# US 2015/0181899 A1 · Tubular Food Casing Having Glued, Permanently Elastic Longitudinal Seam

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0181899 A1
- Document ID: US20150181899A1
- Status: Published application
- Kind: A1
- Application number: 14/619,418
- Filed: 2015-02-11
- Published: 2015-07-02
- Earliest claimed: 2006-06-27
- Assignees: Kalle GmbH
- Applicants: Kalle GmbH
- Inventors: Michael SEELGEN; Holger SCHLANGE
- Web page: https://patentgrep.com/patent/US20150181899A1

## CPC

- A22C 13/0006: {Apparatus for making artificial collagen casings (chemical aspects A22C13/0016)}
- A22C 13/0013: {Chemical composition of synthetic sausage casings}
- B31B 70/00: Making flexible containers, e.g. envelopes or bags
- B65D 65/14: with areas coated with adhesive
- B65D 65/42: Applications of coated or impregnated materials
- A22C 2013/0053: {multilayer casings}
- A22C 2013/0069: {seamed casings, casings with at least one longitudinal seam}
- A22C 2013/0093: {textile casings, casings with at least one layer of textile material}
- A22C 2013/0096: {cellulosic}
- B31B 2155/00: Flexible containers made from webs
- B31B 2160/20: with structural provision for thickness of contents
- B65D 2565/387: Materials used as gas barriers
- Y10T 428/1307: Bag or tubular film [e.g., pouch, flexible food casing, envelope, etc.]
- Y10T 428/1324: Flexible food casing [e.g., sausage type, etc.]
- A22C: PROCESSING MEAT, POULTRY, OR FISH (preserving A23B; obtaining protein compositions for foodstuffs A23J1/00; fish, meat or poultry preparations A23L; disintegrating, e.g. chopping meat, B02C18/00; preparation of proteins C07K1/00)
- B31B: MAKING CONTAINERS OF PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNER ANALOGOUS TO PAPER (making wound articles, e.g. wound tubes, B31C; combined making and filling B65B)
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A shirr-stable, tubular food casing having a glued, permanently elastic longitudinal seam based on a flat fibrous textile material coated with acrylic, collagen and/or a protein derived therefrom is provided. The seam is generated using a reactive hotmelt glue. The glued seam is resistant to boiling for a long time and also exhibits sufficient stability thereafter. Exemplary textile materials include a consolidated nonwoven or spunbonded nonwoven, a woven fabric, loop-formingly knitted fabric, laid fabric, loop-drawingly knitted fabric. To form the casing, the textile material is coated in the flat state. The coated textile material is cut into strips according to the diameter of the casing to be produced and glued using a reactive hotmelt glue, such as a PUR hotmelt glue, to form the tube. The food casing is preferably used as artificial sausage casing or for wrapping cheese or fish.

## Claims

### Claim 1

A shirrable, shirr stable tubular food casing comprising a coated flat support material formed into a tube having a glued, permanently elastic longitudinal seam,
wherein the seam is bonded via a cured, reactive one-component polyurethane-based hotmelt glue,
the flat support material comprises synthetic fibers, and
the flat support material is a woven fabric, loop-formingly knitted fabric, loop-drawingly knitted fabric, laid fabric, consolidated nonwoven, or spunbonded nonwoven,
the polyurethane-based hotmelt glue has a softening temperature ranging from 90° C. to below 160° C., and the hotmelt glue cure consists of a water-cure, with water introduced during tube formation curing the hotmelt glue,
the support material has been desized and comprises a pretreatment of a dilute dispersion of a coating material and a coating, said costing material consisting of acrylic resin(s),
the glue penetrates into the fibers in the material,
wherein (i) the polyurethane-based hotmelt glue has a Brookfield viscosity ranging from 3000 to 7000 mPa·s as measured using an RVT DV-II digital viscosimeter, spindle 27; (ii) the casing has a water content of about 2 to 20% by weight, and (iii) the glued seam is reacted at 25% to 75% relative humidity and 20 to 45° C. for 3 to 7 days and (iv) the hotmelt glue cures via the water introduced during the tube formation and the moisture of the air during curing only counteracts diffusion from the glued tube.

### Claim 2

A shirrable, shirr stable tubular food casing comprising a coated flat textile support material formed into a tube having a glued, permanently elastic longitudinal seam,
wherein the seam is bonded via a cured, reactive polyurethane-based hotmelt glue that does not comprise particles,
the flat support material comprises synthetic fibers, and
the flat support material is a woven, knit or nonwoven fabric,
wherein the polyurethane-based hotmelt glue has a softening temperature ranging from 90° C. to below 160° C., and the hotmelt glue cure consists of a water-cure,
at adhesion surfaces at both edges of the textile, at least two lines of glue are applied at a center line distance of 2 to 10 mm apart and
the glue penetrates into the fibers in the textile support material throughout the textile support materials entire thickness.

