# US 2015/0176727 A1 · Thick, high-strength, sour-resistant line pipe and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0176727 A1
- Document ID: US20150176727A1
- Status: Published application
- Kind: A1
- Application number: 14/407,253
- Filed: 2013-03-29
- Published: 2015-06-25
- Earliest claimed: 2012-06-18
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Akihiko Tanizawa; Haruo Nakamichi; Toru Kawanaka; Noriaki Uchitomi; Takafumi Ozeki
- Web page: https://patentgrep.com/patent/US20150176727A1

## CPC

- F16L 9/02: of metal (F16L9/16 - F16L9/22 take precedence)
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/10: during manufacturing of tubular bodies
- C21D 9/0081: {for slabs; for billets}
- C21D 9/14: wear-resistant or pressure-resistant pipes
- C21D 9/46: for sheet metals
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/18: containing chromium
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- G01N 29/043: {in the interior, e.g. by shear waves}
- C21D 2211/002: Bainite
- G01N 2291/0234: Metals, e.g. steel
- G01N 2291/044: Internal reflections (echoes), e.g. on walls or defects
- G01N 2291/2634: cylindrical from outside
- F16L: PIPES; JOINTS OR FITTINGS FOR PIPES; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING; MEANS FOR THERMAL INSULATION IN GENERAL
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A line pipe having a wall thickness of 20 mm or more and a tensile strength of 560 MPa or more and a production method therefor are provided. The base metal portion contains particular amounts of C, Si, Mn, P, S, Al, Nb, Ca, N, and O, one or more component selected from Cu, Ni, Cr, Mo, V, and Ti as optional components, and the balance being Fe and unavoidable impurities. The microstructure in the pipe thickness direction contains 90% or more bainite and 1% or less of MA in a region that extends from a position 2 mm from an inner surface to a position 2 mm from an outer surface. In a hardness distribution in the pipe thickness direction, the hardness in a region other than a center segregation area is 220 Hv10 or less and the hardness in the center segregation area is 250 Hv10 or less. The major axes of pores, inclusions, and inclusion clusters that are present in a portion that extends from, a position 1 mm from the inner surface to a 3/16 position of the tube thickness and in a portion that extends from a position 1 mm from the outer surface to a 13/16 position of the tube thickness in the tube thickness direction are 1.5 mm or less.

## Claims

### Claim 1

A heavy wall, high-strength line pipe for sour gas service, wherein a chemical composition of a steel pipe base metal portion contains, in terms of % by mass, C: 0.020 to 0.060%, Si: 0.50% or less, Mn: 0.80 to 1.50%, P: 0.008% or less, 5: 0.0015% or less, Al: 0.080% or less, Nb: 0.005 to 0.050%, Ca: 0.0010 to 0.0040%, N: 0.0080% or less, O: 0.0030% or less, and the balance being Fe and unavoidable impurities, Ceq expressed by equation (1) is 0.320 or more, PHIC expressed by equation (2) is 0.960 or less, ACRM expressed by equation (3) is 1.00 to 4.00, and PCA expressed by equation (4) is 4.00 or less;
a microstructure in a pipe thickness direction contains 90% or more bainite and 1% or less martensite-austenite constituent in a region that extends from a position 2 mm from an inner surface to a position 2 mm from an outer surface;
in a hardness distribution in the pipe thickness direction, a hardness of a region other than a center segregation area is 220 Hv10 or less and a hardness of the center segregation area is 250 Hv10 or less; and
major axes of pores, inclusions, and inclusion clusters that are present in a portion that extends from a position 1 mm from the inner surface to a 3/16 position of a pipe thickness and in a portion that extends from a position 1 mm from the outer surface to a 13/16 position of the pipe thickness in the pipe thickness direction are 1.5 mm or less:
Ceq=C+Mn/6+(Cu+Ni)/15+(Cr+Mo+V)/5 equation (1)
PHIC=4.46C+2.37Mn/6+(1.74Cu+1.7Ni)/5+(1.18Cr+1.95Mo+1.74V)/15+22.36P equation (2)
ACRM=(Ca−(1.230−0.000365))/(1.25S) equation (3)
PCA=10000CaS0.28 equation (4)
where respective alloying elements in equations (1) to (4) represent their contents (% by mass) in the chemical composition.

### Claim 2 (depends on 1)

The heavy wall, high-strength line pipe for sour gas service according to claim 1, wherein the chemical composition of the steel pipe base metal portion further contains, in terms of % by mass, at least one selected from Cu: 0.50% or less, Ni: 1.00% or less, Cr: 0.50% or less, Mo: 0.50% or less, V: 0.100% or less, and Ti: 0.030% or less.

### Claim 3 (depends on 1)

The heavy wall, high-strength line pipe for sour gas service according to claim 1, wherein the pipe thickness is 20 mm or more and T/D is 0.045 or less (T representing the pipe thickness (mm) and D representing a pipe diameter (mm)).

