# US 2015/0147679 A1 · Fuel cell interconnect with reduced voltage degradation over time

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147679 A1
- Document ID: US20150147679A1
- Status: Published application
- Kind: A1
- Application number: 14/543,095
- Filed: 2014-11-17
- Published: 2015-05-28
- Earliest claimed: 2013-11-27
- Assignees: Bloom Energy Corporation
- Applicants: Bloom Energy Corporation
- Inventors: Daniel DARGA; Tad ARMSTRONG; Vijay SRIVATSAN; Harald HERCHEN; Cheng-Yu LIN
- Web page: https://patentgrep.com/patent/US20150147679A1

## CPC

- A61M 16/14: by mixing different fluids, one of them being in a liquid phase
- A61M 15/0015: {located upstream of the dispenser, i.e. not traversed by the product}
- A61M 15/0018: {with exhalation check valves}
- A61M 15/0021: {Mouthpieces therefor}
- A61M 15/0086: {Inhalation chambers}
- A61M 16/04: Tracheal tubes (catheters in general A61M25/00)
- A61M 16/06: Respiratory or anaesthetic masks
- A61M 16/0816: {Joints or connectors}
- A61M 16/208: {Non-controlled one-way valves, e.g. exhalation, check, pop-off non-rebreathing valves}
- H01M 8/0208: Alloys
- H01M 8/0228: in the form of layered or coated products
- H01M 8/0271: Sealing or supporting means around electrodes, matrices or membranes
- H01M 8/2425: High-temperature cells with solid electrolytes
- H01M 8/2432: Grouping of unit cells of planar configuration
- H01M 8/2465: Details of groupings of fuel cells
- H01M 8/2483: characterised by internal manifolds
- H01M 8/2484: characterised by external manifolds
- A61M 15/0065: {Inhalators with dosage or measuring devices (A61M15/0028 takes precedence; dosage devices incorporated in aerosol cans B65D83/52)}
- A61M 16/08: Bellows; Connecting tubes {(having means for taking samples G01N1/22); Water traps; Patient circuits}
- A61M 2205/0233: Conductive materials, e.g. antistatic coatings for spark prevention
- A61M 2240/00: Specially adapted for neonatal use
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- A61M: DEVICES FOR INTRODUCING MEDIA INTO, OR ONTO, THE BODY (introducing media into or onto the bodies of animals A61D7/00; means for inserting tampons A61F13/26; devices for administering food or medicines orally A61J; containers for collecting, storing or administering blood or medical fluids A61J1/05); DEVICES FOR TRANSDUCING BODY MEDIA OR FOR TAKING MEDIA FROM THE BODY (surgery A61B; chemical aspects of surgical articles A61L); DEVICES FOR PRODUCING OR ENDING SLEEP OR STUPOR {(Electrotherapy, e.g. producing anaesthesia by the use of alternating or intermittent currents A61N1/36021)}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of making an interconnect for a solid oxide fuel cell stack includes providing a chromium alloy interconnect and providing a nickel mesh in contact with a fuel side of the interconnect. Formation of a chromium oxide layer is reduced or avoided in locations between the nickel mesh and the fuel side of the interconnect. A Cr—Ni alloy or a Cr—Fe—Ni alloy is located at least in the fuel side of the interconnect under the nickel mesh.

## Claims

### Claim 1

A method of making an interconnect for a solid oxide fuel cell stack, comprising:
providing a chromium alloy interconnect; and
providing a nickel mesh in contact with a fuel side of the interconnect;
wherein formation of a chromium oxide layer is reduced or avoided in locations between the nickel mesh and the fuel side of the interconnect.

### Claim 2 (depends on 1)

The method of claim 1, further comprising a Cr—Ni alloy or a Cr—Fe—Ni alloy located at least in the fuel side of the interconnect under the nickel mesh.

### Claim 3 (depends on 1)

The method of claim 1, wherein the formation of the chromium oxide layer is reduced or avoided by at least one of increasing compression pressure between the nickel mesh and the interconnect, providing undiffused Fe in the interconnect under the nickel mesh, reducing surface contamination between the interconnect and the nickel mesh, attaching the nickel mesh to the interconnect, or adding nickel to the interconnect alloy.

