# US 2015/0148475 A1 · (meth)acrylic, propene co-polymers and a method for their production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0148475 A1
- Document ID: US20150148475A1
- Status: Published application
- Kind: A1
- Application number: 14/543,036
- Filed: 2014-11-17
- Published: 2015-05-28
- Earliest claimed: 2013-11-22
- Assignees: Rohm and Haas Company
- Applicants: Rohm and Haas Company
- Inventors: C. Damien Rodowski; Charles J. Rand; Barry Weinstein; James DeFelippis
- Web page: https://patentgrep.com/patent/US20150148475A1

## CPC

- C08F 220/06: Acrylic acid; Methacrylic acid; Metal salts or ammonium salts thereof
- C08F 220/08: Anhydrides
- C08J 3/00: Processes of treating or compounding macromolecular substances
- C08K 3/32: Phosphorus-containing compounds
- C08K 5/53: bound to oxygen and to carbon only
- C08K 5/5313: Phosphinic compounds, e.g. R2=P(:O)OR'
- C08K 5/5317: Phosphonic compounds, e.g. R—P(:O)(OR')2
- C08L 33/02: Homopolymers or copolymers of acids; Metal or ammonium salts thereof
- C08L 33/08: Homopolymers or copolymers of acrylic acid esters
- C08L 33/10: Homopolymers or copolymers of methacrylic acid esters
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention provides telomeric copolymers of acrylic and methacrylic acid which further comprise an olefin polymerization residue and have one or more phosphorus acid groups wherein the phosphorus acid group comprises one or more phosphorus atom in the +1 oxidation state or in the +3 oxidation state, or both. In addition the present invention provides methods of making the telomeric copolymers comprising aqueous solution copolymerizing a monomer mixture comprising acrylic acid and methacrylic acid in the presence of a phosphorus acid group containing reactant having a phosphorus atom in the +1 oxidation state, and thermally treating the resulting telomeric copolymer at 175° C. or higher for a sufficient time to decarboxylate the copolymer.

## Claims

### Claim 1

A copolymer composition comprising a phosphorus acid group containing telomeric copolymer of acrylic acid and methacrylic acid and/or salts thereof having a weight average molecular weight (Mw) of up to 20,000, and having an average of (i) from 19 to 74 wt. % of the copolymerization residue of methacrylic acid, anhydride, or its salts, (ii) from 1 to 20 wt. % of phosphorus acid groups chosen from hypophosphite, phosphite, alkyl phosphinate, alkyl phosphonate, dialkyl phosphinate, and mixtures thereof, (iii) from 0 to 20 wt. % of the copolymerization residue of a third vinyl monomer, and (iv) from 25 to 80 wt. % of the copolymerization residue of acrylic acid, anhydride, or its salts, the wt. % of all monomers and phosphorus acid group forming reactants being based on the total weight of reactants used to make the telomeric copolymer, wherein the telomeric copolymer comprises at least one copolymerization residue of propene (—CH2—CH(CH3)—).

### Claim 2 (depends on 1)

The copolymer composition as claimed in claim 1, wherein the telomeric copolymer has a weight average molecular weight (Mw) of from 1,000 to 16,000.

### Claim 3 (depends on 1)

The copolymer composition as claimed in claim 1, wherein the telomeric copolymer has an average of (iv) from 40 to 62 wt. % of the copolymerization residue of acrylic acid, anhydride, or its salts, the wt. % of all monomers and phosphorus acid group forming reactants being based on the total weight of reactants used to make the telomeric copolymer.

### Claim 4 (depends on 1)

The copolymer composition as claimed in claim 1, wherein the telomeric copolymer comprises the copolymerization residue of (iii) a third vinyl monomer which is resistant to hydrolysis or which can provide desirable flow properties under processing conditions and which is chosen from a an acrylic or other vinyl comonomer.

### Claim 5 (depends on 4)

The copolymer composition as claimed in claim 4, wherein (iii) the third vinyl monomer is chosen from itaconic acid, methacrylamide, acrylomorpholine, acrylamide, C1 to C6 alkyl (meth)acrylamides, C1 to C6 dialkyl (meth)acrylamides, styrene, alpha-methyl styrene, sulfonated styrene and its alkali metal salts, cyanostyrene, hydroxystyrene, acrylonitrile, isopropylacrylamide, t-butylacrylamide, sulfonated acrylamide, and its alkali metal salts.

### Claim 6 (depends on 1)

The copolymer composition as claimed in claim 1, wherein the telomeric copolymer comprises from 75 wt. % to 100 wt. % of the total copolymerization residues of acrylic, methacrylic acid, anhydride thereof, salts thereof and propene (—CH2—CH(CH3)—, based on based on the total weight of monomers used to make the telomeric copolymer.

### Claim 7 (depends on 1)

The copolymer composition as claimed in claim 1, wherein the telomeric copolymers comprise powders, pellets, granules or suspensions thereof in non-aqueous carriers.

### Claim 8 (depends on 1)

A method of making a telomeric copolymer composition as claimed in claim 1 comprising copolymerizing in an aqueous medium (i) from 19 to 74 wt. % of methacrylic acid, or its salts, (ii) from 1 to 20 wt. % of a phosphorus acid group containing reactant having at least one phosphorus atom in the +1 oxidation state, the phosphorus acid groups being chosen from sodium hypophosphite, hypophosphorous acid and its salts, phosphinic acid and its salts, phenylphosphinic acid, alkyl phosphinate, alkyl phosphonate, dialkyl phosphinate, and mixtures thereof, (iii) from 0 to 20 wt. % of a third vinyl monomer, and (iv) from 25 to 80 wt. % of acrylic acid, or its salts, the wt. % of all monomers and phosphorus acid group reactants being based on the total weight of reactants used to make the telomeric copolymer, thermally treating the telomeric copolymer to a temperature ranging from 175° C. to 230° C. for a sufficient time to cause offgassing, thereby facilitating decarboxylation of the telomeric copolymer.

### Claim 9 (depends on 8)

The method of making a telomeric copolymer composition as claimed in claim 8, wherein the thermally treating of the telomeric copolymer is carried out in presence of a radical quenching agent or an anti-oxidant.

### Claim 10 (depends on 8)

The method of making a telomeric copolymer composition as claimed in claim 8, wherein the thermally treating of the telomeric copolymer is carried out under shear.