# US 2015/0260912 A1 · Method for producing deuterium-treated optical fiber, and deuterium-treated optical fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0260912 A1
- Document ID: US20150260912A1
- Status: Published application
- Kind: A1
- Application number: 14/424,053
- Filed: 2013-08-23
- Published: 2015-09-17
- Earliest claimed: 2012-08-27
- Assignees: Sumitomo Electric Industries, Ltd.
- Applicants: Sumitomo Electric Industries, Ltd.
- Inventors: Tetsuya Haruna; Masaaki Hirano; Yoshiaki Tamura
- Web page: https://patentgrep.com/patent/US20150260912A1

## CPC

- G02B 6/02214: {tailored to obtain the desired dispersion, e.g. dispersion shifted, dispersion flattened}
- C03B 37/01807: {Reactant delivery systems, e.g. reactant deposition burners}
- C03B 37/10: Non-chemical treatment (surface treatment of fibres or filaments made from glass, minerals or slags C03C25/00)
- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- C03C 13/047: {containing deuterium}
- C03C 25/60: by diffusing ions or metals into the surface
- C03C 25/607: in the gaseous phase
- C03B 2201/22: doped with deuterium
- C03B 2201/50: doped with alkali metals
- C03B 2207/90: with vapour generated from solid glass precursors, i.e. by sublimation
- C03C 2201/22: containing deuterium
- C03C 2201/50: containing alkali metals
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

An alkali-metal-doped core optical fiber having high hydrogen resistance and a method for manufacturing such an optical fiber are provided. A method for manufacturing a deuterium-treated optical fiber according to the present invention includes a preform-forming step of forming a silica glass optical fiber preform having a core doped with an alkali metal element, a drawing step of drawing the optical fiber preform to form an optical fiber, and an exposing step of exposing the optical fiber to a deuterium gas atmosphere. Alkali-metal-doped core optical fibers can be manufactured by using this method. In the exposing step, the optical fiber is exposed to an atmosphere containing deuterium gas at a temperature of 20° C. or more under conditions where (deuterium gas partial pressure)×(exposure time) is 50 kPa·hour or more.

## Claims

### Claim 1

A method for manufacturing a deuterium-treated optical fiber, comprising:
drawing an optical fiber preform to form a silica glass optical fiber that includes a core region and a cladding region surrounding the core region, the core region containing an alkali metal element, the average concentration of the alkali metal element being 0.5 atomic ppm or more; and
exposing the optical fiber to an atmosphere containing deuterium gas at a temperature of 20° C. or more under conditions where (deuterium gas partial pressure)×(exposure time) is 50 kPa·hour or more.

### Claim 2 (depends on 1)

The method for manufacturing a deuterium-treated optical fiber according to claim 1, wherein
the deuterium gas partial pressure is 5 kPa or less.

### Claim 3 (depends on 1)

The method for manufacturing a deuterium-treated optical fiber according to claim 1, wherein the temperature is 80° C. or less.

### Claim 4 (depends on 1)

The method for manufacturing a deuterium-treated optical fiber according to claim 1, wherein
the exposure time is 200 hours or less.

### Claim 5

A deuterium-treated silica glass optical fiber, comprising:
a core region containing an alkali metal element, the average concentration of the alkali metal element being 0.5 atomic ppm or more; and
a cladding region surrounding the core region,
wherein the deuterium-treated optical fiber was exposed to an atmosphere containing deuterium gas at a temperature of 20° C. or more under conditions where (deuterium gas partial pressure)×(exposure time) is 50 kPa·hour or more, and
exposure of the deuterium-treated optical fiber to an atmosphere containing hydrogen gas having a partial pressure of 1 kPa for 720 hours at a temperature of 25° C. increases an attenuation at a wavelength of 1550 nm by 0.003 dB/km or less.

### Claim 6 (depends on 5)

The deuterium-treated optical fiber according to claim 5, wherein
the average concentration of chlorine in the core region is 1,000 atomic ppm or more.

### Claim 7 (depends on 5)

The deuterium-treated optical fiber according to claim 5, wherein
the maximum concentration of fluorine in the core region is 200 atomic ppm or more.

### Claim 8 (depends on 5)

The deuterium-treated optical fiber according to claim 5, wherein
the concentration of transition metal elements and typical metal elements in the core region is less than 0.5 atomic ppm.

### Claim 9 (depends on 5)

The deuterium-treated optical fiber according to claim 5, wherein
the alkali metal element is potassium.

### Claim 10 (depends on 5)

The deuterium-treated optical fiber according to claim 5, wherein
the attenuation at a wavelength of 1550 nm is 0.180 dB/km or less.

### Claim 11 (depends on 5)

The deuterium-treated optical fiber according to claim 5, wherein
the average concentration of the alkali metal element is 100 atomic ppm or less.

### Claim 12 (depends on 5)

The deuterium-treated optical fiber according to claim 5, wherein
exposure of the deuterium-treated optical fiber to an atmosphere containing hydrogen gas having a partial pressure of 1 kPa for 720 hours at a temperature of 25° C. increases an attenuation at a wavelength in the range of 1530 to 1570 nm by 0.003 dB/km or less.

### Claim 13 (depends on 5)

The deuterium-treated optical fiber according to claim 5, wherein
exposure of the deuterium-treated optical fiber to an atmosphere containing hydrogen gas having a partial pressure of 1 kPa for 720 hours at a temperature of 25° C. increases an attenuation at a wavelength in the range of 1560 to 1620 nm by 0.003 dB/km or less.

### Claim 14 (depends on 5)

The deuterium-treated optical fiber according to claim 5, wherein
exposure of the deuterium-treated optical fiber to an atmosphere containing hydrogen gas having a partial pressure of 1 kPa for 720 hours at a temperature of 25° C. increases an attenuation at a wavelength of 1380 nm by 0.01 dB/km or less.

### Claim 15 (depends on 5)

The deuterium-treated optical fiber according to claim 5, wherein
exposure of the deuterium-treated optical fiber to an atmosphere containing hydrogen gas having a partial pressure of 101 kPa for 20 hours at a temperature of 80° C. increases an attenuation at a wavelength of 1380 nm by 0.2 dB/km or less.

### Claim 16

A deuterium-treated silica glass optical fiber, comprising:
a core region containing an alkali metal element, the average concentration of the alkali metal element being in the range of 0.5 to 100 atomic ppm; and
a cladding region surrounding the core region,
wherein the average concentration of chlorine in the core region is 1,000 atomic ppm or more,
the concentration of transition metal elements and typical metal elements in the core region is less than 0.5 atomic ppm,
the deuterium-treated optical fiber was exposed to an atmosphere containing deuterium gas having a partial pressure in the range of 1 to 5 kPa for 20 to 200 hours at a temperature in the range of 40° C. to 80° C.,
the deuterium-treated optical fiber has an attenuation of 0.180 dB/km or less at a wavelength of 1550 nm, and
exposure of the deuterium-treated optical fiber to an atmosphere containing hydrogen gas having a partial pressure of 1 kPa for 720 hours at a temperature of 25° C. increases an attenuation at a wavelength of 1550 nm by 0.003 dB/km or less.