# US 2015/0147663 A1 · Electrical energy storage device with non-aqueous electrolyte

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147663 A1
- Document ID: US20150147663A1
- Status: Published application
- Kind: A1
- Application number: 14/607,429
- Filed: 2015-01-28
- Published: 2015-05-28
- Earliest claimed: 2013-11-12
- Assignees: Intec Energy Storage Corporation
- Inventors: Alexandre M. Iarochenko
- Web page: https://patentgrep.com/patent/US20150147663A1

## CPC

- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- H01G 9/0029: {Processes of manufacture}
- H01G 9/035: Liquid electrolytes, e.g. impregnating materials (H01G11/54 takes precedence)
- H01G 9/045: based on aluminium
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/137: Electrodes based on electro-active polymers
- H01M 4/38: of elements or alloys
- H01M 4/463: {Aluminium based}
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/606: {containing aromatic main chain polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 10/0568: characterised by the solutes
- H01M 10/0569: characterised by the solvents
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 50/4295: {Natural cotton, cellulose or wood}
- H01M 50/44: Fibrous material
- H01M 50/534: characterised by the material of the leads or tabs
- H01M 4/502: {for non-aqueous cells (H01M4/505 takes precedence)}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 2300/0028: characterised by the solvent
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y02T 10/70: Energy storage systems for electromobility, e.g. batteries
- Y10T 29/49108: Electric battery cell making
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An electrical energy storage device 20 is disclosed as a secondary battery device 22 having an anode 28 containing Aluminum and Indium and a cathode 38 that includes an electroactive layer 42 with a host lattice 44 having a conjugated system with delocalized it electrons. A dopant 48 containing Aluminum is bonded with and intercalated in the host lattice 44. A membrane 34 of cellulose is wetted with a non-aqueous electrolyte 24 containing glycerol and first ions 26 containing Aluminum and having a positive charge and second ions 27 containing Aluminum and having a negative charge, and is sandwiched between the anode 28 and the cathode 38. A method for constructing a secondary battery device 22 is disclosed as well, including steps for producing the electrolyte 24, the anode 28, and the cathode 38 including the dopant 48.

## Claims

### Claim 1

An electrical energy storage device (20) comprising;
an anode (28) comprising a layer of Aluminum,
a membrane (34) sandwiched with said anode (28),
an electrolyte (24) including first ions (26) containing Aluminum and having a positive charge and including second ions (27) containing Aluminum and having a negative charge and said electrolyte (24) impregnating said membrane (34) to carry an ion current through said membrane (34),
a cathode (38) sandwiched with said membrane (34) and disposed in spaced and parallel relationship with said anode (28),
and characterized by,
said electrolyte (24) consisting essentially of glycerol and said first ions (26) containing Aluminum and said second ions (27) containing Aluminum dispersed in said glycerol for migrating between and reacting with said anode (28) of Aluminum and said cathode (38) to charge and discharge the electrical energy storage device (20).

### Claim 2 (depends on 1)

An electrical energy storage device (20) as set forth in claim 1 wherein said first ions (26) containing Aluminum include [Al(ClO4)2{C3H5(OH)3}2]+ and said second ions (27) containing Aluminum include [Al(ClO4)4]−.

### Claim 3

An electrical energy storage device (20) comprising;
an anode (28) comprising a layer of Aluminum,
a membrane (34) sandwiched with said anode (28),
a cathode (38) sandwiched with said membrane (34) and disposed in spaced and parallel relationship with said anode (28),
and characterized by,
said cathode (38) containing a host lattice (44) having a conjugated system with delocalized it electrons and a dopant (48) containing Aluminum Glycerate bonded with said host lattice (44) to alter the electrochemical properties of said host lattice (44) of said cathode (38).

### Claim 4 (depends on 3)

An electrical energy storage device (20) as set forth in claim 3 wherein said dopant (48) contains Aluminum Alcoholate.

