# US 2016/0143291 A1 · Strengthened glass with biocidal property

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0143291 A1
- Document ID: US20160143291A1
- Status: Published application
- Kind: A1
- Application number: 14/948,544
- Filed: 2015-11-23
- Published: 2016-05-26
- Earliest claimed: 2014-11-25
- Assignees: Microban Products Company
- Applicants: Microban Products Company
- Inventors: Alvin Lamar Campbell, JR.
- Web page: https://patentgrep.com/patent/US20160143291A1

## CPC

- A01N 59/16: Heavy metals; Compounds thereof
- A01N: PRESERVATION OF BODIES OF HUMANS OR ANIMALS OR PLANTS OR PARTS THEREOF (preservation of food or foodstuff A23); BIOCIDES, e.g. AS DISINFECTANTS, AS PESTICIDES OR AS HERBICIDES (preparations for medical, dental or toiletry purposes which kill or prevent the growth or proliferation of unwanted organisms A61K); PEST REPELLANTS OR ATTRACTANTS; PLANT GROWTH REGULATORS

## Abstract

A biocidal additive formulation comprises a silver containing glass particle, and a combination of at least two metal based compounds. A metal in each of the metal based compounds is selected from the group consisting of silver, copper, zinc, mercury, tin, lead, bismuth, barium, cadmium, chromium, titanium, and a combination thereof. Another biocidal additive formulation comprises a silver containing glass particle, ZnO, and Bi2O3. A glass substrate possessing a durable biocidal property and an article possessing a durable biocidal property are also provided.

## Claims

### Claim 1

A biocidal additive formulation comprising:
a silver containing glass particle, and
a combination of at least two metal based compounds, wherein a metal in each of the metal based compounds is selected from the group consisting of silver, copper, zinc, mercury, tin, lead, bismuth, barium, cadmium, chromium, titanium, and a combination thereof.

### Claim 2 (depends on 1)

The biocidal additive formulation according to claim 1, wherein the metal of each of the inorganic metal based compounds is selected from the group consisting of silver, zinc, bismuth, and a combination thereof.

### Claim 3

A biocidal additive formulation comprising:
a silver containing glass particle,
ZnO, and
Bi2O3.

### Claim 4 (depends on 3)

The biocidal additive formulation according to claim 3, wherein the silver containing glass particle is present in a range of 0.5% to 2.5%, based on the weight of the biocidal additive formulation.

### Claim 5 (depends on 3)

The biocidal additive formulation according to claim 3, wherein ZnO is in a weight ratio to Bi2O3 in a range of 1:2 to 1:3.

### Claim 6 (depends on 3)

The biocidal additive formulation according to claim 3, wherein ZnO is in a weight ratio to Bi2O3 in a range of 2:1 to 3:1.

### Claim 7 (depends on 3)

The biocidal additive formulation according to claim 3, wherein ZnO is present in an amount of 5% to 85% by weight based on the dry weight of the formulation.

### Claim 8 (depends on 3)

The biocidal additive formulation according to claim 3, wherein Bi2O3 is present in an amount of 5% to 85% by weight based on the dry weight of the formulation.

### Claim 9

A method for making a biocidal glass, the method comprising:
adding a biocidal additive formulation comprised of a silver containing glass particle and at least two metal based compounds as an additive package to a glass batch formulation,
wherein a metal in each of the metal based compounds is selected from the group consisting of silver, copper, zinc, mercury, tin, lead, bismuth, barium, cadmium, chromium, and a combination thereof.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the metal of each of the metal based compounds is selected from the group consisting of silver, zinc, bismuth, and a combination thereof.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the at least two metal based compounds are ZnO and Bi2O3.

### Claim 12 (depends on 9)

The method according to claim 9, wherein the silver containing glass particle is present in a range of 0.5% to 2.5%, based on the weight of the biocidal additive formulation.

### Claim 13 (depends on 9)

The method according to claim 9, wherein ZnO is in a weight ratio to Bi2O3 in a range of 1:2 to 1:3.

### Claim 14 (depends on 9)

The method according to claim 9, wherein ZnO is in a weight ratio to Bi2O3 in a range of 2:1 to 3:1.

### Claim 15 (depends on 9)

The method according to claim 9, wherein the additive package is added in an amount in a range of at least 1% based on a dry weight of the glass batch formulation.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the additive package is added in an amount in a range of 1% to 5% based on a dry weight of a glass batch formulation.

### Claim 17 (depends on 1)

A glass substrate possessing a durable biocidal property comprising a biocidal additive package having the formulation according to claim 1.

### Claim 18 (depends on 17)

The glass substrate according to claim 17, wherein the glass substrate is selected from the group consisting of sandwiched, tempered, strengthened, laminated, and a combination thereof.

### Claim 19 (depends on 1)

An article constructed, in whole or in part, of a glass substrate possessing a durable biocidal property, the article comprising a biocidal additive package having the formulation according to claim 1.

### Claim 20 (depends on 19)

The article according to claim 19, wherein the article is dishware, barware, glassware, device cover, automobile window, partition, shelving, work surface, or a touch screen.