### Claim 4 (depends on 3)

The method of claim 3, wherein the formation of the chromium oxide layer is reduced or avoided by at least two of increasing compression pressure between the nickel mesh and the interconnect, providing undiffused Fe in the interconnect under the nickel mesh, reducing surface contamination between the interconnect and the nickel mesh, attaching the nickel mesh to the interconnect, and adding nickel to the interconnect alloy.

### Claim 5 (depends on 3)

The method of claim 3, wherein the formation of the chromium oxide layer is reduced or avoided by increasing the compression pressure between the nickel mesh and the interconnect by generating a pressure field or gradient on the mesh.

### Claim 6 (depends on 5)

The method of claim 5, wherein interconnect ribs in a middle of the interconnect have a greater height than interconnect ribs in a periphery of the interconnect to generate the pressure field or gradient on the mesh in a solid oxide fuel cell stack.

### Claim 7 (depends on 3)

The method of claim 3, wherein the formation of the chromium oxide layer is reduced or avoided by providing the undiffused Fe in the interconnect under the nickel mesh.

### Claim 8 (depends on 7)

The method of claim 7, wherein providing the undiffused Fe in the interconnect under the nickel mesh comprises pressing a chromium and iron containing powder to form the interconnect followed by partially sintering the interconnect at a lower temperature or a shorter duration than that required for fully alloying the iron and chromium powder particles.

### Claim 9 (depends on 7)

The method of claim 7, wherein providing the undiffused Fe in the interconnect under the nickel mesh comprises pressing mixture of a chromium powder having a first average particle size and iron powder having a second particle size larger than the first particle size to form the interconnect followed by sintering the interconnect.

### Claim 10 (depends on 3)

The method of claim 3, wherein the formation of the chromium oxide layer is reduced or avoided by attaching the nickel mesh to the interconnect using thermal fusing or welding.

### Claim 11 (depends on 3)

The method of claim 3, wherein the formation of the chromium oxide layer is reduced or avoided adding nickel to the interconnect alloy.

### Claim 12 (depends on 11)

The method of claim 11, wherein the nickel fully or partially substitutes iron at least in a fuel side of the interconnect.

### Claim 13 (depends on 12)

The method of claim 12, wherein the nickel fully or partially substitutes iron only in the fuel side of the interconnect by providing nickel powder having a different average particle size than chromium powder in a mold cavity.

### Claim 14 (depends on 12)

The method of claim 12, wherein the nickel fully or partially substitutes iron only in the fuel side of the interconnect by:
providing first metallic powder particles comprising Cr and Fe in a mold cavity;
providing second powder particles comprising nickel in the mold cavity; and
compacting the first and second powder particles to form the interconnect.

### Claim 15 (depends on 14)

The method of claim 14, wherein the first powder particles are provided in the mold cavity first and the second powder particles provided on top of the first powder particles in the mold cavity.

### Claim 16 (depends on 14)

The method of claim 14, wherein the second powder particles are provided in the mold cavity first and the first powder particles provided on top of the second powder particles in the mold cavity.

### Claim 17 (depends on 14)

The method of claim 14, wherein:
the first or the second powder particles are provided to the mold first and the other ones of the first or the second powder particles are electrostatically attracted to a bottom surface of a punch used to compact the powder particles; and
the punch presses the first powder and the second powder to compact the first and the second power particles.

### Claim 18

An interconnect for a solid oxide fuel cell stack, comprising:
a chromium alloy interconnect; and
a nickel mesh in contact with a fuel side of the interconnect;
wherein a Cr—Ni alloy or a Cr—Fe—Ni alloy is located at least in the fuel side of the interconnect under the nickel mesh.

### Claim 19 (depends on 18)

The interconnect of claim 18, wherein interconnect ribs in a middle of the interconnect have a greater height than interconnect ribs in a periphery of the interconnect to generate a pressure field or gradient on the mesh in a solid oxide fuel cell stack.

### Claim 20 (depends on 18)

The interconnect of claim 18, wherein undiffused Fe is located in the fuel side of the interconnect under the nickel mesh.

### Claim 21 (depends on 18)

The interconnect of claim 18, wherein the nickel mesh is welded or thermally fused to the interconnect.

### Claim 22 (depends on 18)

The interconnect of claim 18, wherein the interconnect alloy contains nickel.