# US 2015/0177536 A1 · Electro-optical single crystal element, method for the preparation thereof, and systems employing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0177536 A1
- Document ID: US20150177536A1
- Status: Published application
- Kind: A1
- Application number: 14/390,522
- Filed: 2013-04-04
- Published: 2015-06-25
- Earliest claimed: 2012-04-04
- Assignees: Pengdi Han
- Inventors: Pengdi Han; Welling Yan
- Web page: https://patentgrep.com/patent/US20150177536A1

## CPC

- G02F 1/055: the active material being a ceramic (G02F1/035 takes precedence)
- B29D 11/00932: {Combined cutting and grinding thereof}
- G02F 1/0027: {Ferro-electric materials}
- G02F 1/0136: {for the control of polarisation, e.g. state of polarisation [SOP] control, polarisation scrambling, TE-TM mode conversion or separation (G02F1/0353 takes precedence)}
- G02F 1/05: with ferro-electric properties (G02F1/035, G02F1/055 take precedence)
- G02F 1/21: by interference
- G02F 1/3558: {Poled materials, e.g. with periodic poling; Fabrication of domain inverted structures, e.g. for quasi-phase-matching [QPM]}
- G02F 1/212: {Mach-Zehnder type}
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)

## Abstract

The present invention relates to an Electro-Optical (E-O) crystal elements, their applications and the processes for the preparation thereof. More specifically, the present invention relates to the E-O crystal elements (which can be made from doped or un-doped PMN-PT, PIN-PMN-PT or PZN-PT ferroelectric crystals) showing super-high linear E-O coefficient yc, e.g., transverse effective linear E-O coefficient yTc more than 1100 pm/V and longitudinal effective linear E-O coefficient ylc up to 527 pm/V, which results in a very low half-wavelength voltage Vtx below 200V and Vtx below about 87V in a wide number of modulation, communication, laser, and industrial uses.

## Claims

### Claim 1

A method of producing an electro-optical crystal element, comprising the steps of:
preparing a ferroelectric crystal having a chemical composition represented by one of the chemical formulas:
Pb(Mg1/3Nb2/3)1-xTixO3 where x is defined as 0.22 to 0.38 (I)
or
Pb(Zn1/3Nb2/3)1-yTiO3 where y is defined as 0.04 to 0.11, (II)
wherein, all said crystal elements can be doped or co-doped with Lanthanum (La) up to 6% (wt %), Antimony (Sb), Tantalum (Ta) up to 8% (wt %), Indium (In) up to 31% (wt %), Zirconium (Zr) up to 5% (wt %) and at least one rare earth element from the group consisting of: Cerium (Ce), Erbium (Er), Terbium (Tb), Scandium (Sc), and Neodymium (Nd), up to 8% (wt %);
slicing said crystal element to (011) and forming wafers; and
polarizing into a mm2-symmetric structure by poling said crystal element in <011> direction under 2 times of coercive field (Ec) in a temperature range below 95° C.

### Claim 2 (depends on 1)

The method of producing an electro-optical crystal element, according to claim 1, wherein:
said step of polarizing results in one of a single domain and a multi-nano-domain structure.

### Claim 3 (depends on 1)

The method of producing, according to claim 1, further comprising the steps of:
conducting a dicing of said prepared crystal element; and
conducting a polishing and an optical finishing of said crystal element, thereby forming said electro-optical crystal element.

### Claim 4 (depends on 3)

The method of producing, according to claim 3, further comprising the steps of:
electroding said crystal element.

### Claim 5 (depends on 1)

A method of producing, according to claim 1, further comprising the steps of:
providing a transverse mode crystal element; and
said transverse mode crystal element providing <011> polarization and giving the transverse effective E-O coefficient γrc more than 527 pm/V and half-wave voltage VTπ less than 87.5 V (l/d=1) at room temperature 20° C.

