# US 2015/0175758 A1 · Block copolymer and process for production of heat shrinkable film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0175758 A1
- Document ID: US20150175758A1
- Status: Published application
- Kind: A1
- Application number: 14/605,432
- Filed: 2015-01-26
- Published: 2015-06-25
- Earliest claimed: 2005-09-14
- Assignees: Asahi Kasei Chemicals Corporation
- Applicants: Asahi Kasei Chemicals Corporation
- Inventors: Susumu HOSHI; Ryoko FUKUOKA; Yasutaka NAKAMURA
- Web page: https://patentgrep.com/patent/US20150175758A1

## CPC

- C08J 5/18: Manufacture of films or sheets
- B29C 49/0015: {Making articles of indefinite length, e.g. corrugated tubes}
- C08F 8/04: Reduction, e.g. hydrogenation
- C08F 8/12: Hydrolysis
- C08F 293/00: Macromolecular compounds obtained by polymerisation on to a macromolecule having groups capable of inducing the formation of new polymer chains bound exclusively at one or both ends of the starting macromolecule (on to polymers modified by introduction of unsaturated end groups C08F290/02)
- C08F 297/04: polymerising vinyl aromatic monomers and conjugated dienes
- C08L 51/04: grafted on to rubbers
- C08L 53/02: of vinyl-aromatic monomers and conjugated dienes
- C08L 53/025: {modified}
- B29D 7/01: Films or sheets
- B29K 2025/00: Use of polymers of vinyl-aromatic compounds {or derivatives thereof} as moulding material
- C08J 2353/02: of vinyl aromatic monomers and conjugated dienes
- C08J 2453/02: of vinyl aromatic monomers and conjugated dienes
- C08L 25/08: Copolymers of styrene (C08L29/08, C08L35/06, C08L55/02 take precedence)
- C08L 25/14: with unsaturated esters
- C08L 2201/08: Stabilised against heat, light or radiation or oxydation
- C08L 2201/10: Transparent films; Clear coatings; Transparent materials
- C08L 2203/16: used for films
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- Y10T 428/1331: Single layer [continuous layer]
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention provides a production process of a heat shrinkable film which is transparent, excellent in the balance of physical properties such as rigidity, elongation and shrink properties in both MD and TD, especially has a uniform film thickness and good stability in extrusion molding film while utilizing an inflation method; a block copolymer or hydrogenated product thereof, or a composition composed thereof excellent in tensile properties, optical properties, hardness, stretch properties, molding processability, shrink properties and solvent resistance and therefore suited for extrusion, injection molding and foams. The production process of a heat shrinkable film has a first inflation step of forming a tube having a thickness of from 0.05 to 0.5 mm by using a block copolymer having a vinyl aromatic hydrocarbon content of from 65 to 95 wt. % and a conjugated diene content of from 5 to 35 wt. %, or a hydrogenated product of the block copolymer; and a second inflation step, successively to the first inflation step, stretching the tube to from 1.5 to 5 times the original length in the TD in a fluid of from 65 to 100° C.

## Claims

### Claim at position 1

1-8. (canceled)

### Claim 9

A heat shrinkable film
produced by a first inflation step of forming, at a temperature of from 150 to 250° C., a raw sheet tube having a thickness of from 0.05 to 0.5 mm by using a material which contains a block copolymer having a vinyl aromatic hydrocarbon content of from 65 to 95 wt. % and a conjugated diene content of from 5 to 35 wt. % or hydrogenated product thereof (I) and has a storage elastic modulus (E′), at 50° C., of from 0.7×109 to 2.5×109 Pa; and
a second inflation step, successively to the first inflation step, of stretching the tube to from 1.5 to 5 times the original length in the transverse direction (TD) in a fluid having a viscosity of film, wherein a ratio of the diameter of the raw sheet tube to the diameter of the tube of heat shrinkable film is from 1.5 to 5;
the film having a shrinkage ratio, as measured at 90° C. for 5 seconds, not greater than 20% in the machine direction (MD) and from 20 to 60% in the transverse direction (TD).

### Claim 10

A block copolymer having a vinyl aromatic hydrocarbon content of from 65 to 95 wt. % and a conjugated diene content of from 5 to 35 wt. %, or hydrogenated product thereof (III) having a storage rigidity modulus (E′) at 30° C. of 3×108 Pa or greater, having at least one peak temperature of a loss elastic modulus (E″) within a range of 60° C. or greater but not greater than 110° C., which comprises Component (a) having at least one peak molecular weight, as measured by gel permeation chromatography (GPC), within a range of from 3000 to 300000 and Component (b) polymerized by a trifunctional or higher multifunctional coupling agent and having at least one peak molecular weight within a range exceeding 30000 but not greater than 1000000 at a Component (a)/Component (b) weight ratio of from 10/90 to 90/10.

