# US 2015/0191387 A1 · Methods and apparatuses for producing laminated glass sheets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0191387 A1
- Document ID: US20150191387A1
- Status: Published application
- Kind: A1
- Application number: 14/413,625
- Filed: 2012-07-13
- Published: 2015-07-09
- Earliest claimed: 2012-07-13
- Assignees: Corning Incorporated
- Inventors: Antoine Gaston Denis Bisson; Olivier Fournel; Allan Mark Fredholm; Laurent Joubaud; Jean-Pierre Lereboullet; Xavier Tellier
- Web page: https://patentgrep.com/patent/US20150191387A1

## CPC

- C03B 18/12: Making multilayer, coloured or armoured glass (chemical aspects C03C)
- C03B 5/267: {specially adapted for supplying the float tank}
- C03B 7/08: Feeder spouts, e.g. gob feeders
- C03B 17/02: Forming {molten} glass coated with coloured layers; {Forming molten glass of different compositions or layers; Forming molten glass comprising reinforcements or inserts}
- C03B 18/02: Forming sheets
- C03B 18/06: using mechanical means, e.g. restrictor bars, edge rollers
- Y02P 40/57: Improving the yield, e-g- reduction of reject rates
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

According to one embodiment, a method for forming a laminated glass sheet includes forming a multi-layer glass melt (300) from a molten core glass (106) and at least one molten cladding glass (126). The multi-layer glass melt (300) has a width Wm, a melt thickness Tm and a core to cladding thickness ratio TC:TCl. The multi-layer glass melt (300) is directed onto the surface of a molten metal bath (162) contained in a float tank (160). The width Wm of the multi-layer glass melt (300) is less than the width Wf of the float tank (160) prior to the multi-layer glass melt (300) entering the float tank (160). The multilayer glass melt (300) flows over the surface of the molten metal bath (162) such that the width Wm of the multi-layer glass melt (300) increases, the melt thickness Tm decreases, and the core to cladding thickness ratio TC:TCl remains constant as the multi-layer glass melt (300) solidifies into a laminated glass sheet. The invention also relates to the associated apparatus.

## Claims

### Claim 1

A method for forming a laminated glass sheet, the method comprising:
forming a multi-layer glass melt from a molten core glass and at least one molten cladding glass, wherein the multilayer glass melt has a width Wm, a melt thickness Tm and a core to cladding thickness ratio Tc:Tcl;
directing the multi-layer glass melt onto the surface of a molten metal bath contained in a float tank having a width Wf, wherein the width Wm of the multi-layer glass melt is less than the width Wf of the float tank prior to the entering the float tank; and
flowing the multi-layer glass melt over the surface of the molten metal bath such that the width Wm increases, the melt thickness Tm decreases, and the core to cladding thickness ratio Tc:Tcl remains constant as the multi-layer glass melt solidifies into the laminated glass sheet.

### Claim 2 (depends on 1)

The method of claim 1, further comprising drawing the multi-layer glass melt in a direction of the width Wf of the float tank as the multi-layer glass melt flows over the surface of the molten metal bath.

### Claim 3 (depends on 1)

The method of claim 1, further comprising drawing the multi-layer glass melt in a direction of the width Wf of the float tank and a length Lf of the float tank as the multi-layer glass melt flows over the surface of the molten metal bath.

### Claim 4 (depends on 1)

The method of claim 1, further comprising directing the multi-layer glass melt onto a receiving surface of a receiving plane prior to directing the multi-layer glass melt onto the surface of the molten metal bath.

### Claim 5 (depends on 1)

The method of claim 1, wherein the multi-layer glass melt is formed by:
melting a core glass composition into the molten core glass;
melting a molten cladding glass composition into the at least one molten cladding glass; and
delivering the molten core glass and the at least one molten cladding glass to a slot draw apparatus comprising a core glass slot and at least one cladding glass slot such that the molten core glass passes through the core glass slot and the at least one molten cladding glass passes through the at least one cladding glass slot wherein the slot draw apparatus layers the at least one molten cladding glass and the molten core glass as the molten core glass and the at least one molten cladding glass exit the slot draw apparatus thereby forming the multi-layer glass melt.

### Claim 6 (depends on 5)

The method of claim 5, wherein the core glass slot and the at least one cladding glass slot are oriented in parallel with one another.

### Claim 7 (depends on 5)

The method of claim 5, wherein the slot draw apparatus is positioned over the float tank containing the molten metal bath and oriented at a slot angle greater than or equal to 0° and less than 90° with respect to a surface of the molten metal bath.

