# US 2015/0147861 A1 · Method of manufacturing semiconductor device using surface treatment and semiconductor device manufactured by the method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147861 A1
- Document ID: US20150147861A1
- Status: Published application
- Kind: A1
- Application number: 14/543,820
- Filed: 2014-11-17
- Published: 2015-05-28
- Earliest claimed: 2013-11-26
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: JAEYOUNG PARK; SUNGHO KANG; KICHUL KIM; Sunyoung LEE; HAN KI LEE; BONYOUNG KOO
- Web page: https://patentgrep.com/patent/US20150147861A1

## CPC

- H10D 84/834: {comprising FinFETs}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10D 62/117: {Shapes of semiconductor bodies}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 62/57: the imperfections being on the surface of the semiconductor body, e.g. the body having a roughened surface
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10D 84/0128: {Manufacturing their channels}
- H10D 84/0135: {Manufacturing their gate conductors}
- H10D 84/0149: {Manufacturing their interconnections or electrodes, e.g. source or drain electrodes}
- H10D 84/0151: {Manufacturing their isolation regions}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 14/414: {of metal-silicide materials}
- H10P 50/00: Etching of wafers, substrates or parts of devices
- H10P 70/23: {during, before or after processing of insulating materials}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10D 84/013: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a semiconductor device includes forming a first plurality of recessed regions in a substrate, the substrate having a protruded active region between the first plurality of recessed regions and the protruded active region having an upper surface and a sidewall, forming a device isolation film in the first plurality of recessed regions, the device isolation film exposing the upper surface and an upper portion of the sidewall of the protruded active region, and performing a first plasma treatment on the exposed surface of the protruded active region, wherein the plasma treatment is performed using a plasma gas containing at least one of an inert gas and a hydrogen gas in a temperature of less than or equal to about 700.

## Claims

### Claim 1

A method of performing a surface treatment process, the method comprising:
providing a substrate having an upper surface, the upper surface having a root-mean-square average roughness; and
performing a surface treatment on the upper surface of the substrate using a plasma gas containing at least one of an inert gas and a hydrogen gas to reduce the root-mean-square average roughness,
wherein the surface treatment is performed at a temperature less than or equal to about 700° C.

### Claim 2 (depends on 1)

The method of claim 1, wherein the root-mean-square average roughness of the substrate is less than or equal to about 2 nm after the surface treatment process.

### Claim at position 3

3-5. (canceled)

### Claim 6 (depends on 1)

The method of claim 1, wherein the substrate further comprises a fin protruding from the upper surface of the substrate, the fin having a top surface and at least one sidewall;
wherein the top surface and the sidewall of the fin have a surface roughness; and
wherein the sidewall of the fin is inclined before the surface treatment and is transformed to be substantially perpendicular to the top surface of the fin after the surface treatment.

### Claim 7 (depends on 6)

The method of claim 6, wherein performing the surface treatment comprises:
performing a first surface treatment sub-process to reduce the surface roughness of the fin; and
performing a second surface treatment sub-process to transform the sidewall of the fin to be substantially perpendicular to the upper surface of the fin.

### Claim 8 (depends on 7)

The method of claim 7, wherein the first surface treatment sub-process is performed using a helium gas plasma at a pressure of about 5 Torr to about 25 Torr, a power of about 2 kW to about 4 kW, and a temperature of about 300° C. to about 500° C.

### Claim 9 (depends on 7)

The method of claim 7, wherein the second surface treatment sub-process is performed using a hydrogen gas plasma at a pressure of less than or equal to about 1 Torr, a plasma power of about 2 kW to about 4 kW, and a temperature of about 300° C. to about 500° C.

### Claim 10

A method of manufacturing a semiconductor device, the method comprising:
forming a plurality of trenches and a plurality of protruding portions in a substrate, each protruding portion disposed between two trenches, including a top surface and at least two sidewalls each extending to the top surface, and comprising an active region;
forming a device isolation layer in the plurality of trenches, the device isolation layer exposing the top surfaces of the plurality of protruding portions and upper portions of the sidewalls of the plurality of protruding portions; and
performing a first plasma treatment process on the exposed surfaces of the protruding portions,
wherein the first plasma treatment process is performed using a plasma gas containing at least one of an inert gas and a hydrogen gas at a temperature of less than or equal to about 700° C.

### Claim 11 (depends on 10)

The method of claim 10, further comprising performing a second plasma treatment process on a surface of the plurality of trenches of the substrate before forming the device isolation layer.

### Claim 12 (depends on 10)

The method of claim 10, wherein the protruding portions include fin-type active regions.

### Claim 13 (depends on 12)

The method of claim 12, further comprising:
performing a cleaning process on the surface of the fin-type active regions; and
forming a gate dielectric layer on the surface of the fin-type active regions.

