# US 2015/0148236 A1 · Laser processing of superconductor layers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0148236 A1
- Document ID: US20150148236A1
- Status: Published application
- Kind: A1
- Application number: 14/092,296
- Filed: 2013-11-27
- Published: 2015-05-28
- Earliest claimed: 2013-11-27
- Assignees: Varian Semiconductor Equipment Associates, Inc.
- Applicants: Varian Semiconductor Equipment Associates, Inc.
- Inventors: Connie P. Wang; Paul Murphy; Paul Sullivan; Sukti Chatterjee
- Web page: https://patentgrep.com/patent/US20150148236A1

## CPC

- H10N 60/858: {having multilayered structures, e.g. superlattices}
- H10N 60/0661: {Processes performed after copper oxide formation, e.g. patterning}
- H10N 60/0884: {Treatment of superconductor layers by irradiation, e.g. ion-beam, electron-beam, laser beam or X-rays}
- Y10T 428/24174: including sheet or component perpendicular to plane of web or sheet
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method of forming a superconductor includes exposing a layer disposed on a substrate to an oxygen ambient, and selectively annealing a portion of the layer to form a superconducting region within the layer.

## Claims

### Claim 1

A method of forming a superconductor, the method comprising
exposing a layer disposed on a substrate to an oxygen ambient; and
selectively annealing a portion of the layer to form a superconducting region within the layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the superconducting region has higher critical current than a first region outside of the superconducting region.

### Claim 3 (depends on 2)

The method of claim 2, wherein the superconducting region and the first region have at least three elements in common.

### Claim 4 (depends on 2)

The method of claim 2, wherein the superconducting region and the first region have different crystalline orientations.

### Claim 5 (depends on 1)

The method of claim 1, wherein the selectively annealing comprises directing a laser beam to the portion of the layer from a laser source comprising a CO2-laser, an excimer XeCl laser, N2 laser, Cu vapor laser, or Nd:YAG pulse laser.

### Claim 6 (depends on 5)

The method of claim 5, further comprising scanning the laser beam with respect to the substrate to define the superconductor region in the layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein the layer comprises amorphous material or randomly oriented polycrystalline superconductor crystallites, wherein after the selective annealing the superconductor region comprises superconductor material having a high degree of c-axis preferred orientation in which the crystallites have their c-axes oriented perpendicularly to a plane of the substrate.

### Claim 8 (depends on 1)

The method of claim 1, wherein the layer comprises ReBCO where Re is a rare earth element, wherein before the selectively annealing the portion comprises a set of regions in which crystallites of the layer have their c-axes oriented parallel to a plane of the substrate, wherein after the selectively annealing the superconductor region comprises superconductor material having a high degree of preferred c-axis orientation in which the crystallites have their c-axes oriented perpendicularly to the plane of the substrate.

### Claim 9 (depends on 1)

The method of claim 1, wherein the substrate comprises a set of raised features having sidewalls, and wherein the layer comprises superconductor material disposed on the sidewalls.

### Claim 10 (depends on 1)

The method of claim 1, wherein the selectively annealing comprises generating a temperature of the portion of the layer of greater than 400° C.

### Claim 11 (depends on 1)

The method of claim 1, further comprising:
providing the substrate as a substrate base; and
forming a buffer layer on the substrate base that is operative to generate a c-axis orientation to the selectively annealed portion in which the crystallites have their c-axes oriented perpendicularly to the plane of the substrate.

### Claim 12 (depends on 11)

The method of claim 11, wherein the substrate base comprises a silicon-on-insulator (SOI) substrate wherein a silicon layer of the SOI substrate comprises a thickness less than 10 micrometers.

### Claim 13

A method of forming a superconductor region in a layer disposed on a surface of a substrate, comprising:
directing a laser beam to the surface;
providing an oxygen ambient to the surface; and
moving the substrate with respect to the laser beam to generate a selectively annealed region in the layer, wherein the selectively annealed region comprises superconductor material having a c-axis orientation in which the c-axes of the crystallites are aligned perpendicularly to a plane of the substrate, wherein a first region of the layer disposed outside the selectively annealed region does not comprise a superconductor material having a c-axis orientation.

### Claim 14 (depends on 13)

The method of claim 13, wherein the layer comprises a material in the ReBCO family of material where Re is a rare earth element and the selectively annealed region comprises a set of regions in which crystallites of the layer have their c-axes oriented parallel to a plane of the substrate before the directing the laser beam.

### Claim 15 (depends on 13)

The method of claim 13, wherein the substrate comprises a set of raised features having sidewalls, and the selectively annealed region comprises superconductor material disposed on the sidewalls.

### Claim 16 (depends on 15)

The method of claim 15, further comprising forming a metal on a portion of the layer including the superconductor material disposed on the sidewalls.

### Claim 17 (depends on 13)

The method of claim 13, further comprising, before the directing the laser beam:
forming on a substrate base of the substrate a buffer layer configured to generate epitaxial growth of the superconductor layer; and
depositing the superconductor layer as a poorly crystalline or amorphous layer having a thickness greater than two micrometers.

### Claim 18

An integrated superconductor device, comprising:
a substrate base;
a buffer layer disposed on the substrate base and comprising a preferred crystallographic orientation; and
a superconductor layer disposed on the buffer layer, the superconductor layer comprising a superconducting region, and a non-superconducting region outside the superconducting region, wherein the non-superconducting region and superconducting region have at least three elements in common.

### Claim 19 (depends on 18)

The integrated superconductor device of claim 18, wherein the superconducting region comprises a copper oxide-based superconductor material having a c-axis texture in which the crystallites of the superconducting region have their c-axes oriented perpendicularly to the plane of the substrate.

### Claim 20 (depends on 18)

The integrated superconductor device of claim 18, wherein the superconducting region has a critical current greater than 2 MA/cm2.