# US 2015/0148433 A1 · Method for fabricating three-dimensional network structure material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0148433 A1
- Document ID: US20150148433A1
- Status: Published application
- Kind: A1
- Application number: 14/517,439
- Filed: 2014-10-17
- Published: 2015-05-28
- Earliest claimed: 2013-11-25
- Assignees: Taiwan Carbon Nanotube Technology Corporation
- Applicants: Taiwan Carbon Nanotube Technology Corporation
- Inventors: Chun-Hsien Tsai; Chun-Jung Tsai; Ting-Chuan Lee; Ching-Tung HSU; Chia-Hung LI; Wan-Ju CHEN; Jui-Yu Jao
- Web page: https://patentgrep.com/patent/US20150148433A1

## CPC

- B01J 13/0065: {containing an organic phase}
- A61L 26/0023: {Polysaccharides}
- A61L 26/008: {Hydrogels or hydrocolloids}
- B01J 13/0091: {Preparation of aerogels, e.g. xerogels}
- B01J 20/28047: {Gels}
- C08L 1/286: {substituted with acid radicals, e.g. carboxymethyl cellulose [CMC] (C08L1/282 takes precedence)}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A method for fabricating a three-dimensional network structure material comprises steps: mixing ammonium carboxymethyl cellulose with water or with water and a nanomaterial to form a first gel or a second gel; freeze-drying the first gel or the second gel to sublimate the first gel or the second gel and form a first product or a second product; and heating the first product or the second product at a lower temperature to cure the first product or the second product and obtain a first 3D network structure material or a second 3D network structure material. The present invention uses a simple process using water as the solvent, meeting the environment protection demand and having high economical efficiency. The first and second 3D network structure materials fabricated by the present invention absorb water but do not dissolve in water. Thus, the present invention can be applied to many fields.

## Claims

### Claim 1

A method for fabricating a three-dimensional network structure material, comprising
Step 1: mixing ammonium carboxymethyl cellulose with water to fabricate a first gel;
Step 2: undertaking a freeze-drying process of the first gel to sublimate the first gel and remove water from the first gel to obtain a first product; and
Step 3: undertaking a low-temperature heating process of the first product at a temperature between 50° C. and 380° C. to cure the first product and obtain a first three-dimensional network structure material.

### Claim 2 (depends on 1)

The method for fabricating a three-dimensional network structure material according to claim 1, wherein in Step 1, a weight ratio of ammonium carboxymethyl cellulose to water is between 0.1:100 and 50:100.

### Claim 3 (depends on 1)

The method for fabricating a three-dimensional network structure material according to claim 1, wherein a freeze-drying temperature of the freeze-drying process is between 0° C. and −200° C.

### Claim 4 (depends on 1)

The method for fabricating a three-dimensional network structure material according to claim 1, wherein a heating temperature of the low-temperature heating process is between 80° C. and 350° C., and wherein a time interval of the low-temperature heating process is between 1 minute and 10 hours.

### Claim 5 (depends on 1)

The method for fabricating a three-dimensional network structure material according to claim 1, wherein in Step 1, a first surfactant is added to the ammonium carboxymethyl cellulose and water in fabricating the first gel, and wherein the first surfactant is sodium dodecyl sulfate or sodium dodecyl sulphonate.

### Claim 6 (depends on 5)

The method for fabricating a three-dimensional network structure material according to claim 5, wherein a weight ratio of ammonium carboxymethyl cellulose to water is between 0.1:100 and 80:100; a weight ratio of the first surfactant to water is between 0.01:100 and 50:100.

### Claim 7 (depends on 1)

The method for fabricating a three-dimensional network structure material according to claim 1, wherein in Step 1, glycerol is added to ammonium carboxymethyl cellulose and water in fabricating the first gel, and wherein a weight ratio of glycerol to ammonium carboxymethyl cellulose is between 0.01:1 and 5:1.

### Claim 8

A method for fabricating a three-dimensional network structure material, comprising
Step A: mixing a nanomaterial and ammonium carboxymethyl cellulose with water to fabricate a second gel;
Step B: undertaking a freeze-drying process of the second gel to sublimate the second gel and remove water from the second gel to obtain a second product; and
Step C: undertaking a low-temperature heating process of the second product at a temperature between 50° C. and 380° C. to cure the second product and obtain a second three-dimensional network structure material.

### Claim 9 (depends on 8)

The method for fabricating a three-dimensional network structure material according to claim 8, wherein in Step A, the nanomaterial is mixed with water to form an aqueous dispersion liquid; next, ammonium carboxymethyl cellulose is added to the aqueous dispersion liquid to fabricate the second gel.

### Claim 10 (depends on 9)

The method for fabricating a three-dimensional network structure material according to claim 9, wherein in Step A, a weight ratio of the nanomaterial to water is between 0.01:100 and 50:100; a weight ratio of ammonium carboxymethyl cellulose to the aqueous dispersion liquid is between 0.1:100 and 50:100.

### Claim 11 (depends on 8)

The method for fabricating a three-dimensional network structure material according to claim 8, wherein in Step A, the nanomaterial is acidified to form an acidified nanomaterial; next, the acidified nanomaterial is mixed with ammonium carboxymethyl cellulose and water to fabricate the second gel.

### Claim 12 (depends on 11)

The method for fabricating a three-dimensional network structure material according to claim 11, wherein in Step A, a weight ratio of the nanomaterial to water is between 0.01:100 and 50:100; a weight ratio of ammonium carboxymethyl cellulose to water is between 0.1:100 and 80:100.

### Claim 13 (depends on 8)

The method for fabricating a three-dimensional network structure material according to claim 8, wherein in Step A, a second surfactant is mixed with the nanomaterial, ammonium carboxymethyl cellulose and water and to fabricate the second gel, and wherein the second surfactant is sodium dodecyl sulfate or sodium dodecyl sulphonate.

### Claim 14 (depends on 13)

The method for fabricating a three-dimensional network structure material according to claim 13, wherein in Step A, a weight ratio of the nanomaterial to water is between 0.01:100 and 50:100; a weight ratio of ammonium carboxymethyl cellulose to water is between 0.1:100 and 80:100; a weight ratio of the second surfactant to water is between 0.01:100 and 50:100.

### Claim 15 (depends on 8)

The method for fabricating a three-dimensional network structure material according to claim 8, wherein a freeze-drying temperature of the freeze-drying process is between 0° C. and −200° C.

### Claim 16 (depends on 8)

The method for fabricating a three-dimensional network structure material according to claim 8, wherein a heating temperature of the low-temperature heating process is between 80° C. and 350° C., and wherein a time interval of the low-temperature heating process is between 1 minute and 10 hours.

### Claim 17 (depends on 8)

The method for fabricating a three-dimensional network structure material according to claim 8, wherein in Step A, glycerol is added to the nanomaterial, ammonium carboxymethyl cellulose and water in fabricating the second gel, and wherein a weight ratio of glycerol to ammonium carboxymethyl cellulose is between 0.01:1 and 5:1.

### Claim 18 (depends on 8)

The method for fabricating a three-dimensional network structure material according to claim 8, wherein the nanomaterial is selected from a group consisting of carbon nanotubes, graphene, and carbon nanoribbons.