- Inventors: Gregory K. Krumdick; Krzysztof Pupek; Trevor L. Dzwiniel
- Web page: https://patentgrep.com/patent/US20150318574A1

## CPC

- H01M 10/0569: characterised by the solvents
- H01M 10/052: Li-accumulators
- H01M 2300/0028: characterised by the solvent
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The invention provides a method for producing electrolyte solvent, the method comprising reacting a glycol with a disilazane in the presence of a catalyst for a time and at a temperature to silylate the glycol, separating the catalyst from the silylated glycol, removing unreacted silazane; and purifying the silylated glycol.

## Claims

### Claim 1

A continuous method for producing battery grade electrolyte solvent, the method comprising:
a. reacting a glycol with a disilazane in the presence of a catalyst in a reactor for a time and at a temperature to silylate the glycol;
b. separating the catalyst from the silylated glycol wherein the catalyst remains in the reactor;
c. removing unreacted silazane; and
d. purifying the silylated glycol, wherein the method is conducted without an inert atmosphere.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The method as recited in claim 1 wherein the time is selected from between about 2 and about 6 hours.

### Claim 4 (depends on 1)

The method as recited in claim 1 wherein the temperature is selected from between about 30° C. and about 70° C.

### Claim 5 (depends on 1)

The method as recited in claim 1 wherein the catalyst is a solid catalyst selected from the group consisting of Amberlyst, Nafion, Montmorillonite, and combinations thereof.

### Claim 6 (depends on 1)

The method as recited in claim 1 wherein the catalyst is solid and the catalyst is separated from the silylated glycol by simple particle filtration.

### Claim 7 (depends on 2)

The method as recited in claim 2 wherein the unreacted silazane is returned to the reactor.

### Claim 8 (depends on 1)

The method as recited in claim 1 wherein the silylated glycol is purified in a single fractional distillation.

### Claim 9 (depends on 1)

The method as recited in claim 1 wherein the silylated glycol is more than 99.5 percent pure.

### Claim 10 (depends on 1)

The method as recited in claim 1 wherein the glycol is a polyethylene glycol selected from the group consisting of alkyl ethers of HO(CH2CH2O)xOAlkyl, where x=2-5, Alkyl=group of 1-6 carbon atoms.

### Claim 11 (depends on 1)

The method as recited in claim 1 wherein no solvent is utilized.

### Claim 12 (depends on 1)

The method as recited in claim 1 wherein the only waste product is ammonia.

### Claim 13 (depends on 1)

The method as recited in claim 1 wherein the glycol is 2-(2-methoxyethoxy)ethanol and the silylated glycol is 2,2-dimethyl-3,6,9-trioxa-2-siladecane.

### Claim 14 (depends on 1)

The method as recited in claim 1 wherein the glycol is 2-(2-(2-methoxyethoxy)ethoxy)ethanol and the silylated glycol is 2,2-dimethyl-3,6,9,12-tetraoxa-2-silatridecane.

### Claim 15 (depends on 1)

The method as recited in claim 1 wherein the disilazane is a hexa-substituted disilazane selected from the group consisting of hexamethyldisilazane, 1,3-diethyl-1,1,3,3-tetramethyldisilazane, 1,3-diallyl-1,1,3,3-tetramethyldisilazane, 1,3-diphenyl-1,1,3,3-tetramethyldisilazane, and combinations thereof.

### Claim 16 (depends on 1)

The method as recited in claim 1 wherein the catalyst is immobilized within the reactor.

### Claim 17 (depends on 1)

The method as recited in claim 1 wherein the catalyst is present in a weight percent of between about 0.5 to about 30.