# US 2015/0147651 A1 · Positive active material for rechargeable lithium battery, method of preparing same, and rechargeable lithium battery including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147651 A1
- Document ID: US20150147651A1
- Status: Published application
- Kind: A1
- Application number: 14/281,678
- Filed: 2014-05-19
- Published: 2015-05-28
- Earliest claimed: 2013-11-27
- Assignees: Samsung SDI Co., Ltd.
- Applicants: Samsung SDI Co., Ltd.
- Inventors: Ming-Zi Hong; Do-Hyung Park; Seon-Young Kwon; Joong-Ho Moon; Ji-Hyun Kim; Han-Eol Park; Min-Han Kim; Myong-A Woo; Ki-Hyun Kim; Jong-Seo Choi
- Web page: https://patentgrep.com/patent/US20150147651A1

## CPC

- H01M 4/366: {as layered products}
- C01G 53/502: containing lithium and cobalt
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- C01G 53/506: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.8, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.8
- H01M 4/0416: {involving impregnation with a solution, dispersion, paste or dry powder (H01M4/0438 takes precedence)}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive active material for a rechargeable lithium battery including a core including at least one selected from a nickel-based composite oxide represented by Chemical Formula 1 or a lithium manganese oxide represented by Chemical Formula 2; and a coating layer on a surface of the core and including a lithium metal oxide represented by Chemical Formula 3, the positive active material having a peak at a 2θ value of about 19° to about 22° and another peak at a 2θ value of about 40° to about 45° in an X-ray diffraction pattern using a CuKα ray, is disclosed. A method of preparing the same, and a rechargeable lithium battery including the same, are also disclosed. LiNixCoyMn1-x-yO2 Chemical Formula 1 LiaMnbOc Chemical Formula 2 Li2MO3 Chemical Formula 3 In Chemical Formulae 1 to 3, x, y, a, b, c, and M are the same as in the detailed description.

## Claims

### Claim 1

A positive active material for a rechargeable lithium battery, comprising:
a core including at least one selected from a nickel-based composite oxide represented by Chemical Formula 1 or a lithium manganese oxide represented by Chemical Formula 2; and
a coating layer on a surface of the core and comprising a lithium metal oxide represented by Chemical Formula 3,
wherein the positive active material has a peak at a 2θ value of about 19° to about 22° and another peak at a 2θ value of about 40° to about 45° in an X-ray diffraction pattern using a CuKα ray:
LiNixCoyMn1-x-yO2 Chemical Formula 1
wherein 0.1≦x≦0.8, and 0.1≦y≦0.8,
LiaMnbOc Chemical Formula 2
wherein 1≦a≦2, 1≦b≦2, and 2≦c≦4, and
Li2MO3 Chemical Formula 3
wherein M is at least one tetravalent element selected from Zr or Ti.

### Claim 2 (depends on 1)

The positive active material of claim 1, wherein the positive active material has an intensity ratio of the peak at a 2θ value of about 19° to about 22° to the other peak at a 2θ value of about 40° to about 45° of about 2.0 to about 3.0.

### Claim 3 (depends on 1)

The positive active material of claim 1, wherein the positive active material has an intensity ratio of the peak at a 2θ value of about 19° to about 22° to the other peak at a 2θ value of about 40° to about 45° of about 2.0 to about 2.5.

### Claim 4 (depends on 1)

The positive active material of claim 1, wherein the positive active material comprises about 90 wt % to about 99.9 wt % of the core and about 0.1 wt % to about 10 wt % of the coating layer.

### Claim 5

A method of preparing a positive active material for a rechargeable lithium battery, the method comprising:
mixing at least one core material selected from a nickel-based composite oxide represented by Chemical Formula 1 or a lithium manganese oxide represented by Chemical Formula 2 and a solution comprising a salt comprising at least one tetravalent element selected from Zr or Ti to form a mixture; and
heat-treating the mixture to coat a surface of the core material with a lithium metal oxide represented by Chemical Formula 3:
LiNixCoyMn1-x-yO2 Chemical Formula 1
wherein 0.1≦x≦0.8, and 0.1≦y≦0.8,
LiaMnbOc Chemical Formula 2
wherein 1≦a≦2, 1≦b≦2, and 2≦c≦4, and
Li2MO3 Chemical Formula 3
wherein M is at least one tetravalent element selected from Zr or Ti.

### Claim 6 (depends on 5)

The method of claim 5, wherein the salt comprising the tetravalent element comprises at least one selected from ZrO(NO3)2.rH2O(0≦r≦5), Zr(NO3)2.5H2O, Zr(SO4)2, or Zr(SO4)2.4H2O.

### Claim 7 (depends on 5)

The method of claim 5, wherein the salt comprising the tetravalent element is present in the solution in an amount of about 0.001 to about 10 parts by mole, based on 100 parts by mole of the core material.

### Claim 8 (depends on 5)

The method of claim 5, wherein the solution comprising the salt comprising the tetravalent element is an aqueous solution or an alcohol solution.

### Claim 9 (depends on 5)

The method of claim 5, wherein the heat-treating is performed at a temperature of about 350 to about 1000° C.

### Claim 10 (depends on 5)

The method of claim 5, wherein the heat-treating is performed under an air atmosphere or an oxygen atmosphere.

### Claim 11

A method of preparing a positive active material for a rechargeable lithium battery, the method comprising:
mixing a salt comprising at least one tetravalent element selected from Zr or Ti and a first solvent to form a salt solution;
mixing a chelating agent and a second solvent to form a chelating agent solution;
mixing the salt solution and the chelating agent solution to form a first mixed solution;
mixing the first mixed solution and a homogenizer to form a second mixed solution;
mixing at least one core material selected from a nickel-based composite oxide represented by Chemical Formula 1 or a lithium manganese oxide represented by Chemical Formula 2 and the second mixed solution to form a mixture; and
heat-treating the mixture to coat a surface of the core material with a lithium metal oxide represented by Chemical Formula 3:
LiNixCoyMn1-x-yO2 Chemical Formula 1
wherein 0.1≦x≦0.8, and 0.1≦y≦0.8,
LiaMnbOc Chemical Formula 2
wherein 1≦a≦2, 1≦b≦2, and 2≦c≦4, and
Li2MO3 Chemical Formula 3
wherein M is at least one tetravalent element selected from Zr or Ti.

### Claim 12 (depends on 11)

The method of claim 11, wherein the salt comprising the tetravalent element comprises at least one selected from ZrO(NO3)2.rH2O(0≦r≦5), Zr(NO3)2.5H2O, Zr(SO4)2, or Zr(SO4)2.4H2O.

### Claim 13 (depends on 11)

The method of claim 11, wherein the salt comprising the tetravalent element is present in the salt solution in an amount of about 0.001 to about 10 parts by mole, based on 100 parts by mole of the core material.

### Claim 14 (depends on 11)

The method of claim 11, wherein the first solvent and second solvent each comprise water, alcohol, or a combination thereof.

### Claim 15 (depends on 11)

The method of claim 11, wherein the heat-treating is performed at a temperature of about 350 to about 1000° C.

### Claim 16 (depends on 11)

The method of claim 11, wherein the heat-treating is performed under an air atmosphere or an oxygen atmosphere.

### Claim 17

A rechargeable lithium battery comprising
a positive electrode comprising the positive active material according to claim
a negative electrode; and
an electrolyte.