# US 2015/0147886 A1 · Method For Integrated Circuit Patterning

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147886 A1
- Document ID: US20150147886A1
- Status: Published application
- Kind: A1
- Application number: 14/088,569
- Filed: 2013-11-25
- Published: 2015-05-28
- Earliest claimed: 2013-11-25
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Szu-Ping Tung; Huang-Yi Huang; Neng-Jye Yang; Ching-Hua Hsieh
- Web page: https://patentgrep.com/patent/US20150147886A1

## CPC

- H10P 76/4088: {Processes for improving the resolution of the masks}
- C23G 1/02: with acid solutions
- H10P 50/695: {characterised by the process involved to create the mask, e.g. lift-off masks or sidewalls or to modify the mask}
- H10P 50/73: {using masks for insulating materials}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10P 50/283: {by chemical means}
- H10P 50/667: {by liquid etching only}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23G: CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS

## Abstract

A method of forming a target pattern includes forming a plurality of lines over a substrate with a first mask and forming a spacer layer over the substrate, over the plurality of lines, and onto sidewalls of the plurality of lines. The method further includes removing at least a portion of the spacer layer to expose the plurality of lines and the substrate. The method further includes shrinking the spacer layer disposed onto the sidewalls of the plurality of lines and removing the plurality of lines thereby resulting in a patterned spacer layer over the substrate.

## Claims

### Claim 1

A method of forming a target pattern for an integrated circuit, the method comprising:
forming a plurality of lines over a substrate with a first mask;
forming a spacer layer over the substrate, over the plurality of lines, and onto sidewalls of the plurality of lines;
removing at least a portion of the spacer layer to expose the plurality of lines and the substrate;
shrinking the spacer layer disposed onto the sidewalls of the plurality of lines, wherein the shrinking of the spacer layer is isotropic and includes a wet process using a solution selectively tuned to remove a portion of the spacer layer while the plurality of lines and the substrate remain substantially unaltered; and
after the shrinking of the spacer layer, removing the plurality of lines thereby providing a patterned spacer layer over the substrate.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
etching the substrate using at least the patterned spacer layer as an etch mask; and
after etching, removing the spacer layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the forming the plurality of lines includes:
forming a resist layer over the substrate; and
patterning the resist layer with the first mask.

### Claim 4 (depends on 1)

The method of claim 1, wherein the removing at least a portion of the spacer layer includes an anisotropic etching process.

### Claim 5 (depends on 4)

The method of claim 4, wherein the anisotropic etching process includes dry etching.

### Claim 6 (depends on 1)

The method of claim 1, wherein
the spacer layer includes titanium nitride, titanium oxide, or silicon nitride; and
the wet process uses hydrofluoric acid (HF).

### Claim 7 (depends on 1)

The method of claim 1, wherein:
the spacer layer includes titanium nitride or titanium oxide; and
the wet cleaning process uses SC1 solution.

### Claim 8 (depends on 7)

The method of claim 7, wherein the SC1 solution includes a 1:1:5 mixture of ammonium hydroxide (NH4OH), hydrogen peroxide (H2O2), and water (H2O).

### Claim 9 (depends on 8)

The method of claim 8, wherein the shrinking the spacer layer is performed at a temperature between about 25 and about 80 degrees Celsius.

### Claim 10 (depends on 1)

The method of claim 1, wherein:
the spacer layer includes silicon nitride; and
the wet process uses phosphoric acid (H2PO4−).

### Claim 11 (depends on 10)

The method of claim 10, wherein the shrinking the spacer layer is performed at a temperature between about 25 and about 80 degrees Celsius.

### Claim 12 (depends on 1)

The method of claim 1, further comprising:
trimming the plurality of lines before the forming the spacer layer.

### Claim 13

A method of forming a target pattern for an integrated circuit, the method comprising:
patterning a substrate with a first mask thereby forming a first plurality of features;
forming a spacer layer over the substrate and over sidewalls of the first plurality of features;
anisotropically etching at least a portion of the spacer layer to expose the first plurality of features and to expose the substrate;
cleaning the spacer layer with a chemical solution to isotropically reduce a thickness of the spacer layer while keeping the plurality of features and the substrate substantially unaltered; and
after the cleaning of the spacer layer, removing the first plurality of features.

### Claim 14 (depends on 13)

The method of claim 13, wherein:
the spacer layer uses titanium nitride or titanium oxide; and
the chemical solution uses hydrofluoric acid (HF) or SC1 solution.

### Claim 15 (depends on 14)

The method of claim 14, wherein the thickness of the spacer layer is reduced with an etching rate about 10 to 30 angstroms per minute.

### Claim 16 (depends on 13)

The method of claim 13, wherein:
the spacer layer uses silicon nitride; and
the chemical solution uses hydrofluoric acid (HF) or phosphoric acid (H2PO4−).

### Claim 17 (depends on 16)

The method of claim 16, wherein the thickness of the spacer layer is reduced with an etching rate about 10 to 30 angstroms per minute.

### Claim 18

A method comprising:
forming two lines over a substrate using a photolithograph process, the two lines having a first dimension in a first direction;
depositing a first material over the substrate, over the two lines and onto sidewalls of the two lines;
performing an anisotropic etching process to the first material to expose the substrate and the two lines;
performing a wet cleaning process to the first material to reduce a thickness of the first material such that the first material disposed onto the sidewalls of the two lines are spaced away by a second dimension in the first direction; and
after the performing of the wet cleaning process, removing the two lines.

### Claim 19 (depends on 18)

The method of claim 18, wherein:
the first material uses a dielectric material containing metal;
the wet cleaning process uses a chemical solution with a pH about 3 to 6 or with a pH about 8 to 10; and
the wet cleaning process reduces the thickness of the first material with an etching rate about 10 to 30 angstroms per minute.

### Claim 20 (depends on 18)

The method of claim 18, wherein the first dimension and the second dimension are about the same.