# US 2015/0148437 A1 · Mineral-filled polypropylene composition for foaming

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0148437 A1
- Document ID: US20150148437A1
- Status: Published application
- Kind: A1
- Application number: 14/403,856
- Filed: 2013-05-22
- Published: 2015-05-28
- Earliest claimed: 2012-06-01
- Assignees: Basell Poliolefine Italia S.r.l.
- Applicants: Basell Poliolefine Italia S.r.l.
- Inventors: Dieter Langenfelder; Jürgen Rohrmann
- Web page: https://patentgrep.com/patent/US20150148437A1

## CPC

- C08J 9/0061: {characterized by the use of several polymeric components}
- C08J 9/0028: {containing nitrogen}
- C08J 9/0066: {Use of inorganic compounding ingredients}
- C08J 9/122: {Hydrogen, oxygen, CO2, nitrogen or noble gases}
- C08K 3/34: Silicon-containing compounds
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08L 23/10: Homopolymers or copolymers of propene
- C08L 23/12: Polypropene
- C08L 23/14: Copolymers of propene (C08L23/16 takes precedence)
- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C09J 107/02: Latex
- C08J 2203/06: CO2, N2 or noble gases
- C08J 2323/10: Homopolymers or copolymers of propene
- C08J 2323/14: Copolymers of propene (C08J2323/16 takes precedence)
- C08J 2423/06: Polyethene
- C08J 2423/14: Copolymers of propene (C08J2423/16 takes precedence)
- C08J 2423/16: Ethene-propene or ethene-propene-diene copolymers
- C08J 2423/20: having four to nine carbon atoms
- C08K 3/04: Carbon
- C08L 23/06: Polyethylene
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2207/02: Heterophasic composition
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

The present invention relates to a new polypropylene composition for the production of foamed molded articles, such as finished parts for the automotive industry.

## Claims

### Claim 1

A composition comprising:
(A) from 30 to 85% by weight of one or more propylene-based components being selected from the group consisting of propylene homopolymers, propylene copolymers and heterophasic propylene polymer, such first propylene-based component having a flexural modulus determined in accordance with ISO 178 higher than 800 MPa;
(B) from 1 to 20% by weight of a heterophasic propylene polymer comprising:
(B1) from 20 to 90% by weight of a crystalline polypropylene;
(B2) from 10 to 80% by weight, preferably from 15 to 60% by weight, of a copolymer of ethylene and at least one C3-C10 alpha-olefin, such copolymer containing from 10 to 70% by weight of ethylene, being soluble in xylene at room temperature, and having an intrinsic viscosity in tetrahydronaphtalene at 135° C. from 3.5 dl/g, to 8 dl/g;
(C) from 1 to 30% by weight, of an ethylene-based plastomer, having a hardness (Shore A, ASTM D-2240) value equal to or lower than 90 points;
(D) from 5 to 30% by weight of talc.
(E) from 1 to 10%, by weight of high-density polyethylene (HDPE); and
(F) from 0.1 to 1.5% by weight of an anti-scratch additive.

### Claim 2 (depends on 1)

The composition according to claim 1, wherein the copolymer (B2) has an intrinsic viscosity in tetrahydronaphtalene at 135° C. of from 5 to 8 dl/g.

### Claim 3 (depends on 1)

The composition according to claim 1, wherein the component (B) comprises (percent by weight):
A) 20%-90% of a crystalline polypropylene component containing from 25% to 75% of a fraction AI having a melt flow rate MFRI of from 0.5 to 10 g/10 min., and from 75% to 25% of a fraction AII having a melt flow rate MFRII such that a ratio MFRI/MFRI is from 30 to 2000; and wherein fractions AI and AII are independently selected from the group consisting of a propylene homopolymer, a random copolymer of propylene containing up to 8% of ethylene, and a random copolymer of propylene containing up to 8% of at least one C4-C10 alpha-olefin; and
B) 10%-80% of a copolymer component of ethylene and at least one C3-C10 alpha-olefin, the copolymer containing from 10 to 70% of ethylene, and optionally minor amounts of a diene, said copolymer being soluble in xylene at room temperature, and having an intrinsic viscosity in tetrahydronaphtalene at 135° C. from 4 to 9 dl/g.

### Claim 4 (depends on 1)

The composition according to claim 1, wherein the component (B) comprises (percent by weight):
A) 50-90% of a crystalline polypropylene component comprising:
AI) from 25 to 75% of a fraction having a melt flow rate MFRI of from 0.1 to 10 g/10 min.; and
AII) from 25 to 75% of a fraction having a melt flow rate value MFRII equal to or lower than 100 g/10 min.;
wherein the ratio MFRII/MFRI is from 5 to 60, and the fractions (AI) and (AII) are independently selected from the group consisting of a propylene homopolymer, a random copolymer of propylene containing up to 3% of ethylene, and a random copolymer of propylene containing up to 6% of at least one C4-C10 alpha-olefin; and
B) 10%-50% of a copolymer component of ethylene and at least one C3-C10 alpha-olefin, the copolymer containing from 15% to 50% of ethylene and optionally minor amounts of a diene;
said composition having a value of the intrinsic viscosity of the fraction soluble in xylene at room temperature (about 25° C.) equal to or higher than 3.5 dl/g.

### Claim 5 (depends on 1)

The composition according to claim 1, wherein the anti-scratch additive is selected from the group consisting of erucamide, oleamide and polydimethylsiloxane.

### Claim 6 (depends on 1)

The composition according to claim 1, having a melt flow rate value (ISO 1133—230° C., 2.16 Kg) of from 10 to 150 g/10 min.

### Claim 7 (depends on 1)

A foamed article comprising the composition of claim 1.

### Claim 8

(canceled)

### Claim 9 (depends on 7)

A vehicle comprising the foamed article of claim 7.