# US 2015/0147892 A1 · Method for fabricating semiconductor structure, and solid precursor delivery system

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147892 A1
- Document ID: US20150147892A1
- Status: Published application
- Kind: A1
- Application number: 14/092,362
- Filed: 2013-11-27
- Published: 2015-05-28
- Earliest claimed: 2013-11-27
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Chung-Liang CHENG; Chien-Hao TSENG; Yen-Yu CHEN; Ching-Chia WU; Chang-Sheng LEE; Wei ZHANG
- Web page: https://patentgrep.com/patent/US20150147892A1

## CPC

- C23C 16/4402: {Reduction of impurities in the source gas}
- C23C 16/4481: {by evaporation using carrier gas in contact with the source material (C23C16/4486 takes precedence)}
- C23C 16/4485: {by evaporation without using carrier gas in contact with the source material (C23C16/4486 takes precedence)}
- C23C 16/45544: {characterized by the apparatus}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- H10D 64/01332: {Making the insulator}
- H10D 64/01336: {on single crystalline silicon, e.g. chemical oxidation using a liquid}
- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method for fabricating a semiconductor structure is provided, including: providing a solid precursor having a first average particle size; solving the solid precursor in an organic solvent into an intermediate; recrystallizing the intermediate to form solid granules, wherein the solid granules has a second average particle size larger than the first average particle size; vaporizing the solid granules to form a film-forming gas; and depositing the film-forming gas on a substrate to form a resistance film. A method for modifying a resistance film source in a semiconductor fabrication and a solid precursor delivery system are also provided. The method for fabricating a semiconductor structure in the present disclosure can remove small particles or ultra-small particles from solid precursor, and does not need extra time to dump cracked solid precursor.

## Claims

### Claim 1

A method for fabricating a semiconductor structure, comprising:
providing a solid precursor having a first average particle size;
solving the solid precursor in an organic solvent into an intermediate;
recrystallizing the intermediate to form solid granules, wherein the solid granules have a second average particle size larger than the first average particle size;
vaporizing the solid granules to form a film-forming gas; and
depositing the film-forming gas on a substrate to form a resistance film.

### Claim 2 (depends on 1)

The method of claim 1, wherein fabricating the semiconductor structure is performed by atomic layer deposition.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first average particle size is in the range of 300 μm to 500 μm.

### Claim 4 (depends on 1)

The method of claim 1, wherein recrystallizing the intermediate is performed at a temperature in the range of −30° C. to 10° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the second average particle size is in the range of 1 mm to 10 mm.

### Claim 6 (depends on 1)

The method of claim 1, wherein depositing the film-forming gas is depositing on a semiconductor wafer.

### Claim 7 (depends on 6)

The method of claim 6, wherein depositing the film-forming gas is depositing on a metal gate.

### Claim 8

A method for modifying a resistance film source in a semiconductor fabrication, comprising:
solving a solid precursor in an organic solvent into an intermediate;
recrystallizing the intermediate to form solid granules;
transporting the solid granules to a collecting room;
vaporizing the solid granules by to form a film-forming gas; and
to delivering the film-forming gas to a deposition chamber by a carrier gas.

### Claim 9 (depends on 8)

The method of claim 8, wherein the semiconductor fabrication is an atomic layer deposition process.

### Claim 10 (depends on 9)

The method of claim 9, wherein the atomic layer deposition process is applied in high-k metal gate technology.

### Claim 11 (depends on 8)

The method of claim 8, wherein recrystallizing the intermediate is performed at a temperature in the range of −30° C. to 10° C.

### Claim 12 (depends on 8)

The method of claim 8, wherein delivering the film-forming gas is performed by an inert gas.

### Claim 13 (depends on 12)

The method of claim 12, wherein delivering the film-forming gas is performed by argon.

### Claim 14

A solid precursor delivery system for a semiconductor fabrication, comprising:
a recrystallization reservoir, comprising:
cooling elements around the recrystallization reservoir;
a precursor entry port, wherein a solid precursor enters the recrystallization reservoir through the precursor entry port;
a solvent entry port, wherein an organic solvent enters the recrystallization reservoir through the solvent entry port; and
a granule exit port;
a gas tank;
a deposition chamber; and
a collecting room, comprising:
heating elements around the collecting room;
a granule entry port connecting to the granule exit port;
a gas entry port connecting to the gas tank; and
a gas exit port connecting to the deposition chamber.

### Claim 15 (depends on 14)

The system of claim 14, wherein the solid precursor is Pentakis-dimethylamino tantalum (PDMAT), tantalum chloride (TaCl5), tantalum fluoride (TaF5), hafnium chloride (HfCl4), niobium fluoride (NbF5), or molybdenum fluoride (MoF5).

### Claim 16 (depends on 14)

The system of claim 14, wherein the organic solvent is pentane, hexane, cyclopentane, or cyclohexane.

### Claim 17 (depends on 14)

The system of claim 14, wherein the gas tank is an inert gas tank.

### Claim 18 (depends on 17)

The system of claim 17, wherein the gas tank is an argon gas tank.

### Claim 19 (depends on 14)

The system of claim 14, wherein the deposition chamber is an atomic layer deposition chamber.

### Claim 20 (depends on 19)

The method of claim 19, wherein the atomic layer deposition chamber is applied in high-k metal gate technology.