### Claim 11 (depends on 10)

A block copolymer or hydrogenated product thereof (III) according to claim 10, wherein Component (a) has at least one peak molecular weight within a range of from 50000 to 250000.

### Claim 12 (depends on 10)

A block copolymer or hydrogenated product thereof (III) according to claim 10, wherein Component (b) has at least one peak molecular weight within a range exceeding 350000 but not greater than 900000.

### Claim 13 (depends on 10)

A block copolymer or hydrogenated product thereof (III) according to claim 10, wherein the storage elastic modulus (E′) at 30° C. is 5×108 Pa or greater and the loss elastic modulus (E′) has at least one peak temperature within a range of 65° C. or greater but not greater than 105° C.

### Claim 14 (depends on 10)

A composition comprising a block copolymer or hydrogenated product thereof (III) as claimed in claim 10 and at least one of the following polymers (α) to (ε) as polymer (IV):
(α) a block copolymer composed of a vinyl aromatic hydrocarbon and a conjugated diene or hydrogenated product thereof which does not contain the block copolymer or hydrogenated product thereof (III),
(β) a vinyl aromatic hydrocarbon polymer,
(γ) a copolymer composed of a vinyl aromatic hydrocarbon and an aliphatic unsaturated carboxylic acid derivative, and
(ε) a rubber-modified styrene polymer,
at a (III)/(IV) weight ratio of from 1/99 to 99/1.

### Claim 15 (depends on 14)

A composition according to claim 14, wherein a (E′40/E′20) ratio, that is a ratio of a storage elastic modulus at 40° C. (E′40) to a storage elastic modulus at 20° C. (E′20) is from 0.75 to 1, at least one peak temperature of a function tan δ in measurement of a dynamic viscoelasticity is present within a range of from 70 to 125° C., and a weight ratio of the block copolymer or hydrogenated product thereof (III) to the polymer (IV) is from 5/95 to 95/5.

### Claim 16 (depends on 14)

A composition according to claim 14, which further comprises from 0.01 to 5 parts by weight, based on 100 parts by weight of the block copolymer or hydrogenated product thereof (III) and the polymer (IV), of at least one lubricant selected from fatty acid amides, paraffins, hydrocarbon resins and fatty acids.

### Claim 17 (depends on 14)

A composition according to claim 14, which further comprises from 0.05 to 3 parts by weight, based on 100 parts by weight of the block copolymer or hydrogenated product thereof (III) and the polymer (IV), of at least one stabilizer selected from 2-[1-(2-hydroxy-3,5-di-t-pentylphenyl)ethyl]-4,6-di-t-pentylphenyl acrylate, 2-t-butyl-6-(3-t-butyl-2-hydroxy-5-methylbenzyl)-4-methylphenyl acrylate and 2,4-bis[(octylthio)methyl]-o-cresol.

### Claim 18 (depends on 14)

A composition according to claim 14, which further comprises from 0.05 to 3 parts by weight, based on 100 parts by weight of the block copolymer or hydrogenated product thereof (III) and the polymer (IV), of at least one ultraviolet absorber or light stabilizer selected from benzophenone ultraviolet absorbers, benzotriazole ultraviolet absorbers and hindered amine light stabilizers.

### Claim 19 (depends on 10)

A sheet film comprising the block copolymer or hydrogenated product thereof (III) as claimed in claim 10.

### Claim 20 (depends on 10)

A heat shrinkable film comprising the block copolymer or hydrogenated product thereof (III) as claimed in claim 10.

### Claim 21 (depends on 10)

A heat shrinkable film obtained by a production process comprising a first inflation step of forming a tube having a thickness of from 0.05 to 0.5 mm at a draft ratio of from 1 to 15 by using the block copolymer or hydrogenated product thereof (III) as claimed in claim 10; and a second inflation step, successively to the first inflation step, of stretching the tube to from 1.5 to 5 times the original length in the TD in a fluid of from 65 to 100° C.

### Claim 22 (depends on 14)

A sheet film comprising the composition as claimed in of claim 14.

### Claim 23 (depends on 14)

A heat shrinkable film comprising the composition as claimed in claim 14.

### Claim 24 (depends on 14)

A heat shrinkable film obtained by a production process comprising a first inflation step of forming a tube having a thickness of from 0.05 to 0.5 mm at a draft ratio of from 1 to 15 by using a composition as claimed in claim 14 and a second inflation step, successively to the first inflation step, of stretching the tube to 1.5 to 5 times the original length in the TD in a fluid of from 65 to 100° C.