### Claim 8

A method for forming a laminated glass sheet, the method comprising:
forming a molten core glass from a core glass composition;
forming a molten cladding glass from a cladding glass composition;
providing a slot draw apparatus comprising a core slot and at least one cladding slot, wherein:
the core slot and the at least one cladding slot are oriented in parallel with one another;
the slot draw apparatus is positioned over a float tank containing a molten metal bath and oriented at a slot angle greater than or equal to 0° and less than 90° with respect to a surface of the molten metal bath; and
a width Ws of the slot draw apparatus is less than a width Wf of the float tank;
delivering the molten core glass and the molten cladding glass to the slot draw apparatus such that the molten core glass passes through the core slot and the molten cladding glass passes through the at least one cladding slot, the molten cladding glass and the molten core glass forming a multi-layer glass melt with a width Wm, a melt thickness Tm, and a core to cladding thickness ratio Tc:Tcl, upon exiting the slot draw apparatus, wherein the width Wm is less than the width Wf;
directing the multi-layer glass melt onto the surface of the molten metal bath wherein, as the multi-layer glass melt flows over the surface of the molten metal bath, the width Wm of the multi-layer glass melt increases, the melt thickness Tm decreases, and the core to cladding thickness ratio Tc:Tcl remains constant as the multi-layer glass melt solidifies into the laminated glass sheet.

### Claim 9 (depends on 8)

The method of claim 8, further comprising:
directing the multi-layer glass melt onto a receiving surface of a receiving plane prior to directing the multi-layer glass melt onto the surface of the molten metal bath.

### Claim 10 (depends on 9)

The method of claim 9, wherein the receiving surface of the receiving plane is oriented at a receiving plane angle greater than or equal to 0° and less than 90° with respect to a surface of the molten metal bath.

### Claim 11 (depends on 8)

The method of claim 8, further comprising:
contacting an upper surface of the multi-layer glass melt with a plurality of top rollers when the multi-layer glass melt is on the surface of the molten metal bath; and
drawing the multi-layer glass melt in a direction of the width Wf of the float tank with the plurality of top rollers.

### Claim 12 (depends on 8)

The method of claim 8, further comprising:
contacting an upper surface of the multi-layer glass melt with a plurality of top rollers when the multi-layer glass melt is on the surface of the molten metal bath; and
drawing the multi-layer glass melt in a direction of the width Wf and a length Lf of the float tank with the plurality of top rollers.

### Claim 13 (depends on 8)

The method of claim 8, wherein the core slot has a core height the at least one cladding slot has a cladding height Hcl and the core height Hc is not equal to the cladding height Hcl.

### Claim 14 (depends on 8)

The method of claim 8, wherein the at least one cladding slot of the slot draw apparatus comprises a first cladding slot and a second cladding slot and the core slot is positioned between the first cladding slot and the second cladding slot.

### Claim 15 (depends on 14)

The method of claim 14, wherein the first cladding slot has a first height Hcla and the second cladding slot has a second height Hclb and the first height Hcla is not equal to the second height Hclb.

### Claim 16 (depends on 14)

The method of claim 14, wherein the core slot has a core height Hc, the first cladding slot has a first height Hcla and the second cladding slot has a second height Hclb, wherein the core height Hc is greater than the first height Hcla and the second height Hclb.

### Claim 17 (depends on 8)

The method of 16 claim 8, wherein the core slot and the at least one cladding slot comprise a plurality of reinforcing webs.

### Claim 18 (depends on 17)

The method of claim 17, wherein the reinforcing webs are recessed from an outlet of the slot draw apparatus

### Claim 19 (depends on 1)

The method of claim 1 wherein the laminated glass sheet has a width greater than 4 meters.

### Claim 20

An apparatus for forming a laminated glass sheet, the apparatus comprising:
a core glass melting vessel;
a cladding glass melting vessel;
a slot draw apparatus comprising a core glass slot and at least one cladding glass slot, wherein:
the core glass slot and the at least one cladding glass slot, are oriented in parallel with one another;
the core glass slot is fluidly coupled to the core glass melting vessel such that molten core glass can be delivered from the core glass melting vessel to the core glass slot;
the at least one cladding glass slot is fluidly coupled to the cladding glass melting vessel such that molten cladding glass can be delivered from the cladding glass melting vessel to the at least one cladding glass slot; and
a float tank containing a molten metal bath, the float tank having a width Wf which is greater than a width Ws of the slot draw apparatus, wherein the slot draw apparatus is positioned over the float tank and oriented at a slot angle greater than or equal to 0° and less than 90° with respect to a surface of the molten metal bath.