# US 2015/0275326 A1 · Preheating and annealing of cold rolled metal strip

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0275326 A1
- Document ID: US20150275326A1
- Status: Published application
- Kind: A1
- Application number: 14/431,624
- Filed: 2013-10-05
- Published: 2015-10-01
- Earliest claimed: 2012-10-05
- Assignees: Linde Aktiengesellschaft
- Applicants: Linde Aktiengesellschaft
- Inventors: Henrik Gripenberg; Johannes Lodin
- Web page: https://patentgrep.com/patent/US20150275326A1

## CPC

- C21D 9/56: Continuous furnaces for strip or wire
- C21D 1/52: with flames
- C21D 9/52: for wires; for strips {; for rods of unlimited length}
- C21D 9/563: {Rolls; Drums; Roll arrangements}
- C21D 9/63: the strip being supported by a cushion of gas
- C22C 9/00: Alloys based on copper
- C22C 21/00: Alloys based on aluminium
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22F 1/04: of aluminium or alloys based thereon
- C22F 1/08: of copper or alloys based thereon
- F27B 9/28: for treating continuous lengths of work
- F27B 9/36: Arrangements of heating devices
- F27D 9/00: Cooling of furnaces or of charges therein (casings, linings, walls or roofs incorporating cooling arrangements F27D1/12)
- F27D 13/00: Apparatus for preheating charges; Arrangements for preheating charges
- F27D 99/0033: {using burners}
- F27B 2009/3615: {Burner in the ceiling directed vertically downwards}
- F27D 2099/0043: {Impulse burner}
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE

## Abstract

A method of continuously annealing a cold rolled metal strip, by continuously transporting the strip along a transport path where a ramp of direct flame impingement (DFI) burners are located for heating the strip. The ramp is located perpendicular, or substantially perpendicular, to the direction of movement of the strip and the DFI burners are mutually located such that the whole width of the strip is heated to the same, or substantially the same, temperature. The velocity of the strip on the transport path passing the ramp and the heating power of the DFI burners is adapted to heat the strip to annealing temperature, and the preheated strip is annealed in a continuous soaking furnace or annealing furnace.

## Claims

### Claim 1

A method of preheating a cold rolled metal strip prior to continuous annealing, comprising:
continuously transporting the strip along a transport path where a ramp of direct flame impingement (DFI) burners are located for heating the strip, wherein the ramp is located perpendicular, or substantially perpendicular, to the direction of movement of the strip, wherein the DFI burners are located such that the whole width of the strip is heated to the same, or substantially the same, temperature, and wherein the velocity of the strip on the transport path passing the ramp and the heating power of the DFI burners are adapted to heat the strip to annealing temperature.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the ramp comprises at least one ramp above and at least one ramp below the transport path.

### Claim 3 (depends on 1)

The method according to claim 1, wherein there are two or more successive ramps of DFI burners.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the DFI burners are located in a furnace, in particular in a direct flame impingement (DFI) furnace.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the strip is an unwound metal strip from a cold coil.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the strip is provided to the transportation path directly from a rolling stand.

### Claim 7 (depends on 6)

The method according to claim 6, wherein a safety wall is located between the DFI burners and the rolling stand.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the strip is preheated to a temperature of between about 450° C. and about 600° C.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the strip is preheated in a few seconds or less.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the strip is an aluminum strip, a copper strip, an iron strip, or an alloy of aluminum, of copper and/or of iron.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the strip comprises a thickness between 0.5 mm to a maximum thickness at which the strip can be coiled.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the strip comprises a thickness of about 0.9 mm to about 1 mm.

### Claim 13

A method of continuously annealing a cold rolled metal strip, comprising:
preheating the strip by;
continuously transporting the strip along a transport path where a ramp of direct flame impingement (DFI) burners are located for heating the strip, wherein the ramp is located perpendicular, or substantially perpendicular, to the direction of movement of the strip, wherein the DFI burners are located such that the whole width of the strip is heated to the same, or substantially the same, temperature, and wherein the velocity of the strip on the transport path passing the ramp and the heating power of the DFI burners are adapted to heat the strip to annealing temperature and
annealing the preheated strip in a continuous soaking furnace or annealing furnace.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the heat treated strip is wound to a coil.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the heat treated and coiled strip is placed in the soaking furnace for partial annealing and for removing dislocations.

### Claim 16 (depends on 8)

The method according to claim 8, wherein the strip is preheated to a temperature of about 540° C.

### Claim 17 (depends on 9)

The method according to claim 9, wherein the strip is preheated in about one second.