# US 2015/0175848 A1 · Polishing agent, polishing method, and manufacturing method of semiconductor integrated circuit device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0175848 A1
- Document ID: US20150175848A1
- Status: Published application
- Kind: A1
- Application number: 14/566,928
- Filed: 2014-12-11
- Published: 2015-06-25
- Earliest claimed: 2013-12-24
- Assignees: Asahi Glass Company, Limited
- Applicants: Asahi Glass Company, Limited
- Inventors: Yuiko YOSHIDA; Iori Yoshida; Junko Anzai
- Web page: https://patentgrep.com/patent/US20150175848A1

## CPC

- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- B24B 37/044: {characterised by the composition of the lapping agent}
- H10P 52/00: Grinding, lapping or polishing of wafers, substrates or parts of devices
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A first polishing agent contains: cerium oxide particles; and water, wherein, in IR spectrum of the cerium oxide particle, a value A found by a formula below from a ratio (I/I′) between a value I of an absorbance of 3566 cm−1 and a value I′ of an absorbance of 3695 cm−1, and a crystallite diameter XS, is 0.08 or less. A=(I/I′)/XS A second polishing agent contains: cerium oxide particles; and water, wherein, in the cerium oxide particle, a deviation B of a lattice constant found by a formula below from a theoretical lattice constant (a′) and a lattice constant (a) measured by powder X-ray diffraction, is −0.16% or more. B(%)=(1−a/a′)×100

## Claims

### Claim 1

A polishing agent comprising:
cerium oxide particles; and
water,
wherein, in said cerium oxide particle, a value A found by a formula below from a ratio (I/I′) between a value I of an absorbance of 3566 cm−1 and a value I′ of an absorbance of 3695 cm−1, with an absorbance of 3900 cm−1 of an infrared absorption spectrum as a criterion, and a crystallite diameter XS measured by X-ray diffraction is 0.08 or less.
A=(I/I′)/XS

### Claim 2 (depends on 1)

The polishing agent according to claim 1,
wherein the crystallite diameter XS of said cerium oxide particle is 20 nm or more to 60 nm or less.

### Claim 3 (depends on 1)

The polishing agent according to claim 1,
wherein in said cerium oxide particle, a ratio (XS/D) between the crystallite diameter XS and an average primary particle diameter D obtained by a scanning electron microscope is 0.4 or more to 1.0 or less.

### Claim 4 (depends on 3)

The polishing agent according to claim 3,
wherein the average primary particle diameter D of said cerium oxide particles is 30 nm or more to 100 nm or less.

### Claim 5

A polishing agent comprising:
cerium oxide particles; and
water,
wherein, in said cerium oxide particle, a deviation B of a lattice constant found by a formula below from a theoretical lattice constant (a′) and a lattice constant (a) measured by powder X-ray diffraction is −0.16% or more, and an average secondary particle diameter D′ of said cerium oxide particles is 90 nm or more to 500 nm or less.
B(%)=(1−a/a′)×100

### Claim 6 (depends on 5)

The polishing agent according to claim 5,
wherein the average secondary particle diameter D′ of said cerium oxide particles is 95 nm or more to 250 nm or less.

### Claim 7 (depends on 5)

The polishing agent according to claim 5,
wherein the average secondary particle diameter D′ of said cerium oxide particles is 95 nm or more to 200 nm or less.

### Claim 8 (depends on 1)

A polishing method comprising polishing by a relative motion between a surface to be polished and a polishing pad which are brought into contact with each other while a polishing agent is supplied to the polishing pad,
wherein the polishing agent according to claim 1 is supplied to the polishing pad.

### Claim 9 (depends on 5)

A polishing method comprising polishing by a relative motion between a surface to be polished and a polishing pad which are brought into contact with each other while a polishing agent is supplied to the polishing pad,
wherein the polishing agent according to claim 5 is supplied to the polishing pad.

### Claim 10 (depends on 8)

A manufacturing method of a semiconductor integrated circuit device, comprising a step of polishing the surface to be polished by the polishing method according to claim 8.

### Claim 11 (depends on 9)

A manufacturing method of a semiconductor integrated circuit device, comprising a step of polishing the surface to be polished by the polishing method according to claim 9.