# US 2015/0197688 A1 · METHOD FOR PRODUCING A DOPED SiO2 SLURRY AND USE OF THE SiO2 SLURRY

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0197688 A1
- Document ID: US20150197688A1
- Status: Published application
- Kind: A1
- Application number: 14/411,332
- Filed: 2013-06-25
- Published: 2015-07-16
- Earliest claimed: 2012-06-26
- Assignees: Heraeus Quarzglas GmbH & Co. KG
- Applicants: Heraeus Quarzglas GmbH & Co., KG
- Inventors: Mario Such; Gerhard Schoetz; Andreas Langner
- Web page: https://patentgrep.com/patent/US20150197688A1

## CPC

- C09K 11/77064: {Aluminosilicates}
- C01B 33/18: Preparation of finely divided silica neither in sol nor in gel form; After-treatment thereof (preparation of aerogels by dehydrating gels C01B33/158; treatment to enhance the pigmenting or filling properties C09C)
- C03B 19/066: {for the production of quartz or fused silica articles (other processes specially adapted for the production of quartz or fused silica articles C03B20/00)}
- C03C 1/006: {to produce glass through wet route}
- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- C03C 4/12: for luminescent glass; for fluorescent glass
- C09K 11/025: {non-luminescent particle coatings or suspension media}
- C03B 2201/06: Doped silica-based glasses
- C03B 2201/32: doped with aluminium (C03B2201/36 takes precedence)
- C03B 2201/34: doped with rare earth metals, i.e. with Sc, Y or lanthanides, e.g. for laser-amplifiers
- C03B 2201/36: doped with rare earth metals and aluminium, e.g. Er-Al co-doped
- C03C 3/061: {by leaching a soluble phase and consolidating}
- C03C 2201/06: Doped silica-based glasses
- C03C 2201/3488: Ytterbium
- C03C 2201/36: containing rare earth metals and aluminium, e.g. Er-Al co-doped
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

The invention relates to a method for producing a doped SiO2 slurry in which an SiO2 suspension is brought into interaction with at least one doping solution, wherein the SiO2 suspension and/or the doping solution act on one another in the form of an atomised spray, the average droplet diameter of which is in the range between 10 μm and 100 μm. The invention further relates to the use of an SiO2 slurry doped by the atomised spray method for the production of doped quartz glass, particularly for the production of laser-active quartz glass.

## Claims

### Claim 1

A method for producing a doped SiO2 slurry, said method comprising:
providing at least one doping solution continually to a SiO2 suspension that contains SiO2 particles in an aqueous liquid so as to form the doped SiO2 slurry,
wherein, while the doped SiO2 slurry is being formed, the doped SiO2 slury is continuously kept in motion, and
wherein the SiO2 suspension or the doping solution act on each other another with the SiO2suspension or the doping solution being in the form of a spray mist having a mean drop diameter that is in a range between 10 μm and 100 μm.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the mean drop diameter is in a range between 10 μm and 50 μm.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the SiO2 suspension and the at least one doping solution are in the form of spray mists and are intermixed in a mist phase thereof.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the SiO2 suspension or the doping solution are atomized into the spray mist using one or more spray nozzles.

### Claim 5 (depends on 1)

The method according to claim 1, wherein, when the spray mist is generated, an operating pressure in the range of 0.5 bar to 10 bar is used.

### Claim 6 (depends on 1)

The method according to claim 1, wherein, when the spray mist is generated, a flow rate in the range of 0.2 l/h to 4.0 l/h is used.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the SiO2 suspension or the doping solution or the at least partly doped SiO2 slurry is kept in motion using one or more propeller stirrers.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the SiO2 suspension or the doping solution is filtered prior to the generation of the spray mist thereof.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the SiO2 suspension has a pH of more than 12.

### Claim 10

(canceled)

### Claim 11

(canceled)

### Claim 12 (depends on 1)

The method according to claim 1, wherein, when the spray mist is generated, an operating pressure of less than 5 bar is used.

### Claim 13 (depends on 1)

The method according to claim 1, wherein, when the spray mist is generated, a flow rate in the range of 0.2 l/h to 0.5 l/h is used.