### Claim 6 (depends on 1)

A method of producing, according to claim 1, further comprising the steps of:
providing a longitudinal mode crystal element;
coating a transparent electrodes on said longitudinal mode crystal element; and
said longitudinal mode crystal element providing <011> polarization of longitudinal effective E-O coefficient γlc more than 427 pm/V and Vlπ less than 300 V at room temperature 20° C.

### Claim 7

A method of producing an electro-optical crystal element, comprising the steps of:
preparing a ferroelectric crystal having a chemical composition represented by the chemical formula:
y*[Pb(In1/2Nb1/2)O3]-(1-y)*[Pb(Mg1/3Nb2/3)1-xTixO3] (III)
where x is defined as 0.0 to 0.35, y as 0.0 to 0.35 slicing said crystal element to (011) wafers; and
polarizing into mm2 symmetric structure by poling said crystal element in <011> direction under 2 times of coercive field (Ec) in a temperature range below 95° C.

### Claim 8 (depends on 7)

The method of producing an electro-optical crystal element, according to claim 7, wherein:
said step of polarizing results in one of a single domain and a multi-nano-domain structure.

### Claim 9 (depends on 7)

The method of producing, according to claim 7, further comprising the steps of:
conducting a dicing of said prepared crystal element; and
conducting a polishing and an optical finishing of said crystal element, thereby forming said electro-optical crystal element.

### Claim 10 (depends on 9)

The method of producing, according to claim 9, further comprising the steps of:
electroding said crystal element.

### Claim 11 (depends on 7)

A method of producing, according to claim 7, further comprising the steps of:
providing a transverse mode crystal element; and
said transverse mode crystal element providing <011> polarization and giving the transverse effective E-O coefficient γTc above 500 pm/V and half-wave voltage VTπ less than 12 V (l/d=7) at room temperature 20° C.

### Claim 12 (depends on 7)

A method of producing, according to claim 7, further comprising the steps of:
providing a longitudinal mode crystal element;
coating a transparent electrode on said longitudinal mode crystal element; and
said longitudinal mode crystal element providing <011> polarization of longitudinal effective E-O coefficient γlc above 427 pm/V and Vlπ less than 300 V at room temperature 20° C.

### Claim 13 (depends on 7)

An electro-optical system, said system being one of an amplitude modulator and a phase modulator, comprising:
a longitudinal mode electro-optical crystal element produced by a method acceding to claim 7; and
said longitudinal mode electro-optical crystal element including means for providing <011> polarization of longitudinal effective E-O coefficient γlc above 427 pm/V and Vlπ less than 300 V at room temperature 20° C.

### Claim 14 (depends on 1)

An electro-optical system, said system being one of an amplitude modulator and a phase modulator, comprising:
a transverse mode electro-optical crystal element produced by a method according to claim 1; and
said transverse mode electro-optical crystal element including means for providing <011> polarization and giving the transverse effective E-O coefficient γTc above 500 pm/V and half-wave voltage VTπ less than 87.5 V (l/d=1) at room temperature 20° C.

### Claim 15 (depends on 7)

An electro-optical system, said system being one of an amplitude modulator and a phase modulator, comprising:
a transverse mode electro-optical crystal element produced by a method acceding to claim 7; and
said transverse mode electro-optical crystal element including means for providing <011> polarization and giving the transverse effective E-O coefficient γTπ above 500 pm/V and half-wave voltage VTπ less than 12 V (l/d=7) at room temperature 20° C.

### Claim 16 (depends on 1)

An electro-optical modulator system for laser beams, comprising:
a Mach-Zehnder-type interferometer modulator on an (011) surface of an optical electrical crystal element; and
said optical electrical crystal element produced by a method according to claim 1.

### Claim 17 (depends on 7)

An electro-optical modulator system for laser beams, comprising:
a Mach-Zehnder-type interferometer modulator on an (011) surface of an optical electrical crystal element; and
said optical electrical crystal element produced by a method according to claim 7.