US 2016/0109777 A1Published application
Pretreatment of transparent conductive oxide (tco) thin films for improved electrical contact
AssigneeView, Inc.
InventorsTodd Martin, Abhishek Anant Dixit, Fabian Strong, Anshu A. Pradhan
Life of this patent
Estimating the term…
Abstract
Certain embodiments relate to optical devices and methods of fabricating optical devices that pre-treat a sub-layer to enable selective removal of the pre-treated sub-layer and overlying layers. Other embodiments pertain to methods of fabricating an optical device that apply a sacrificial material layer.
Claims42
A method of fabricating an optical device, the method comprising, in the following order:
- (a) exposing a sub-layer of the optical device to an energy source;
- (b) depositing one or more material layers of the optical device on the sub-layer;
- and
- (c) ablating the one or more material layers and the sub-layer with a laser to expose an underlying layer.
1 more element
(canceled)
(canceled)
(canceled)
(canceled)
A method of fabricating an optical device, the method comprising:
- i) applying a sacrificial material layer to a portion of the area of one or more sub-layers of the optical device;
- ii) depositing one or more material layers of the optical device on the sacrificial material layer and the one or more sub-layers;
- and
- iii) applying a laser to the portion to ablate the optical device at least down to the sacrificial material layer.
1 more element
An optically switchable device comprising:
- a substantially transparent substrate;
- a lower conductor layer disposed over the substantially transparent substrate;
- and
- a bus bar on the lower conductor layer of a portion of the area of a substrate wherein the remainder of the area has an electrochromic device stack with a sacrificial material layer and/or a sub-layer on top of the lower conductor layer.
1 more element
Dependencies are inferred from the claim text.