# US 2015/0177635 A1 · Toner and two-component developer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0177635 A1
- Document ID: US20150177635A1
- Status: Published application
- Kind: A1
- Application number: 14/574,771
- Filed: 2014-12-18
- Published: 2015-06-25
- Earliest claimed: 2013-12-20
- Assignees: Canon Kabushiki Kaisha
- Applicants: Canon Kabushiki Kaisha
- Inventors: Kosuke Fukudome; Shuhei Moribe; Satoshi Mita; Kunihiko Nakamura; Noriyoshi Umeda; Yoshiaki Shiotari; Naoki Okamoto; Tetsuya Ida
- Web page: https://patentgrep.com/patent/US20150177635A1

## CPC

- G03G 9/08755: {Polyesters}
- G03G 9/081: {by mixing the toner components in a liquefied state; melt kneading; reactive mixing}
- G03G 9/08728: {Polymers of esters}
- G03G 9/08788: {Block polymers}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- G03G 9/107: having magnetic components
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

A toner contains toner particles. The toner particles are made of a resin containing an amorphous polyester resin, a releasing agent, an additive and a coloring agent. The additive has a polyester portion and a crystalline acrylic portion that are chemically bound to each other.

## Claims

### Claim 1

A toner comprising toner particles made of a resin containing:
an amorphous polyester resin;
a releasing agent;
an additive and
a coloring agent,
wherein
the additive comprises a resin having a polyester portion and a crystalline acrylic portion that are chemically bound to each other, and
the crystalline acrylic portion has a partial structure expressed by the following chemical formula:
wherein R represents a hydrocarbon group having a carbon number of 18 to 30, and X represents hydrogen or a methyl group.

### Claim 2 (depends on 1)

The toner according to claim 1, wherein the toner particles are prepared through a melt-kneading step.

### Claim 3 (depends on 1)

The toner according to claim 1, wherein the additive has a melting peak on a temperature-endothermic curve thereof prepared by differential scanning calorimetry, the melting peak:
i) lying at a peak temperature Tmc in the range of 50° C. to 70° C.;
ii) representing a heat of melting in the range of 2.00 J/g to 20.00J/g for 1 g of the additive; and
iii) having a half-width of 5.00° C. or less.

### Claim 4 (depends on 3)

The toner according to claim 3, wherein the releasing agent has a melting peak on a temperature-endothermic curve thereof prepared by differential scanning calorimetry, and the melting peak thereof satisfies the relationship:
3≦Tmb−Tmc≦23,
where Tmb represents the melting peak temperature in degrees Celsius of the releasing agent and Tmc represents the melting peak temperature in degrees Celsius of the additive.

### Claim 5 (depends on 1)

The toner according to claim 1, wherein the toner particles contain a crystalline polyester resin.

### Claim 6 (depends on 1)

A two-component developer comprising: