# US 2015/0175800 A1 · Epoxy resin composition for semiconductor encapsulation and method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0175800 A1
- Document ID: US20150175800A1
- Status: Published application
- Kind: A1
- Application number: 14/415,231
- Filed: 2013-07-16
- Published: 2015-06-25
- Earliest claimed: 2012-07-19
- Assignees: Nagase Chemtex Corporation
- Applicants: Nagase Chemtex Corporation
- Inventors: Yukari Kouno; Katsushi Kan
- Web page: https://patentgrep.com/patent/US20150175800A1

## CPC

- C08L 63/00: Compositions of epoxy resins; Compositions of derivatives of epoxy resins
- C08G 59/245: {aromatic}
- C08G 59/42: Polycarboxylic acids; Anhydrides, halides or low molecular weight esters thereof
- C08G 59/4223: {aromatic}
- C08G 59/4238: {heterocyclic}
- C08G 59/686: {containing nitrogen}
- C08K 3/36: Silica
- C08L 33/06: of esters containing only carbon, hydrogen and oxygen, which oxygen atoms are present only as part of the carboxyl radical
- H10W 72/071: {Connecting or disconnecting}
- H10W 74/47: comprising organic materials, e.g. plastics or resins
- C08G 2190/00: Compositions for sealing or packing joints
- C08L 2203/206: use in coating or encapsulating of electronic parts
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/325: {Die-attach connectors having a filler embedded in a matrix}
- H10W 72/354: {comprising polymers}
- H10W 74/00: Encapsulations, e.g. protective coatings
- H10W 74/012: {of encapsulations on active surfaces of flip-chip devices, e.g. forming underfills}
- H10W 74/15: on active surfaces of flip-chip devices, e.g. underfills
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

There are provided an epoxy resin composition for encapsulation, which is particularly suitable for use in resin pre-setting type flip-chip mounting of a Cu post chip, and which is capable of suppressing defects due to the generation of voids; and a method for manufacturing a semiconductor device using a Cu post chip. The present invention provides an epoxy resin composition for semiconductor encapsulation for flip-chip mounting, which contains an epoxy resin (A), a curing agent (B), a curing accelerator (C), and 3 to 64 parts by weight, relative to 100 parts by weight of the component (A), of thermally thickening resin particles (D) having a volume-average primary particle diameter of 0.2 to 10 μm; and a method for manufacturing a semiconductor device by resin pre-setting type flip-chip mounting of a Cu post chip using the composition.

## Claims

### Claim 1

An epoxy resin composition for semiconductor encapsulation for flip-chip mounting, the composition containing an epoxy resin (A), a curing agent (B), a curing accelerator (C), and 3 to 64 parts by weight, relative to 100 parts by weight of the component (A), of thermally thickening resin particles (D) having a volume-average primary particle diameter of 0.2 to 10 μm.

### Claim 2 (depends on 1)

The composition according to claim 1, wherein the thermally thickening resin particles (D) are acrylic resin particles.

### Claim 3 (depends on 1)

The composition according to claim 1, wherein the content of the thermally thickening resin particles (D) is 6 to 50 parts by weight.

### Claim 4 (depends on 1)

The composition according to claim 1, wherein the curing agent (B) is an acid anhydride.

### Claim 5 (depends on 1)

The composition according to claim 1, wherein the composition contains 3 to 15 parts by weight of the curing accelerator (C) relative to 100 parts by weight of the epoxy resin (A).

### Claim 6 (depends on 1)

The composition according to claim 1, wherein the composition further contains 30 to 67 parts by weight of an inorganic filler relative to 100 parts by weight of the whole of the resin composition.

### Claim 7 (depends on 1)

The composition according to claim 1, wherein the thickening onset temperature of the composition at a frequency of 1 Hz and a temperature rise rate of 10° C./minute is 50 to 120° C.

### Claim 8 (depends on 7)

The composition according to claim 7, wherein the thickening onset temperature is 60 to 100° C.

### Claim 9 (depends on 1)

The composition according to claim 1, wherein the viscosity of the composition within the range of 15° C. or higher and lower than 50° C. is 1 to 300 Pa·s.

### Claim 10 (depends on 1)

The composition according to claim 1, wherein the flip-chip is a flip-chip having a Cu bump which has a solder layer formed at a tip of a Cu post.

### Claim 11 (depends on 1)

The composition according to claim 1, wherein the flip-chip mounting is resin pre-setting mounting.

### Claim 12

A method for manufacturing a semiconductor device with flip-chip mounting, the method comprising step (1) of supplying a liquid epoxy resin composition for semiconductor encapsulation to an electrode surface of a substrate having an electrode, step (2) of thickening the resin composition by heating the substrate, and step (3) of press-pressurizing a semiconductor chip with a bump formed, against the thickened resin composition under heating, and simultaneously spreading and filling the resin composition in a gap between the substrate and the semiconductor chip.

### Claim 13 (depends on 12)

The method for manufacturing a semiconductor device according to claim 12, wherein the temperature of the resin composition during its supply is 15° C. or higher and lower than 50° C. and the viscosity is 1 to 300 Pa·s in step (1), and the viscosity of the thickened epoxy resin composition is within the range of 10 to 4000 Pa·s in step (2).

### Claim 14 (depends on 12)

The method for manufacturing a semiconductor device according to claim 12, wherein heating conditions include a heating temperature of 50 to 120° C. and a heating time of 1 to 30 minutes in step (2).

### Claim 15 (depends on 12)

The method for manufacturing a semiconductor device according to claim 12, wherein in step (3) the press pressurization is carried out at a pressing rate of 0.01 to 5 mm/s under heating so that the resin temperature during the press pressurization is 150 to 180° C.

### Claim 16 (depends on 12)

The method for manufacturing a semiconductor device according to claim 12, wherein the method further comprises step (4) of electrically connecting the bump to the electrode surface on the substrate and step (5) of heating the resin composition to cure it.

### Claim 17 (depends on 16)

The method for manufacturing a semiconductor device according to claim 16, wherein the bump is a Cu bump which has a solder layer formed at a tip of a Cu post and the substrate having an electrode is a substrate that, excluding its electrode surface, is covered with a solder resist, and wherein heating is conducted to a temperature equal to or higher than a solder melting temperature in step (4).

### Claim 18 (depends on 12)

The method for manufacturing a semiconductor device according to claim 12, wherein the following composition is used as an epoxy resin composition for semiconductor encapsulation:
an epoxy resin composition for semiconductor encapsulation for flip-chip mounting, the composition containing an epoxy resin (A), a curing agent (B), a curing accelerator (C), and 3 to 64 parts by weight, relative to 100 parts by weight of the component (A), of thermally thickening resin particles (D) having a volume-average primary particle diameter of 0.2 to 10 μm.