### Claim 4 (depends on 1, 1000, 1150)

A method for producing a heavy wall, high-strength line pipe for sour gas service, the method comprising reheating a continuously cast slab having the chemical composition according to claim 1 to 1000 to 1150° C.; hot-rolling the reheated slab at a total reduction ratio of 40 to 90% in an un-recrystallized temperature range; conducting accelerated cooling from a surface temperature of Ar3-t ° C. or more (where t represents a plate thickness (mm)) to a temperature in the range of 200 to 400° C., in which cooling from 700 to 600° C. is conducted at an average cooling rate of 200° C./s or less in a portion that extends from a position 1 mm from a front surface to a 3/16 position of the plate thickness and in a portion that extends from a position 1 mm from a rear surface to a 13/16 position of the plate thickness in a plate thickness direction and at a cooling rate of 20° C./s or more at a center in the plate thickness direction; conducting, immediately after the accelerated cooling, reheating to a surface temperature of 525° C. or more and a plate thickness center temperature of 400 to 500° C.; conducting cold working to bend the resulting plate into a pipe; and welding butted portions of two edges to form a welded steel pipe.

### Claim 5 (depends on 4)

The method for producing a heavy wall, high-strength line pipe for sour gas service according to claim 4, wherein after the hot rolling, descaling is conducted at an impingement pressure of the injection flow of 1 MPa or more at a steel plate surface immediately before the accelerated cooling.

### Claim 6 (depends on 4)

The method for producing a heavy wall, high-strength line pipe for sour gas service according to claim 4, wherein a pipe thickness is 20 mm or more and T/D is 0.045 or less (T representing the pipe thickness (mm) and D representing a pipe diameter (mm)).

### Claim 7 (depends on 4)

A method for judging resistance to HIC of a heavy wall, high-strength line pipe for sour gas service, wherein, after a welded steel pipe is produced by the method according to claim 4, samples are cut out from a base metal of the steel pipe and ultrasonic flaw detection is conducted with a 20 MHz or higher probe in a portion that extends from a position 1 mm from an inner surface to a 3/16 position of the pipe thickness and in a portion that extends from a position 1 mm from an outer surface to a 13/16 position of the pipe thickness in a pipe thickness direction, the ultrasonic flaw detection being conducted over a region having an area of at least 200 mm2 in a pipe circumferential direction and a pipe longitudinal direction to detect whether or not there is a reading value that indicates 1.5 mm or more.

### Claim 8 (depends on 2)

The heavy wall, high-strength line pipe for sour gas service according to claim 2, wherein the pipe thickness is 20 mm or more and T/D is 0.045 or less (T representing the pipe thickness (mm) and D representing a pipe diameter (mm)).

### Claim 9 (depends on 2, 1000, 1150)

A method for producing a heavy wall, high-strength line pipe for sour gas service, the method comprising reheating a continuously cast slab having the chemical composition according to claims 2 to 1000 to 1150° C.; hot-rolling the reheated slab at a total reduction ratio of 40 to 90% in an un-recrystallized temperature range; conducting accelerated cooling from a surface temperature of Ar3-t ° C. or more (where t represents a plate thickness (mm)) to a temperature in the range of 200 to 400° C., in which cooling from 700 to 600° C. is conducted at an average cooling rate of 200° C./s or less in a portion that extends from a position 1 mm from a front surface to a 3/16 position of the plate thickness and in a portion that extends from a position 1 mm from a rear surface to a 13/16 position of the plate thickness in a plate thickness direction and at a cooling rate of 20° C./s or more at a center in the plate thickness direction; conducting, immediately after the accelerated cooling, reheating to a surface temperature of 525° C. or more and a plate thickness center temperature of 400 to 500° C.; conducting cold working to bend the resulting plate into a pipe; and welding butted portions of two edges to form a welded steel pipe.

### Claim 10 (depends on 5)

The method for producing a heavy wall, high-strength line pipe for sour gas service according to claim 5, wherein a pipe thickness is 20 mm or more and T/D is 0.045 or less (T representing the pipe thickness (mm) and D representing a pipe diameter (mm)).

### Claim 11 (depends on 5)

A method for judging resistance to HIC of a heavy wall, high-strength line pipe for sour gas service, wherein, after a welded steel pipe is produced by the method according to claim 5, samples are cut out from a base metal of the steel pipe and ultrasonic flaw detection is conducted with a 20 MHz or higher probe in a portion that extends from a position 1 mm from an inner surface to a 3/16 position of the pipe thickness and in a portion that extends from a position 1 mm from an outer surface to a 13/16 position of the pipe thickness in a pipe thickness direction, the ultrasonic flaw detection being conducted over a region having an area of at least 200 mm2 in a pipe circumferential direction and a pipe longitudinal direction to detect whether or not there is a reading value that indicates 1.5 mm or more.

### Claim 12 (depends on 6)

A method for judging resistance to HIC of a heavy wall, high-strength line pipe for sour gas service, wherein, after a welded steel pipe is produced by the method according to claim 6, samples are cut out from a base metal of the steel pipe and ultrasonic flaw detection is conducted with a 20 MHz or higher probe in a portion that extends from a position 1 mm from an inner surface to a 3/16 position of the pipe thickness and in a portion that extends from a position 1 mm from an outer surface to a 13/16 position of the pipe thickness in a pipe thickness direction, the ultrasonic flaw detection being conducted over a region having an area of at least 200 mm2 in a pipe circumferential direction and a pipe longitudinal direction to detect whether or not there is a reading value that indicates 1.5 mm or more.