# US 2015/0177421 A1 · Light reflection film and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0177421 A1
- Document ID: US20150177421A1
- Status: Published application
- Kind: A1
- Application number: 14/219,020
- Filed: 2014-03-19
- Published: 2015-06-25
- Earliest claimed: 2013-12-19
- Assignees: Hon Hai Precision Industry Co., Ltd.
- Applicants: Hon Hai Precision Industry Co., Ltd.
- Inventors: FENG-YUEN DAI; CHAU-JIN HU; KUN-CHAN WU; JIA-MING WANG
- Web page: https://patentgrep.com/patent/US20150177421A1

## CPC

- B29D 11/00788: {Producing optical films}
- G02B 5/0284: {used in reflection}
- G02B 5/0808: {having a single reflecting layer (G02B5/0883, G02B5/0891 take precedence)}
- B29K 2105/0032: {Pigments, colouring agents or opacifiyng agents}
- B29K 2509/00: Use of inorganic materials not provided for in groups {B29K2503/00 - B29K2507/00,} as filler
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A method of manufacturing a light refection film includes: preparing a precursor, the precursor includes white pigments and liquid UV (ultraviolet) curing material. The white pigments are evenly dispersed in the UV curing material, and a weight ratio of the white pigments and the UV curing material ranges from 20:80 to 38:62. Then the following step is providing a first base, and arranging a blocking part on the first base to limit a receiving area of the precursor. The precursor is thereafter dropped into the receiving area of the precursor. A second base is then brought to press the precursor, the precursor is cured by exposure UV to form the light reflection film, finally the first base, the second base, and the blocking part are removed to obtain the light reflection film. The present disclosure also provides a light reflection film obtained by the method.

## Claims

### Claim 1

A light reflection film, comprising UV curing material and white pigments evenly dispersed in the UV curing material, wherein a weight ratio of the white pigments and the UV curing material ranges from 20:80 to 38:62.

### Claim 2 (depends on 1)

The light reflection film of claim 1, wherein a thickness of the light reflection film is no more than 0.2 mm.

### Claim 3 (depends on 1)

The light reflection film of claim 1, wherein an average particle diameter of the white pigments ranges from about 0.1 μm to about 0.4 μm.

### Claim 4 (depends on 1)

The light reflection film of claim 1, wherein the white pigments are selected from the group consisting of ZnO, ZnWO4, SiO2, TiO2, CaCO3, CaSO4, BaSO4, and Al2O3.

### Claim 5

A method of manufacturing a light reflection film, comprising:
preparing a precursor and a first base, and arranging a blocking part on the first base to define a receiving area on the first base, wherein the precursor comprises white pigments and liquid UV curing material, the white pigments are evenly dispersed in the UV curing material, and a weight ratio of the white pigments and the UV curing material ranges from 20:80 to 38:62;
dropping the precursor into the receiving area;
providing a second base to press and flatten the precursor;
curing the precursor to form the light reflection film; and
removing the first base, the second base, and the blocking part to obtain the light reflection film.

### Claim 6 (depends on 5)

The method of manufacturing the light reflection film of claim 5, wherein a thickness of the light reflection film is no more than 0.2 mm.

### Claim 7 (depends on 5)

The method of manufacturing the light reflection film of claim 5, wherein an average particle diameter of the white pigments ranges from about 0.1 μm to about 0.4 μm.

### Claim 8 (depends on 5)

The method of manufacturing the light reflection film of claim 5, wherein before preparing the precursor, the white pigments are treated by a process of surface treatment to increase a surface evenness and smooth thereof to thereby increase a reflectivity thereof.

### Claim 9 (depends on 8)

The method of manufacturing the light reflection film of claim 8, wherein the white pigments are selected from the group consisting of ZnO, ZnWO4, SiO2, TiO2, CaCO3, CaSO4, BaSO4, and Al2O3.

### Claim 10 (depends on 9)

The method of manufacturing the light reflection film of claim 9, wherein the white pigments are made of ZnO, and an average particle diameter of the white pigments is about 0.1 μm.

### Claim 11 (depends on 9)

The method of manufacturing the light reflection film of claim 9, wherein the white pigments are made of a mixture consisting of ZnO, ZnWO4 and SiO2, a weight ratio of ZnO, ZnWO4 and SiO2 is 7:3:18, and an average particle diameter of the white pigments is about 0.2 μm.

### Claim 12 (depends on 9)

The method of manufacturing the light reflection film of claim 9, wherein the white pigments are made of a mixture consisting of CaSO4 and CaCO3, a weight ratio of CaSO4 and CaCO3 is 15:15, and an average particle diameter of the white pigments is about 0.4 μm.

### Claim 13 (depends on 9)

The method of manufacturing the light reflection film of claim 9, wherein the white pigments are made of TiO2, an average particle diameter of the white pigments is about 0.3 μm.

### Claim 14 (depends on 14)

The method of manufacturing the light reflection film of claim 14, wherein the white pigments consist of spherical TiO2 particles.

### Claim 15 (depends on 9)

The method of manufacturing the light reflection film of claim 9, wherein the white pigments are made of a mixture consisting of TiO2 and Al2O3, a weight ratio of TiO2 and Al2O3 is 30:5, and an average particle diameter of the white pigments is about 0.3 μm.

### Claim 16 (depends on 9)

The method of manufacturing the light reflection film of claim 9, wherein the white pigments are made of a mixture consisting of BaSO4 and Al2O3, a weight ratio of BaSO4 and Al2O3 is 15:23, and an average particle diameter of the white pigments is about 0.2 μm.