# US 2016/0144482 A1 · Diamond enhanced insert with controlled diamond frame strength

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0144482 A1
- Document ID: US20160144482A1
- Status: Published application
- Kind: A1
- Application number: 14/949,520
- Filed: 2015-11-23
- Published: 2016-05-26
- Earliest claimed: 2014-11-21
- Assignees: Smith International, Inc.
- Applicants: Smith International, Inc.
- Inventors: Yi Fang; Haibo Zhang; J. Daniel Belnap
- Web page: https://patentgrep.com/patent/US20160144482A1

## CPC

- B24D 3/10: for porous or cellular structure, e.g. for use with diamonds as abrasives
- B24D 18/0009: {using moulds or presses}
- B24D 99/005: {Segments of abrasive wheels}
- E21B 10/46: characterised by wear resisting parts, e.g. diamond inserts
- E21B 10/55: with preformed cutting elements
- E21B 10/567: with preformed cutting elements mounted on a distinct support, e.g. polycrystalline inserts
- E21B 10/5735: {Interface between the substrate and the cutting element}
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS

## Abstract

A Diamond Enhanced Insert (DEI) includes a working layer of a polycrystalline diamond material (PCD). The PCD material includes a first phase that includes a number of particles of a first material. The PCD material also includes a second phase that is adapted as a catalyst. The PCD material has a fracture toughness greater than 12.5 MPa·√m, a flexural strength of greater than 800 MPa, and a diamond frame strength of less than 400 MPa.

## Claims

### Claim 1

A Diamond Enhanced Insert (DEI), comprising:
a working layer of a polycrystalline diamond (PCD) material comprising:
a first phase comprising a plurality of particles of a first material,
a second phase adapted as a catalyst,
wherein a fracture toughness of the PCD material is greater than 12.5 MPa·√m, a flexural strength of the material is greater than 800 MPa, and a diamond frame strength of the PCD material is less than 400 MPa.

### Claim 2 (depends on 1)

The DEI according to claim 1, wherein the diamond frame strength of the PCD material is less than 400 MPa and greater than 100 MPa.

### Claim 3 (depends on 1)

The DEI according to claim 1, the first phase further comprising:
a plurality of inter-particle bonds, facilitated by the second phase, between the plurality of particles that impart fracture toughness and diamond frame strength to the working layer.

### Claim 4 (depends on 1)

The DEI according to claim 1, wherein the plurality of particles of a first material comprises diamond grains of an average particles size of 30 microns.

### Claim 5 (depends on 1)

The DEI according to claim 1, wherein the second phase comprises less than 10% by weight cobalt and more than 90% by weight tungsten carbide.

### Claim 6 (depends on 1)

The DEI according to claim 1, wherein the second phase comprises less than 20% by weight cobalt and more than 20% by weight tungsten carbide.

### Claim 7 (depends on 1)

The DEI according to claim 1, wherein the first phase occupies greater than 75% by volume of the working layer and the second phase occupies less than 25% by volume of the working layer.

### Claim 8 (depends on 1)

The DEI according to claim 1, wherein the first phase occupies greater than 65% by volume of the working layer and the second phase occupies less than 35% by volume of the working layer.

### Claim 9 (depends on 1)

The DEI according to claim 1, further comprising:
an attachment body adapted to attach the DEI to a boring tool.

### Claim 10 (depends on 9)

The DEI according to claim 9, wherein the working layer is disposed on the attachment body.

### Claim 11 (depends on 9)

The DEI according to claim 9, further comprising:
a transition layer adapted to attach the working layer to the attachment body, wherein the transition layer is disposed on the attachment body.

### Claim 12 (depends on 11)

The DEI according to claim 11, wherein the working layer is disposed on the transition layer.

### Claim 13

A method of forming a Diamond Enhanced Insert (DEI), comprising:
compacting a powder mixture comprising a first phase comprising a plurality of diamond grains and a second phase adapted as a catalyst to form a green composite, and
sintering the green composite to form a polycrystalline diamond (PCD) material.

### Claim 14 (depends on 13)

The method according to claim 13, wherein sintering the green composite comprises a high temperature, high pressure process.

### Claim 15 (depends on 13)

The method according to claim 13, wherein the green composite is sintered directly on a transition layer to form a working layer of the sintered PCD material disposed on the transition layer.

### Claim 16 (depends on 13)

The method according to claim 13, wherein the green composite is sintered directly on an attachment body to form a working layer of the sintered PCD material disposed on the attachment body.

### Claim 17 (depends on 13)

The method according to claim 13, wherein sintering the green composite activates the second phase and causes a plurality of inter-diamond-grain bonds to form between the plurality of diamond grains,
wherein the inter-diamond-grain bonds impart fracture toughness, transverse rupture strength, and diamond frame strength to the PCD material.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the plurality of inter-diamond grain bonds impart a fracture toughness of greater than 12.5 MPa·√m, a transverse rupture strength of greater than 800 MPa, and a diamond frame strength of less than 400 MPa.

### Claim 19 (depends on 17)

The method according to claim 17, wherein the plurality of inter-diamond grain bonds impart a fracture toughness of greater than 12.5 MPa·√m, a transverse rupture strength of greater than 800 MPa, and a diamond frame strength of less than 400 MPa and greater than 100 MPa.

### Claim 20 (depends on 17)

The method according to claim 17, wherein a quantity of the plurality of inter-diamond-grain bonds is set by a ratio of the first phase to the second phase.