### Claim 14 (depends on 12)

The method of claim 12, further comprising:
forming a first gate dielectric layer on the surface of a first fin-type active region of the fin-type active regions;
forming a first gate electrode pattern having an upper surface and a sidewall on the first gate dielectric layer, the first gate electrode pattern crossing the first fin-type active region and partially covering the upper surface and sidewall of the first fin-type active region;
forming a plurality of recessed regions by etching a portion of each of the fin-type active regions and portions of the substrate adjacent to each of those portions; and
forming a source/drain epitaxial layer in the plurality of recessed regions.

### Claim 15 (depends on 14)

The method of claim 14, further comprising performing a second plasma treatment process on a surface of the plurality of recessed regions before forming the source/drain epitaxial layer.

### Claim 16 (depends on 14)

The method of claim 14, further comprising:
forming an interlayer insulating layer on the source/drain epitaxial layer, the interlayer insulating layer covering a sidewall of the first gate electrode pattern but not covering the upper surface of the first gate electrode pattern;
exposing the upper surface and the sidewall of the fin-type active region by removing the first gate electrode pattern and the first gate dielectric layer;
performing a plasma treatment on the upper surface and the sidewall of the fin-type active region;
forming a second gate dielectric layer on the upper surface and the sidewall of the fin-type active region; and
forming a second gate electrode pattern including metal on the second gate dielectric layer.

### Claim 17

(canceled)

### Claim 18 (depends on 12)

The method of claim 12, wherein the substrate comprises a low-voltage transistor region and a high-voltage transistor region,
wherein the fin-type active region includes a first fin formed in the low-voltage transistor region and a second fin formed in the high-voltage transistor region,
wherein the method further comprises:
forming a first gate dielectric layer on the first fin and a second gate dielectric layer on the second fin;
forming a sacrificial layer pattern having an upper surface and a sidewall on the first and the second gate dielectric layer;
forming an interlayer dielectric layer exposing the upper surface of the sacrificial layer pattern on the sidewall of the sacrificial layer pattern;
removing the sacrificial layer pattern to expose the first and the second gate dielectric layer;
removing the first gate dielectric layer to expose the first fin;
performing a second plasma treatment process on the first fin;
forming a high-k dielectric layer on the first fin; and
forming a gate electrode layer on the high-k dielectric layer.

### Claim 19 (depends on 10)

The method of claim 10, wherein the first plasma treatment process includes a first sub-process for reducing the roughness of the exposed surfaces of the protruding portions and performed at a pressure between about 5 Torr and 25 Torr and using a plasma gas including an inert gas, and a second sub-process for changing the angle between the sidewalls of the protruding portion and a top surface of the device isolation layer and performed at a pressure less than about 1 Torr and using a plasma gas including hydrogen.

### Claim 20

A method of manufacturing a semiconductor device, comprising:
providing a substrate;
etching the substrate to form a plurality of trenches, each trench having two opposite sidewall surfaces and an upper surface at the bottom of the trench;
performing a first plasma treatment process in the trenches to reduce a surface roughness of the surfaces of the trenches;
forming a device isolation layer that covers the upper surfaces at the bottom of the trenches and a lower portion of the sidewall surfaces of the trenches;
performing a second plasma treatment process on fin portions of the substrate, each fin portion including an exposed top surface of the substrate and opposite exposed sidewall surfaces at upper portions of the sidewall surfaces of the trenches, to reduce a surface roughness of these surfaces;
forming a first gate dielectric layer on a surface of a first fin portion of the substrate; and
forming a first gate electrode pattern having an upper surface and a sidewall on the first gate dielectric layer, the first gate electrode pattern crossing the first fin portion and partially covering the top surface and sidewalls of the first fin portion.

### Claim 21 (depends on 20)

The method of claim 20, further comprising:
forming recessed regions on either side of the first gate electrode pattern by etching part of the first fin portion; and
forming a source/drain epitaxial layer in each recessed region.

### Claim 22 (depends on 21)

The method of claim 21, further comprising:
prior to forming the source/drain epitaxial layer in each recessed region, performing a third plasma treatment process to reduce surface roughness of the recessed regions on either side of the first gate electrode pattern

### Claim 23

(canceled)

### Claim 24 (depends on 22)

The method of claim 22, wherein each of the first, second, and third plasma treatment processes include using a plasma gas containing at least one of an inert gas and a hydrogen gas at a temperature of less than or equal to about 700° C.

### Claim 25 (depends on 24)

The method of claim 24, wherein at least one of the first, second, or third plasma treatment processes include a first and second sub-process, the first subprocess using a first gas and performed at a first pressure, and the second subprocess using a second, different gas and performed at a second pressure at least five times smaller than the first pressure.

### Claim at position 24

26-34. (canceled)