Abstract
Ultralow expansion titania-silica glass. The glass has high hydroxyl content and optionally include one or more dopants. Representative optional dopants include boron, alkali elements, alkaline earth elements or metals such as Nb, Ta, Al, Mn, Sn Cu and Sn. The glass is prepared by a process that includes steam consolidation to increase the hydroxyl content. The high hydroxyl content or combination of dopant(s) and high hydroxyl content lowers the fictive temperature of the glass to provide a glass having a very low coefficient of thermal expansion (CTE), low fictive temperature (Tf), and low expansivity slope.
Claims20
A glass comprising:
- 9.0 wt % to 16.0 wt % TiO2;
- 84.0 wt % to 91.0 wt % SiO2;
- and
- 900 ppm to 3000 ppm OH.
Dependencies are inferred from the claim text.