintained in the thereby heated oven for 10 minutes to 15 minutes; and
the compression mold is heated beforehand to a temperature ranging from 240° C. to 280° C. and the plate is compressed in the thereby heated compression mold for 5 minutes to 10 minutes, under a pressure ranging from 100 MPa to 150 MPa.

### Claim 18 (depends on 12)

The method of claim 12, wherein:
the compression mold is heated beforehand to a temperature ranging from 330° C. to 350° C. and the plate is compressed in the thereby heated compression mold under a pressure ranging from 100 MPa to 150 MPa; and
the plate is maintained under compression at least until the temperature of the compression mold attains 200° C. by the cooling.