# US 2015/0234107 A1 · Method for producing retardation film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0234107 A1
- Document ID: US20150234107A1
- Status: Published application
- Kind: A1
- Application number: 14/702,312
- Filed: 2015-05-01
- Published: 2015-08-20
- Earliest claimed: 2008-02-14
- Assignees: Zeon Corporation
- Applicants: Zeon Corporation
- Inventors: Taku HATANO; Kohei ARAKAWA; Shunsuke YAMANAKA
- Web page: https://patentgrep.com/patent/US20150234107A1

## CPC

- G02B 5/3083: {Birefringent or phase retarding elements (G02B5/3008, G02B5/3016 take precedence; systems for polarisation control G02B27/286; manufacturing phase modulating patterns by lithographic processes G03F7/001)}
- B29C 48/0018: {combined with shaping by orienting, stretching or shrinking, e.g. film blowing (B29C48/0017 takes precedence)}
- B29C 48/21: the layers being joined at their surfaces
- B29C 55/023: {using multilayered plates or sheets}
- B29C 55/045: {in a direction which is not parallel or transverse to the direction of feed, e.g. oblique}
- B29C 55/143: {firstly parallel to the direction of feed and then transversely thereto}
- B29D 11/0073: {Optical laminates}
- B29C 48/0021: {combined with joining, lining or laminating}
- B29C 48/08: flexible, e.g. films
- B29C 59/12: in an environment other than air
- B29C 59/14: by plasma treatment {(plasma tubes per se H01J)}
- B29K 2025/04: {Polymers of styrene}
- B29K 2069/00: Use of PC, i.e. polycarbonates {or derivatives thereof}, as moulding material
- B29K 2995/0018: having particular optical properties, e.g. fluorescent or phosphorescent
- B29K 2995/0034: Polarising
- B29L 2011/00: Optical elements, e.g. lenses, prisms
- B29L 2011/0066: {Optical filters}
- B29L 2031/3475: {Displays, monitors, TV-sets, computer screens}
- G02F 1/13363: Birefringent elements, e.g. for optical compensation
- Y10T 428/31507: Of polycarbonate
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for producing a retardation film comprising the steps of: co-extruding or simultaneously casting a thermoplastic resin A and a thermoplastic resin B to obtain a laminated film comprising a layer of the thermoplastic resin A and a layer of the thermoplastic resin B; and uniaxially stretching the laminated film at least twice to cross a molecular orientation axis in the layer of the thermoplastic resin A and a molecular orientation axis in the layer of the thermoplastic resin B each other at almost right angles.

## Claims

### Claim 1

A method for producing a retardation film comprising steps of:
co-extruding or simultaneously casting a thermoplastic resin A and a thermoplastic resin B to obtain a laminated film comprising a layer of the thermoplastic resin A and a layer of the thermoplastic resin B, and
uniaxially stretching the laminated film at least twice to cross a molecular orientation axis in the layer of the thermoplastic resin A and a molecular orientation axis in the layer of the thermoplastic resin B each other at an angle of 70 degrees to 110 degrees,
in which the thermoplastic resin A has a positive or negative intrinsic birefringence and the thermoplastic resin B has an intrinsic birefringence of the same sign as a sign of the thermoplastic resin A.

### Claim 2 (depends on 1)

The method according to claim 1, in which an absolute value of difference between a deflection temperature under load TsA of the thermoplastic resin A and a deflection temperature under load TsB of the thermoplastic resin B is 5° C. or more.

### Claim 3 (depends on 1)

The method according to claim 1, in which a rupture elongation of the thermoplastic resin A at the temperature of TsB is 50% or more and a rupture elongation of the thermoplastic resin B at the temperature of TsA is 50% or more.

### Claim 4 (depends on 1)

The method according to claim 1, in which one of the thermoplastic resin A and the thermoplastic resin B is 40 or more in Abbe number, and the another is 30 or less in Abbe number.

### Claim 5 (depends on 1)

The method according to claim 1, in which the laminated film has a characteristic that a phase of linearly polarized light entering vertically into the film plane and having an oscillating surface of an electric vector in an X-Z plane against a phase of linearly polarized light entering vertically into the film plane and having an oscillating surface of an electric vector in a Y-Z plane either lags or leads if and when the laminated film is uniaxially stretched in the direction of the X axis at both stretching temperatures T1 and T2, in which the X axis is an uniaxially stretching direction, the Y axis is a direction perpendicular to the uniaxially stretching direction in the film plane, and the Z axis is a direction of a thickness of the film.

### Claim 6 (depends on 1)

The method according to claim 1, in which a stretching temperature in the uniaxially stretching is different by each time.

### Claim 7 (depends on 1)

The method according to claim 1, in which the first uniaxially stretching is carried out at a temperature of T1 or T2, and the second uniaxially stretching is carried out at a temperature of T2 or T1 different from the temperature in the first uniaxially stretching.

### Claim 8 (depends on 7)

The method according to claim 7, in which the second uniaxially stretching is carried out at a temperature of T2, if TsA>TsB, or the second uniaxially stretching is carried out at a temperature of T1, if TsA<TsB, in which TsA is a deflection temperature under load of the thermoplastic resin A and TsB is a deflection temperature under load of the thermoplastic resin B.

### Claim 9 (depends on 1)

The method according to claim 1, in which a stretching ratio in the second uniaxially stretching is smaller than a stretching ratio in the first uniaxially stretching.

### Claim 10 (depends on 1)

The method according to claim 1, in which the laminated film has a characteristic that an absolute value of a phase difference which appears in a resin having a high deflection temperature under load is smaller than an absolute value of the phase difference which appears in a resin having a low deflection temperature under load if and when the laminated film is stretched at low temperature TL, and an absolute value of a phase difference which appears in the resin having the low deflection temperature under load is smaller than an absolute value of a phase difference which appears in the resin having the high deflection temperature under load if and when the laminated film is stretched at high temperature TH, wherein TH is T1 and TL is T2 or TH is T2 and TL is T1.

### Claim 11 (depends on 1)

A retardation film which is obtained by the method according to claim 1.

### Claim 12 (depends on 11)

The retardation film according to claim 11, the retardation film satisfying a relation of R450<R550<R650, in which R450 is a retardation value of light having a wavelength of 450 nm at an incident angle of 0 degrees, R550 is a retardation value of light having a wavelength of 550 nm at an incident angle of 0 degrees, and R650 is a retardation value of light having a wavelength of 650 nm at an incident angle of 0 degrees.