# US 2015/0148911 A1 · Method for manufacturing bone implants and bone implant

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0148911 A1
- Document ID: US20150148911A1
- Status: Published application
- Kind: A1
- Application number: 14/411,881
- Filed: 2013-06-27
- Published: 2015-05-28
- Earliest claimed: 2012-06-27
- Assignees: Instytut Wysokich Cisnien Polskiej Akademii Nauk
- Inventors: Witold Lojkowski; Tadeusz Chudoba; Elzbieta Pietrzykowska; Aleksandra Kedzierska; Dariusz Smolen; Wojciech Swieszkowski; Krzysztof Kurzydlowski
- Web page: https://patentgrep.com/patent/US20150148911A1

## CPC

- A61F 2/28: Bones
- A61L 27/12: Phosphorus-containing materials, e.g. apatite
- C04B 35/447: based on phosphates {, e.g. hydroxyapatite}
- C04B 35/62655: {Drying, e.g. freeze-drying, spray-drying, microwave or supercritical drying}
- C04B 35/645: Pressure sintering
- A61F 2310/00293: containing a phosphorus-containing compound, e.g. apatite
- A61L 2400/12: Nanosized materials, e.g. nanofibres, nanoparticles, nanowires, nanotubes; Nanostructured surfaces
- C04B 2235/3212: Calcium phosphates, e.g. hydroxyapatite
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/604: Pressing at temperatures other than sintering temperatures
- C04B 2235/6562: Heating rate
- C04B 2235/6567: Treatment time
- C04B 2235/662: Annealing after sintering
- C04B 2235/767: Hexagonal symmetry, e.g. beta-Si3N4, beta-Sialon, alpha-SiC or hexa-ferrites
- C04B 2235/77: Density
- C04B 2235/781: Nanograined materials, i.e. having grain sizes below 100 nm
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- A61F: FILTERS IMPLANTABLE INTO BLOOD VESSELS; PROSTHESES; DEVICES PROVIDING PATENCY TO, OR PREVENTING COLLAPSING OF, TUBULAR STRUCTURES OF THE BODY, e.g. STENTS; ORTHOPAEDIC, NURSING OR CONTRACEPTIVE DEVICES; FOMENTATION; TREATMENT OR PROTECTION OF EYES OR EARS; BANDAGES, DRESSINGS OR ABSORBENT PADS; FIRST-AID KITS (dental prosthetics A61C)
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

To manufacture the implant a nanopowder of synthetic hydroxyapatite (Hap) is used having a hexagonal structure, average grain size in a range from 3 to 30 nm and the specific surface area greater than 200 m2/g. First the nanopowder is formed to the desired geometric shape, and then the shape is fixed. In the step of shape information the dried nanopowder is pressed in the mold under the pressure ranging from 50 Mpa to 2 GPa. In the step of fixing the pressed nanopowder at room temperature is subjected to the pressure rising from the ambient value to the peak value selected from a range of 1 to 8 GPa and to a temperature selected from a range of 100° C. to 600° C. for a period of time selected from a range from 30 seconds to 5 minutes. The density of thus produced implant, determined by helium method, is not less than 75% of the theoretical density.

## Claims

### Claim 1

A method for manufacturing bone implants using hydroxyapatite (HAp),
comprising a step of formation of HAp powder into a desired geometric shape, and a step of fixing the formed shape, characterized in that for the implant manufacturing a powdered synthetic hydroxyapatite is used having hexagonal structure, average grain size in a range from 3 to 30 nm and specific surface area greater than 200 m2/g, wherein during the step of formation the nanopowder is dried at
a temperature not exceeding 300° C. for at least one minute and then the drained nanopowder is compressed in a mold of desired geometric shape at a pressure ranging from 50 MPa to 2 GPa, while in the step of fixing the pressed nanopowder at a room temperature is subjected to a pressure rising from the ambient value to the peak value selected from a range from 1 to 8 GPa and to a temperature selected from a range of 100° C. to 600° C. for a period selected from a range of 30 seconds to 5 minutes.

### Claim 2 (depends on 1)

The method according to claim 1, characterized by the fact that in the step of fixing the pressed nanopowder is first subjected to the increasing pressure, and nest the desired peak value of the pressure is maintained, the nanopowder is heated to the desired temperature and that temperature is maintained for a selected period of time.

### Claim 3 (depends on 1)

The method according to claim 1, wherein in the step of fixing the pressed nanopowder is heated to a desired temperature and at the same time the pressure is being raised, and then the desired peak value of the pressure is maintained, and the pressed nanopowder is kept in a given temperature for a selected period of time.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the rate of pressure rise in the step of fixing is at least 5 MPa per second.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the rate of temperature rise in the step of fixing is at least 1° C. per second.

### Claim 6

A bone implant of hydroxyapatite (HAp), characterized in that its density determined by helium method is not less than 75% of the theoretical density, the average grain size of the material forming the implant determined on the basis of the PN-EN standard is not larger than 50 nm, nanohardness of this material, measured by Berkovich indenter using a load of 4 mN, is not less than 3 GPa, and solubility, determined according to ISO 10993-4 norm, is from 5 to 35 mg/dm3.

### Claim 7 (depends on 1)

The bone implant of hydroxyapatite (HAp), wherein its density determined by helium method is not less than 75% of the theoretical density, the average grain size of the material forming the implant determined on the basis of the PN-EN standard is not larger than 50 nm, nanohardness of this material, measured by Berkovich indenter using a load of 4 mN, is not less than 3 GPa, and solubility, determined according to ISO 10993-4 norm, is from 5 to 35 mg/dm3, characterized by the fact that it manufactured by the method according to claim 1.