# US 2015/0147575 A1 · Fast ion exchangeable glasses with high indentation threshold

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147575 A1
- Document ID: US20150147575A1
- Status: Published application
- Kind: A1
- Application number: 14/543,925
- Filed: 2014-11-18
- Published: 2015-05-28
- Earliest claimed: 2013-11-26
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Matthew John Dejneka; John Christopher Mauro
- Web page: https://patentgrep.com/patent/US20150147575A1

## CPC

- C03C 4/18: for ion-sensitive glass
- C03C 3/091: containing aluminium
- C03C 3/093: containing zinc or zirconium
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- Y10T 428/315: Surface modified glass [e.g., tempered, strengthened, etc.]
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Alkali aluminosilicate glasses that are ion exchangeable to high compressive stresses, have fast ion exchange kinetics, and high intrinsic damage resistance. The glasses achieve all of the above desired properties either with only small amounts of P2O5 (<1 mol %) or without addition of any P2O5.

## Claims

### Claim 1

A glass, the glass comprising:
from about 50 mol % to about 72 mol % SiO2;
from about 12 mol % to about 22 mol % Al2O3;
up to about 6.5 mol % B2O3;
up to about 1 mol % P2O5;
from about 11 mol % to about 21 mol % Na2O;
up to about 0.95 mol % K2O;
up to about 4 mol % MgO;
up to about 5 mol % ZnO; and
up to about 2 mol % CaO, wherein
Na2O+K2O−Al2O3≦2.0 mol,
B2O3−(Na2O+K2O−Al2O3)>1 mol %,
24 mol %≦RAlO4≦45 mol %, where R is at least one of Na, K, and Ag, and
the glass is substantially free of TiO2.

### Claim 2 (depends on 1)

The glass of claim 1, wherein the glass is substantially free of at least one of P2O5 and Li2O.

### Claim 3 (depends on 2)

The glass of claim 2, wherein the glass is substantially free of Li2O.

### Claim 4 (depends on 1)

The glass of claim 1, wherein 56 mol %≦SiO2+B2O3≦75 mol %.

### Claim 5 (depends on 1)

The glass of claim 1, wherein the glass comprises up to about 0.75 mol % K2O.

### Claim 6 (depends on 1)

The glass of claim 1, wherein the glass is ion exchanged and has a Vickers crack indentation threshold of at least about 9.5 kgf.

### Claim 7 (depends on 6)

The glass of claim 6, wherein the glass has a layer under compressive stress CS of greater than about 500 MPa, the layer extending from a surface of the glass to a depth of layer DOL, wherein CS·DOL=44000 MPa·μm.

### Claim 8 (depends on 6)

The glass of claim 6, wherein the glass has a compressive stress of greater than about 800 MPa and a depth of layer of at least about 40 μm, and has been ion exchanged for less than about four hours.

### Claim 9 (depends on 6)

The glass of claim 6, wherein the glass has a compressive stress of greater than about 800 MPa and a depth of layer of at least about 52 μm, and has been ion exchanged for less than about eight hours.

### Claim 10 (depends on 6)

The glass of claim 6, wherein the glass has a compressive stress of greater than about 800 MPa and a depth of layer of at least about 30 μm, and has been ion exchanged for less than about two hours.

### Claim 11 (depends on 1)

The glass of claim 1, wherein the glass is substantially free of As2O3 and Sb2O5.

### Claim 12 (depends on 1)

The glass of claim 1, wherein the glass further comprises at least one fining agent.

### Claim 13 (depends on 12)

The glass of claim 12, wherein the at least one fining agent comprises at least one of SnO2, CeO2, As2O3, Sb2O5, Cl−, and F−.

### Claim 14 (depends on 13)

The glass of claim 13, wherein the at least one fining agent comprises at least one of up to about 0.5 mol % SnO2, up to about 0.5 mol % As2O3, and up to about 0.5 mol % Sb2O3.

### Claim 15 (depends on 1)

The glass of claim 1, wherein the glass has a liquidus viscosity of at least 100 kpoise.

### Claim 16 (depends on 15)

The glass of claim 15, wherein the glass is down-drawable.

### Claim 17

A glass comprising:
from about 55 mol % to about 62 mol % SiO2;
from about 16 mol % to about 20 mol % Al2O3;
from about 4 mol % to about 6.5 mol % B2O3;
from about 14 mol % to about 18 mol % Na2O;
from about 0.2 mol % to about 0.75 mol % K2O;
up to about 0.5 mol % MgO;
up to about 0.5 mol % ZnO; and
up to about 0.5 mol % CaO, wherein
the glass is substantially free of P2O5,
Na2O+K2O−Al2O3≦0.5 mol %,
B2O3−(Na2O+K2O−Al2O3)>4 mol %,
28 mol %≦RAlO4≦45 mol %, where R is at least one of Na, K, and Ag, and
the glass is substantially free of TiO2.

### Claim 18 (depends on 17)

The glass of claim 17, wherein the glass is substantially free of Li2O.

### Claim 19 (depends on 17)

The glass of claim 17, wherein 56 mol %≦SiO2+B2O3≦70 mol %.

### Claim 20 (depends on 17)

The glass of claim 17, wherein 0 mol %≦Σ[R′O]≦0.5 mol %, where R′ is at least one of Ca, Mg, and Zn.

### Claim 21 (depends on 17)

The glass of claim 17, wherein the glass is substantially free of As2O3 and Sb2O3.

### Claim 22 (depends on 17)

The glass of claim 17, wherein the glass further comprises at least one fining agent, the fining agent comprising at least one of SnO2, CeO2, As2O3, and Sb2O5, Cl−, and F−.

### Claim 23 (depends on 22)

The glass of claim 22, wherein the at least one fining agent comprises at least one of up to about 0.5 mol % SnO2, up to about 0.5 mol % As2O3, and up to about 0.5 mol % Sb2O3.

### Claim 24 (depends on 17)

The glass of claim 17, wherein the glass has a liquidus viscosity of at least 100 kpoise.

### Claim 25 (depends on 24)

The glass of claim 24, wherein the glass is down-drawable.

### Claim 26 (depends on 17)

The glass of claim 17, wherein the glass is ion exchanged and has a Vickers crack indentation threshold of at least about 9.5 kgf.

### Claim 27 (depends on 26)

The glass of claim 26, wherein the glass has a layer under compressive stress CS of greater than 500 MPa, the layer extending from a surface of the glass to a depth of layer DOL, wherein CS·DOL=44000 MPa·μm.

### Claim 28 (depends on 26)

The glass of claim 26, wherein the glass has a compressive stress of greater than about 800 MPa and a depth of layer of at least about 40 μm, and has been ion exchanged for less than about four hours.

### Claim 29 (depends on 26)

The glass of claim 26, wherein the glass has a compressive stress of greater than about 800 MPa and a depth of layer of at least about 52 μm, and has been ion exchanged for less than about eight hours.

### Claim 30 (depends on 26)

The glass of claim 26, wherein the glass has a compressive stress of greater than about 800 MPa and a depth of layer of at least about 30 μm, and has been ion exchanged for less than about two hours.