# US 2016/0126084 A1 · Method of producing a halogen lamp and halogen lamp

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0126084 A1
- Document ID: US20160126084A1
- Status: Published application
- Kind: A1
- Application number: 14/932,114
- Filed: 2015-11-04
- Published: 2016-05-05
- Earliest claimed: 2014-11-04
- Assignees: Vosla GmbH
- Applicants: vosla GmbH
- Inventors: Markus Winkler; Martin Polster
- Web page: https://patentgrep.com/patent/US20160126084A1

## CPC

- H01K 1/325: {Reflecting coating}
- H01K 1/32: provided with coatings on the walls; Vessels or coatings thereon characterised by the material thereof
- H01K 3/005: {Methods for coating the surface of the envelope}
- H01K 5/00: Lamps for general lighting (H01K9/00 - H01K13/00 take precedence)
- H01K 7/02: for producing a narrow beam of light; for approximating a point-like source of light, e.g. for searchlight, for cinematographic projector (producing narrow beams by optical means external to lamp F21V)
- H01K: ELECTRIC INCANDESCENT LAMPS (details, apparatus or processes for manufacture applicable to both discharge devices and incandescent lamps H01J; light sources using a combination of incandescent and other types of light generation H01J61/96, H05B35/00)

## Abstract

The present invention relates to a method for producing a halogen lamp, comprising the following steps: providing a glass tube blanket; dip-coating of the glass tube blanket using a sol gel process having an inorganic coating; forming a lamp bulb from the coated glass tube blanket. The present invention relates further to a halogen lamp produced accordingly.

## Claims

### Claim 1

A method of producing a halogen lamp, the method comprising:
Providing a glass tube blanket;
Dip-coating the glass tube blanket using a sol gel process having an inorganic coating;
Forming a lamp bulb from the coated glass tube blanket.

### Claim 2 (depends on 1)

The method of claim 1, wherein the glass tube blanket is suspended and dipped in the sol for dip-coating such that an end portion of the glass tube blanket remains uncoated.

### Claim 3 (depends on 2)

The method of claim 2, wherein electrical components of the halogen lamp are introduced into the glass tube blanket for forming the lamp bulb and are melted portion-wise in the uncoated end portion of the glass tube blanket.

### Claim 4 (depends on 1)

The method of claim 1, wherein the glass tube blanket is made of hard glass.

### Claim 5 (depends on 1)

The method of claim 1, wherein a low pressure is generated in the inner cavity volume of the glass tube blanket for coating the inner surface of the glass tube blanket such that a sol determined for the sol gel process rises up until a predefined extent within the cavity.

### Claim 6 (depends on 1)

The method of claim 1, wherein the coating is applied during dip-coating both on the inner surface and on the outer surface of the glass tube blanket.

### Claim 7 (depends on 1)

The method of claim 1, wherein the coating applied during a dip-coating comprises a coating reflecting infrared radiation.

### Claim 8 (depends on 7)

The method of claim 7, wherein the dip-coating of the glass tube blanket using a sol gel process comprises a structure of an alternating layer system, which comprises in particular between 5 and 30 single layers and having a thickness of 0.3 μm to 3 μm.

### Claim 9 (depends on 7)

The method of claim 7, wherein the alternating layer system alternately comprises single layers having a high and low refraction index.

### Claim 10 (depends on 7)

The method of claim 7, wherein the dip-coating of the glass tube blanket using a sol gel process comprises applying at least a transparent layer having nano pigments reflecting infrared radiation.

### Claim 11 (depends on 1)

The method of claim 1, wherein the dip-coating of the glass tube blanket using a sol gel process comprises applying an absorption layer.

### Claim 12 (depends on 1)

The method of claim 1, wherein the sol gel process comprises a pull out step of the pulling out of the glass tube blanket from the sol, at a relative humidity of the ambient air between 30% and 70%.

### Claim 13 (depends on 1)

The method of claim 1, wherein the sol gel process comprises a tempering step in which the glass tube blanket pulled out from the sol is exposed to a bake-out temperature between 250° C. and 550° C.

### Claim 14

A halogen lamp, comprising a lamp bulb made of hard glass comprising an inorganic coating at least on its inner surface.

### Claim 15 (depends on 14)

The halogen lamp of claim 14, wherein the lamp bulb comprises the inorganic coating both on its inner surface and on its outer surface.

### Claim 16 (depends on 14)

The halogen lamp of claim 14, wherein the halogen lamp is made using a method of producing a halogen lamp, comprising:
Providing a glass tube blanket;
Dip-coating the glass tube blanket using a sol gel process having an inorganic coating;
Forming a lamp bulb from the coated glass tube blanket.