### Claim 5

A secondary battery device (22) comprising;
an anode (28) consisting of a layer of 99.4 to 99.9 wt % of solid Aluminum of 99.95% purity and 0.1 to 0.6 wt % of Indium and having a rectangular shape with a first length of 1.2 cm and a first width of 1.7 cm and a first thickness of 0.1 mm,
a negative lead (30) of an electrically conductive material in electrical contact with said anode (28) for conducting electrical current with external circuitry,
a cement (32) including particles of metal disposed between and bonding said anode (28) and said negative lead (30) for conducting electrical current therebetween,
a membrane (34) of cellulose having a third thickness of 0.08 mm and defining a plurality of pores (36) and sandwiched with said anode (28) for providing electrical insulation therebetween,
an electrolyte (24) including first ions (26) containing Aluminum and having a positive charge and including second ions (27) containing Aluminum and having a negative charge and said electrolyte (24) impregnating said pores (36) of said membrane (34) to carry an ion current through said membrane (34),
a cathode (38) having a rectangular shape with a second length of 1.4 cm and a second width of 1.9 cm and a second thickness of 0.1 mm disposed adjacent and parallel to said membrane (34) with said membrane (34) being sandwiched between said cathode (38) and said anode (28),
said cathode (38) including a carrier sheet (40) of cellulose and an electroactive layer (42) integrated with and upon said carrier sheet (40) facing said anode (28),
a positive lead (50) containing graphite in electrical contact with said electroactive layer (42) of said cathode (38) for conducting electrical current with external circuitry,
an adhesive (52) containing graphite disposed between and bonding said electroactive layer (42) and said positive lead (50) for conducting electrical current therebetween,
and characterized by,
said electrolyte (24) consisting essentially of glycerol and said first ions (26) including [Al(ClO4)2{C3H5(OH)3}2]+ and said second ions (27) including [Al(ClO4)4]− for migrating between and reacting with said anode (28) and said cathode (38) to charge and discharge said secondary battery device (22),
said electroactive layer (42) of said cathode (38) containing a host lattice (44) having a conjugated system with delocalized it electrons and defining voids and a dopant (48) containing Aluminum Alcoholate and Aluminum Glycerate bonded with said conjugated system of said host lattice (44) and intercalated in said voids to alter the electrochemical properties of said electroactive layer (42) of said cathode (38) to increase the rate of the reactions with said first ions (26) and said second ions (27) for charging and discharging said secondary battery device (22).

### Claim 6 (depends on 5)

The secondary battery device (22) as set forth in claim 5 wherein said host lattice (44) of said electroactive layer (42) comprises flakes (54) of graphite having particle size of 200 to 300 μm and a binder material wettable by glycerol.

### Claim 7 (depends on 6)

The secondary battery device (22) as set forth in claim 6 wherein said binder material comprises alkyl glue.

### Claim 8 (depends on 6)

The secondary battery device (22) as set forth in claim 6 wherein said binder material comprises acrylic glue.

### Claim 9 (depends on 5)

The secondary battery device (22) as set forth in claim 5 wherein said host lattice (44) of said electroactive layer (42) comprises particles of amorphous thermally expandable graphite and manganese dioxide and activated manganese dioxide and acetylene black and a binder material being wettable by glycerol and an electrically conductive paint including graphite.

### Claim 10 (depends on 9)

The secondary battery device (22) as set forth in claim 9 wherein said binder material is alkyl glue.

### Claim 11 (depends on 9)

The secondary battery device (22) as set forth in claim 9 wherein said binder material is acrylic glue.

### Claim 12 (depends on 9)

The secondary battery device (22) as set forth in claim 9 wherein said binder material is an electrically conductive paint including graphite.

### Claim 13 (depends on 5)

The secondary battery device (22) as set forth in claim 5 wherein said host lattice (44) of said electroactive layer (42) includes a polyconjugated linear hydrocarbon polymer.

### Claim 14 (depends on 5)

The secondary battery device (22) as set forth in claim 5 wherein said host lattice (44) of said electroactive layer (42) includes a cyclic polyconjugated chain polymer of polyaniline.

### Claim 15

A method for constructing an electrical energy storage device (20) having an anode (28) and a membrane (34) and an electrolyte (24) and a cathode (38), said method comprising;
wetting the membrane (34) with an electrolyte (24),
stacking the membrane (34) upon and parallel to the anode (28),
stacking the cathode (38) upon and parallel to the membrane (34) with the membrane (34) disposed between the anode (28) and the cathode (38),
and characterized by,
dissolving Aluminum Perchlorate powder in glycerol to saturation to make the electrolyte (24).

### Claim 16 (depends on 15)

The method as set forth in claim 15 further comprising steps for making a doping fluid (62) for carrying a dopant (48) containing Aluminum into an electrode (28, 38) of an electrical energy storage device (20) using filings (70) containing Aluminum, said method comprising;
dissolving AlCl3 powder in ethanol to create a background solution (66),
and characterized by,
combining the background solution (66) with glycerol to produce a binary solvent (68),
immersing the filings (70) containing Aluminum in the binary solvent (68) until the filings (70) containing Aluminum have dissolved to produce the doping fluid (62).

