# US 2015/0148515 A1 · Polyester resin and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0148515 A1
- Document ID: US20150148515A1
- Status: Published application
- Kind: A1
- Application number: 14/405,189
- Filed: 2013-05-21
- Published: 2015-05-28
- Earliest claimed: 2012-06-05
- Assignees: SK Chemicals Co., Ltd.
- Applicants: SK Chemicals Co., Ltd.
- Inventors: Ji-Hyun Kim; Yoo Jin Lee
- Web page: https://patentgrep.com/patent/US20150148515A1

## CPC

- C08G 63/199: Acids or hydroxy compounds containing cycloaliphatic rings
- C08G 63/672: Dicarboxylic acids and dihydroxy compounds
- C08G 63/83: Alkali metals, alkaline earth metals, beryllium, magnesium, copper, silver, gold, zinc, cadmium, mercury, manganese, or compounds thereof {(C08G63/823 takes precedence)}
- C08G 63/863: {Germanium or compounds thereof}
- C08K 5/49: Phosphorus-containing compounds {(C08K5/0091 takes precedence)}
- C08L 67/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08L67/06 takes precedence)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

There is provided a polyester resin including: moieties of dicarboxylic acid components including terephthalic acid; and moieties of diol components including 5 to 60 mole % of isosorbide, 10 to 80 mole % of a cyclohexanedimethanol, and the balance of other diol compounds, wherein the polyester resin has an intrinsic viscosity of 0.5 to 1.0 dl/g and oxygen permeability of less than 20 cc*mm/(m2*day*atm), as measured by ASTM D 3985, and There is also provided a method for preparing the polyester resin, including: esterifying diol components including 5 to 60 mole % of isosorbide, 10 to 80 mole % of a cyclohexanedimethanol, and the balance of other diol compounds, with dicarboxylic acid components including terephthalic acid in the presence of an esterification reaction catalyst including a zinc compound; adding a phosphorus-based stabilizer to the esterification reaction mixture at the time when the degree of esterification reaches at least 80%; and subjecting the esterification reaction product to polycondensation.

## Claims

### Claim 1

A polyester resin comprising:
moieties of dicarboxylic acid components comprising terephthalic acid; and
moieties of diol components comprising 5 to 60 mole % of isosorbide, 10 to 80 mole % of a cyclohexanedimethanol, and the balance of other diol compounds,
wherein the polyester resin has an intrinsic viscosity of 0.5 to 1.0 dl/g, and oxygen permeability of less than 20 cc*mm/(m2*day*atm), as measured by ASTM D 3985.

### Claim 2 (depends on 1)

The polyester resin according to claim 1,
wherein the polyester resin contains 1 to 100 ppm of a zinc-based catalyst, in terms of the central metal atom content, based on the total amount of the resin, and 10 ppm to 300 ppm of a phosphorus-based stabilizer.

### Claim 3 (depends on 1)

The polyester resin according to claim 1,
wherein the other diol compounds comprise at least one compound selected from the group consisting of aliphatic diol compounds and aromatic diol compounds.

### Claim 4 (depends on 1)

The polyester resin according to claim 1,
wherein the phosphorus-based stabilizer comprises at least one compound selected from the group consisting of phosphoric acid, trimethyl phosphate, triethyl phosphate, triphenyl phosphate, and triethyl phosphonoacetate.

### Claim 5 (depends on 1)

The polyester resin according to claim 1,
wherein the zinc-based catalyst comprises at least one compound selected from the group consisting of zinc acetate, zinc acetate dihydrate, zinc chloride, zinc sulfate, zinc sulfide, zinc carbonate, zinc citrate, and zinc gluconate.

### Claim 6 (depends on 1)

The polyester resin according to claim 1,
further comprising 1 to 100 ppm of at least one polycondensation reaction catalyst selected from the group consisting of titanium compounds, germanium compounds, antimony compounds, aluminum compounds, and tin compounds, based on the total amount of the resin.

### Claim 7 (depends on 1)

A method for preparing the polyester resin according to claim 1, the method comprising:
esterifying diol components comprising 5 to 60 mole % of isosorbide, 10 to 80 mole % of a cyclohexanedimethanol, and the balance of other diol compounds, with dicarboxylic acid components comprising terephthalic acid, in the presence of an esterification reaction catalyst comprising a zinc compound;
adding a phosphorus-based stabilizer to the esterification reaction mixture at the time when the degree of esterification reaches at least 80%; and
subjecting the esterification reaction product to polycondensation.

### Claim 8 (depends on 7)

The method according to claim 7,
wherein the amount of the diol components or dicarboxylic acid components remaining unreacted without participating in the esterification reaction is less than 20%.

### Claim 9 (depends on 7)

The method according to claim 7,
wherein the phosphorus-based stabilizer is used in an amount of 10 ppm to 300 ppm, based on the weight of the resin.

### Claim 10 (depends on 7)

The method according to claim 7,
wherein the molar ratio between the dicarboxylic acid components and the diol components in the esterification reaction is from 1:1.05 to 1:3.0.

### Claim 11 (depends on 7)

The method according to claim 7,
wherein the esterification reaction is carried out at a pressure of 0 to 10.0 kg/cm2 and a temperature of 150 to 300° C.

### Claim 12 (depends on 7)

The method according to claim 7,
wherein the esterification reaction is carried out for 200 to 330 minutes.

### Claim 13 (depends on 7)

The method according to claim 7,
wherein the polycondensation reaction is carried out at a temperature of 150 to 300° C. and a reduced pressure of 600 to 0.01 mmHg for 1 to 24 hours.

### Claim 14 (depends on 7)

The method according to claim 7,
further comprising adding at least one catalyst compound selected from the group consisting of titanium compounds, germanium compounds, antimony compounds, aluminum compounds, and tin compounds.