# US 2015/0175476 A1 · Method for Forming a Smooth Glaze-Like Coating on a Substrate Made of a Ceramic Matrix Composite Material Containing Sic, and Part Made of a Ceramic Material Composite Provided with Such a Coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0175476 A1
- Document ID: US20150175476A1
- Status: Published application
- Kind: A1
- Application number: 14/343,110
- Filed: 2012-08-31
- Published: 2015-06-25
- Earliest claimed: 2011-09-06
- Inventors: Pascal Diss; Lionel Montagne; Sofia Perez-Villar
- Web page: https://patentgrep.com/patent/US20150175476A1

## CPC

- C03C 8/04: containing zinc
- B05D 7/50: {Multilayers}
- C03C 3/091: containing aluminium
- C03C 3/093: containing zinc or zirconium
- C03C 8/02: Frit compositions, i.e. in a powdered or comminuted form
- C03C 8/16: with vehicle or suspending agents, e.g. slip
- C04B 35/565: based on silicon carbide
- C04B 41/009: {characterised by the material treated}
- C04B 41/52: Multiple coating or impregnating {multiple coating or impregnating with the same composition or with compositions only differing in the concentration of the constituents, is classified as single coating or impregnation}
- C04B 41/89: for obtaining at least two superposed coatings having different compositions
- C03C 2205/00: Compositions applicable for the manufacture of vitreous enamels or glazes
- Y10T 428/263: Coating layer not in excess of 5 mils thick or equivalent
- Y10T 428/264: Up to 3 mils
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The method includes depositing on the entire surface of a substrate a refractory cement paste formed by a powder mainly constituted by silica and alumina and mixed with a liquid. The method includes filling the cement paste in hollow portions in a relief of the surface; performing a heat treatment to harden the cement paste after it has set to obtain a first coating layer of refractory cement; and depositing a slip on the first layer, and formed of a glass frit in suspension in a liquid. The method includes performing a heat treatment for glazing by softening and spreading the glass in order to obtain a second coating layer forming a glaze covering the first layer. The composition of the glass frit is selected to form a glass having a glazing temperature lower than 1100° C. and a glass transition temperature lower than 750° C.

## Claims

### Claim at position 1

1-12. (canceled)

### Claim 13

A method of forming a coating having a smooth outside surface of glazed appearance on a substrate of ceramic matrix composite material containing silicon carbide, the method including:
depositing a refractory cement paste on a surface of the substrate, the paste being formed by a powder mainly constituted by silica and alumina and mixed with a liquid, the cement paste filling in the hollow portions in relief of the surface in order to reduce its irregularities and covering the entire surface of the substrate;
performing heat treatment to harden the cement after it has set so as to obtain a first coating layer of refractory cement;
depositing a slip on the first coating layer, the slip being formed of a glass frit in suspension in a liquid, the glass frit being mainly constituted by a powder of silica, boron oxide, alumina, and at least one alkali metal oxide; and
performing heat treatment for glazing by softening and spreading the glass in order to obtain a second coating layer forming a glaze covering the first coating layer;
wherein the composition of the glass frit is selected to form a glass having a glazing temperature lower than 1100° C. and a glass transition temperature lower than 750° C.

### Claim 14 (depends on 13)

A method according to claim 13, wherein a coloring agent is added to the slip.

### Claim 15 (depends on 13)

A method according to claim 13, wherein the liquid of the cement paste is selected from the group consisting of: a solution of sodium silicate; a solution of phosphoric acid; and a solution of aluminum monophosphate (Al(H2PO4)3).

### Claim 16 (depends on 13)

A method according to claim 13, wherein a first coating layer of refractory cement is formed having a minimum thickness of not less than 60 μm.

### Claim 17 (depends on 13)

A method according to claim 13, wherein the glass frit is constituted by powder having a grain size of less than 40 μm.

### Claim 18 (depends on 13)

A method according to claim 13, wherein the composition of the glass frit, in molar percentages, is as follows:
55% to 65% SiO2;
10% to 25% B2O3;
7% to 15% Al2O3;
1% to 12% of at least one alkali metal oxide; and
1% to 20% of at least one oxide selected from the group consisting of: ZrO2, TiO2, V2O5, ZnO, CaO, MgO, and BaO.

### Claim 19 (depends on 13)

A method according to claim 13, wherein the second coating layer forming a glaze has thickness of not less than 100 μm.

### Claim 20

A part comprising a substrate of ceramic matrix composite material containing silicon carbide that is provided on a surface with a coating having a smooth outside surface of glazed appearance, wherein the coating is formed:
of a first coating layer in contact with the surface of the substrate, the first coating layer being made of a refractory cement essentially constituted of silica and of alumina and filling in the hollow portions in relief of the surface in order to reduce its irregularity; and
a second coating layer forming a glaze of glass constituted mainly of oxides of silicon, of boron, of aluminum, and of at least one alkali metal, the glass having a melting temperature lower than 1100° C. and a glass transition temperature lower than 750° C.

### Claim 21 (depends on 20)

A part according to claim 20, wherein the glaze also contains a coloring agent.

### Claim 22 (depends on 20)

A part according to claim 20, wherein the first coating layer of refractory cement has a minimum thickness of not less than 60 μm.

### Claim 23 (depends on 20)

A part according to claim 20, wherein the second coating layer forming a glaze has a thickness of not less than 100 μm.

### Claim 24 (depends on 20)

A part according to claim 20, wherein the composition of the glass of the glaze in molar percentages is as follows:
55% to 65% SiO2;
10% to 25% B2O3;
7% to 15% Al2O3;
1% to 12% of at least one alkali metal oxide; and
1% to 20% of at least one oxide selected from the group consisting of: ZrO2, TiO2, V2O5, ZnO, CaO, MgO, and BaO.