### Claim 17

A method for constructing a secondary battery device (22) having an anode (28) and a negative lead (30) and a membrane (34) and an electrolyte (24) and a cathode (38) having a carrier sheet (40) of cellulose using a cathodic mixture (60), said method comprising;
heating a plate of Aluminum of 99.95% purity and 0.1 to 0.6 wt % of Indium to a temperature of 450° C.,
rolling the plate to reduce the thickness of the plate while cooling at a rate of more than 10° C. per minute to a reduced thickness,
reheating the reduced thickness of the plate and rerolling the reduced thickness of the plate into a foil (56) coated with Aluminum Oxide and surface contaminants and having a thickness between 0.05 and 0.1 mm,
rinsing the foil (56) with ethanol to remove surface contaminants therefrom,
submerging the foil (56) in a solution of water and Hydroxide having a concentration of 4 mol for one minute for removing the Aluminum Oxide from the surface of the foil (56),
rinsing the foil (56) with water for removing the Hydroxide therefrom,
subjecting the foil (56) to 70° C. for 30 minutes for evaporating moisture therefrom,
surrounding the foil (56) with an anhydrous environment,
dividing the foil (56) into a rectangular shape to define the anode (28) having a first length of 1.2 cm and a first width of 1.7 cm,
attaching a negative lead (30) to the anode (28) with a cement (32) including particles of silver,
wetting the membrane (34) with the electrolyte (24),
stacking the membrane (34) upon and parallel to the anode (28),
applying the cathodic mixture (60) in a thin film layer to one side of the carrier sheet (40) of cellulose to soak into the carrier sheet (40),
subjecting the cathodic mixture (60) to a temperature of 50 to 60° C. to solidify the cathodic mixture (60) into a host lattice (44) being disposed upon and within the carrier sheet (40),
wetting the host lattice (44) with a doping fluid (62) containing a dopant (48) to allow the dopant (48) to bond with and intercalate into the host lattice (44) to produce an electroactive layer (42),
attaching a positive lead (50) in electrical contact with the electroactive layer (42) of the cathode (38) with an adhesive (52) containing graphite,
stacking the cathode (38) upon and parallel to the membrane (34) with the membrane (34) disposed between the anode (28) and the cathode (38),
and characterized by,
dissolving Aluminum Perchlorate powder in glycerol to saturation to produce the electrolyte (24),
dissolving AlCl3 powder in ethanol to produce a background solution (66),
combining 40 wt % of the background solution (66) with 60 wt % of glycerol to produce a binary solvent (68),
grating 1 cm3 of 99.4 to 99.9 wt % of Aluminum of 99.95% purity and 0.1 to 0.6 wt % of Indium to make filings (70) with an equivalent surface area of 20 to 30 cm2,
immersing the filings (70) in 150 to 200 ml of the binary solvent (68) until the filings (70) have dissolved to produce the doping fluid (62).

### Claim 18 (depends on 17)

The method as set forth in claim 17 further comprising a step for making the cathodic mixture (60) characterized by;
mixing 5 wt % of alkyl glue with 60 wt % of ethanol with 35 wt % of flakes (54) of graphite to make the cathodic mixture (60).

### Claim 19 (depends on 17)

The method as set forth in claim 17 further comprising a step for making the cathodic mixture (60) characterized by;
mixing amorphous thermally expandable graphite powder with 1-5 wt % MnO2 with 1-5 wt % activated MnO2 with 1-5 wt % acetylene black to make an intermediate mixture.

### Claim 20 (depends on 19)

The method as set forth in claim 19, further comprising the step of adding a binder of alkyl glue and ethanol to the intermediate mixture to make the cathodic mixture (60) having a consistency of thick spreadable paste.

### Claim 21 (depends on 19)

The method as set forth in claim 19, further comprising the step of adding a binder of acrylic glue to the intermediate mixture to make the cathodic mixture (60) having a consistency of thick spreadable paste.

### Claim 22 (depends on 19)

The method as set forth in claim 19, further comprising the step of adding a binder of graphite paint to the intermediate mixture to make the cathodic mixture (60) having a consistency of thick spreadable paste.