### Claim 3 (depends on 2)

The food casing as claimed in claim 2, wherein one or more of the adhesion surfaces has been plasma activated and/or pro-heated prior to glue application.

### Claim 4 (depends on 2)

The food casing as claimed in claim 2, wherein the coated flat textile is coated with 3 to 5 layers of polymer.

### Claim 5 (depends on 2)

The food casing as claimed in claim 2, wherein the synthetic fibers are selected from polyester, polyamide, polyolefin, poly(vinyl acetate), polyacrylonitrile, poly(vinyl chloride), or corresponding copolymers.

### Claim 6 (depends on 2)

The food casing as claimed in claim 2, wherein the flat support material has a weight of 8 to 300 g/m2.

### Claim 7 (depends on 2)

The food casing as claimed in claim 2, wherein the food casing has a total weight in the dry state of 40 to 400 g/m2.

### Claim 8 (depends on 2)

The food casing as claimed in claim 2, wherein the flat support material has been pretreated with a diluted dispersion of the coating polymer.

### Claim 9 (depends on 2)

The food casing as claimed in claim 2, wherein the flat support material is impregnated with melamine/formaldehyde resin, hydroxypropylated starch ethers, acrylic resins, or polyamine-polyamide-epichlorohydrin resins.

### Claim 10 (depends on 2)

The food casing as claimed in claim 2, wherein the flat support material is colored with dyes and/or color pigments.

### Claim 11 (depends on 2)

The food casing as claimed in claim 2, wherein the flat textile support is coated with acrylic resin.

### Claim 12 (depends on 2)

The food casing as claimed in claim 2, wherein, on the inside and/or outside, the food casing further comprises at least one layer having barrier properties for oxygen and/or water vapor.

### Claim 13 (depends on 2)

The food casing as claimed in claim 2, wherein, on the inside, the food casing further comprises an impregnation or coating and/or agents which comprise transferable color, aroma, odor and/or taste substances.

### Claim 14 (depends on 2)

The food casing as claimed in claim 2, wherein the food casing is finally processed into shined sticks or sections closed at one end.

### Claim 15 (depends on 2)

The food casing as claimed in claim 2, wherein said food casing has an oxygen permeability of 100 to 1000 cm2/m2d, determined as specified in ISO 7783-2 at 53% relative humidity measured on a 5 cm2 size piece of the casing having a water content of 8 to 10% by weight and a plasticizer content of about 15% by weight.

### Claim 16 (depends on 2)

The food casing as claimed in claim 2, wherein (i) the polyurethane-based hotmelt glue has a Brookfield viscosity ranging from 3000 to 7000 mPa·s as measured using an RVT DV-II digital viscosimeter, spindle 27; (ii) the casing has a water content of about 2 to 20% by weight, and (iii) the glued seam is reacted at 25% to less than 50% relative humidity and 20 to 45° C. for 3 to 7 days and (iv) the hotmelt glue cures via the water introduced during the tube formation alone.

### Claim 17 (depends on 2)

A process for producing a food casing as claimed in claim 2, which comprises the following steps in the stated sequence:
a) providing a flat fibrous material;
b) coating one or both sides of the flat fibrous material with at least one layer of coating comprising acrylic resin, collagen and/or a protein derived therefrom;
c) optionally costing one or both sides of the coated flat fibrous material with a barrier layer,
d) drying the coating(s);
e) optionally cutting the coated whole-width flat fibrous material into strips;
f) optionally printing the strips;
g) forming the coated flat fibrous material or strips via a forming shoulder to give a tube having overlapping longitudinal edges;
h) gluing the overlapping region using a reactive hotmelt glue;
i) curing the glued seam at 25 to 75% relative humidity and 20 to 45° C. for 3 to 7 days; and
j) optionally finally processing the food casing.

### Claim 18 (depends on 17)

The process as claimed in claim 17, wherein the reactive hot melt glue is a reactive PUR hotmelt glue having a Brookfield viscosity of 3000 to 7000 mPa·s.

### Claim 19 (depends on 17)

The process as claimed in claim 17, wherein the reactive hotmelt glue is applied as a thin melt film to the longitudinal edge of the casing which after joining is on the lower side of the overlapping region.