# US 2015/0148218 A1 · Strontium cobaltite oxygen sponge catalyst and methods of use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0148218 A1
- Document ID: US20150148218A1
- Status: Published application
- Kind: A1
- Application number: 14/090,120
- Filed: 2013-11-26
- Published: 2015-05-28
- Earliest claimed: 2013-11-26
- Assignees: UT-Battelle, LLC
- Applicants: UT-Battelle, LLC
- Inventors: Ho Nyung Lee; Hyoungjeen Jeen; Woo Seok Choi; Michael Biegalski; Chad M. Folkman; I-Cheng Tung; Dillon D. Fong; John W. Freeland; Dongwon Shin; Hiromichi Ohta; Matthew F. Chisholm
- Web page: https://patentgrep.com/patent/US20150148218A1

## CPC

- B01J 20/04: comprising compounds of alkali metals, alkaline earth metals or magnesium
- B01J 23/78: with alkali- or alkaline earth metals
- B01J 23/847: Vanadium, niobium or tantalum {or polonium}
- C01G 51/66: containing alkaline earth metals, e.g. SrCoO3
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 35/33: Electric or magnetic properties
- B01J 37/349: {making use of flames, plasmas or lasers}
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/77: by unit-cell parameters, atom positions or structure diagrams
- C01P 2006/42: Magnetic properties
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Rapid, reversible redox activity may be accomplished at significantly reduced temperatures, as low as about 200° C., from epitaxially stabilized, oxygen vacancy ordered SrCoO2.5 and thermodynamically unfavorable perovskite SrCoO3-δ. The fast, low temperature redox activity in SrCoO3-δ may be attributed to a small Gibbs free energy difference between the two topotactic phases. Epitaxially stabilized thin films of strontium cobaltite provide a catalyst adapted to rapidly transition between oxidation states at substantially low temperatures. Methods of transitioning a strontium cobaltite catalyst from a first oxidation state to a second oxidation state are described.

## Claims

### Claim 1

A catalyst comprising epitaxially stabilized strontium cobaltite adapted to transition from a first oxidation state to a second oxidation state at a temperature between about 200° C. and about 340° C.

### Claim 2 (depends on 1)

The catalyst of claim 1 wherein the catalyst in said first oxidation state is ferromagnetic and electro-conductive and the catalyst in said second oxidation state is antiferromagnetic and electro-insulating.

### Claim 3 (depends on 1)

The catalyst of claim 1 wherein said transition from said first oxidation state to said second oxidation state occurs in less than about 1 minute.

### Claim 4 (depends on 1)

The catalyst of claim 1 wherein said transition from said first oxidation state to said second oxidation state occurs within a temperature range of about 210° C.-320° C.

### Claim 5 (depends on 1)

The catalyst of claim 1 wherein said transition from a first oxidation state to a second oxidation state is rapidly reversible at substantially low temperatures.

### Claim 6 (depends on 1)

The catalyst of claim 1 wherein said transition from said first oxidation state to said second oxidation state is a reduction process and said first oxidation state is strontium cobaltite in a perovskite phase and said second oxidation state is strontium cobaltite in a brownmillerite phase.

### Claim 7 (depends on 6)

The catalyst of claim 6 wherein said reduction process is completed in less than about 1 minute and at a temperature of between about 210° C. and 320° C.

### Claim 8 (depends on 6)

The catalyst of claim 6 wherein said transition from said first oxidation state to said second oxidation state is a reversible process, wherein said reversible process is an oxidation process and said brownmillerite phase of said strontium cobaltite is oxidized to said perovskite phase of said strontium cobaltite.

### Claim 9 (depends on 8)

The catalyst of claim 8 wherein said oxidation process is completed in less than about 1 minute and at a temperature of between about 201° C. and 320° C.

### Claim 10 (depends on 8)

The catalyst of claim 8 where said perovskite phase of strontium cobaltite is represented by the chemical formulation SrCoO3-δ.

### Claim 11 (depends on 10)

The catalyst of claim 10 wherein δ is less than 0.3.

### Claim 12 (depends on 1)

An article comprising a thin film having the catalyst of claim 1.

### Claim 13 (depends on 12)

The article of claim 12, wherein the article is an electromechanical device.

### Claim 14 (depends on 13)

The article of claim 13, wherein said electromechanical device is selected from the group consisting of: a fuel cell, an electrolyzer, a battery, a sensor, and a catalytic converter.

### Claim 15

A method of transitioning a strontium cobaltite catalyst from a first oxidation state to a second oxidation state, the method comprising the steps of:
providing a substrate supporting at least a thin layer of the strontium cobaltite catalyst in the said first oxidation state;
elevating a temperature of said catalyst in said first oxidation state; and
providing a vacuum atmosphere to said catalyst in said first oxidation state,
wherein said temperature is elevated to within a range of 210° C.-320° C. for a first period of time to effect the transition of the catalyst to said second oxidation state.

### Claim 16 (depends on 15)

The method of claim 15 wherein said period of time is less than about 1 minute.

### Claim 17 (depends on 15)

The method of claim 15 wherein said catalyst in said first oxidation state is in a perovskite phase and said catalyst in said second oxidation state is in a brownmillerite phase.

### Claim 18 (depends on 13)

The method of claim 13 further comprising the steps of:
reversing said transitioning of said catalyst from a first oxidation state to said second oxidation state by transitioning said catalyst from said second oxidation state to said first oxidation state by:
elevating said temperature of said catalyst in said second oxidation state; and
providing oxygen for a second period of time,
wherein said second period of time is sufficient to effect the transition of the catalyst to the first oxidation state.

### Claim 19

An epitaxially stabilized thin film of strontium cobaltite adapted to transition between SrCoO2.5 and SrCoO3-δ oxidation states.

### Claim 20 (depends on 19)

The film of claim 19 wherein the strontium cobaltite is stabilized on a substrate selected from the group consisting of: perovskite (ABO3), SrTiO3, and (LaAlO3)0.3—(Sr2AlTaO6)0.7
wherein A is selected from the group consisting of: an alkaline metal, and an alkaline earth element; B is a transitional metal; and O is oxygen.