# US 2015/0306660 A1 · Continuous casting method for slab made of titanium or titanium alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0306660 A1
- Document ID: US20150306660A1
- Status: Published application
- Kind: A1
- Application number: 14/646,366
- Filed: 2014-01-23
- Published: 2015-10-29
- Earliest claimed: 2013-01-23
- Assignees: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
- Applicants: Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
- Inventors: Eisuke KUROSAWA; Takehiro NAKAOKA; Kazuyuki TSUTSUMI; Hideto OYAMA; Hidetaka KANAHASHI; Hitoshi ISHIDA; Daiki TAKAHASHI; Daisuke MATSUWAKA
- Web page: https://patentgrep.com/patent/US20150306660A1

## CPC

- B22D 11/041: for vertical casting (B22D11/043, B22D11/049 - B22D11/059 take precedence)
- B22D 11/001: {of specific alloys}
- B22D 11/103: Distributing the molten metal, e.g. using runners, floats, distributors
- B22D 11/11: Treating the molten metal
- B22D 11/115: by using magnetic fields
- B22D 11/117: by treating with gases (B22D11/118, B22D11/119 take precedence)
- B22D 21/005: {with high melting point, e.g. Be 1280 degrees C, Ti 1725 degrees C}
- B22D 27/02: Use of electric or magnetic effects {(for continuous casting B22D11/015, B22D11/11)}
- B22D 27/04: Influencing the temperature of the metal, e.g. by heating or cooling the mould
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

A continuous casting method in which a molten metal obtained by melting titanium or a titanium alloy is injected into a bottomless mold having a rectangular cross-section and withdrawn downward while being caused to solidify, wherein a plasma torch (7) is caused to rotate in the horizontal direction above the surface of the molten metal (12) in the mold (2), and a horizontally rotating flow is generated by electromagnetic stirring on at least the surface of the molten metal (12) in the mold (2). It is thereby possible to cast a slab in which the casting surface condition is excellent.

## Claims

### Claim 1

A continuous casting method for continuously casting a slab made of titanium or a titanium alloy by injecting molten metal having titanium or a titanium alloy melted therein into a bottomless mold having a rectangular cross section and withdrawing the molten metal downward while being solidified,
wherein a plasma torch is configured to horizontally rotate on the surface of the molten metal in the mold, and
a horizontally rotating flow is generated by electromagnetic stirring at least on the surface of the molten metal in the mold.

### Claim 2 (depends on 1)

The continuous casting method for the slab made of titanium or a titanium alloy according to claim 1, wherein, when a length of a long side of the slab is denoted as L and a coordinate axis x is set in the long side direction of the slab, where the origin 0 lies at the central part thereof, in a vicinity of mold walls at long side parts of the mold, absolute values of average values of flow rates in the x-axis direction at the surface of the molten metal located in a range of −2 L/5≦x≦2 L/5 are set to 300 mm/sec or more.

### Claim 3 (depends on 2)

The continuous casting method for the slab made of titanium or a titanium alloy according to claim 2, wherein the vicinity of the mold walls at the long side parts of the mold is a location 10 mm away from the mold walls at the long side parts of the mold.

### Claim 4 (depends on 2)

The continuous casting method for the slab made of titanium or a titanium alloy according to claim 2, wherein standard deviations σ of the absolute values of the flow rates of the molten metal in the x-axis direction, concerning to variations due to locations and time, are confined in a range of 50 mm/sec≦σ≦85 mm/sec.

### Claim 5 (depends on 1)

The continuous casting method for the slab made of titanium or a titanium alloy according to claim 1, wherein a flow rotating in an opposite direction to a rotational direction of the plasma torch is generated at least on the surface of the molten metal.

### Claim 6 (depends on 3)

The continuous casting method for the slab made of titanium or a titanium alloy according to claim 3, wherein standard deviations σ of the absolute values of the flow rates of the molten metal in the x-axis direction, concerning to variations due to locations and time, are confined in a range of 50 mm/sec≦σ≦85 mm/sec.

### Claim 7 (depends on 2)

The continuous casting method for the slab made of titanium or a titanium alloy according to claim 2, wherein a flow rotating in an opposite direction to a rotational direction of the plasma torch is generated at least on the surface of the molten metal.