- Number: US 2015/0147574 A1
- Document ID: US20150147574A1
- Status: Published application
- Kind: A1
- Application number: 14/540,328
- Filed: 2014-11-13
- Published: 2015-05-28
- Earliest claimed: 2013-11-25
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Douglas Clippinger Allan; Xiaoju Guo; Guangli Hu; Gaozhu Peng
- Web page: https://patentgrep.com/patent/US20150147574A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 3/083: containing aluminium oxide or an iron compound
- C03C 3/085: containing an oxide of a divalent metal
- C03C 3/091: containing aluminium
- C03C 3/093: containing zinc or zirconium
- C03C 4/18: for ion-sensitive glass
- C03C 21/005: {to introduce in the glass such metals or metallic ions as Ag, Cu}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- Y10T 428/315: Surface modified glass [e.g., tempered, strengthened, etc.]
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for generating various stress profiles for chemically strengthened glass. An alkali aluminosilicate glass is brought into contact with an ion exchange media such as, for example, a molten salt bath containing an alkali metal cation that is larger than an alkali metal cation in the glass. The ion exchange is carried out at temperatures greater than about 420° C. and at least about 30° C. below the anneal point of the glass.

## Claims

### Claim 1

A method of strengthening an alkali aluminosilicate glass comprising first metal cations and having an anneal point, the method comprising:
a. immersing the alkali aluminosilicate glass in a molten salt bath, the molten salt bath comprising at least one salt of a second metal, wherein cations of the second metal are larger than the first metal cations;
b. ion exchanging the cations of the second metal from the molten salt bath for the first metal cations in the alkali aluminosilicate glass at a temperature of greater than about 420° C. and at least about 30° C. less than the anneal point, wherein ion exchanging forms a region of compressive stress, the region extending from a surface of the glass to a depth of layer of at least 40 μm into the glass, and wherein a compressive stress at a first depth is at least about 50% of a compressive stress at the surface, the first depth being between about 30% and about 70% of the depth of layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first metal cations are sodium cations and the second cations are at least one of potassium cations, rubidium cations, or silver cations.

### Claim 3 (depends on 2)

The method of claim 2, wherein the molten salt bath comprises at least one of potassium sulfate and potassium nitrate.

### Claim 4 (depends on 3)

The method of claim 3, wherein the molten salt bath further comprises up to about 10 wt % of at least one sodium salt.

### Claim 5 (depends on 1)

The method of claim 1, wherein the compressive stress at the surface is at least about 100 MPa.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first depth is about 25 nm.

### Claim 7 (depends on 6)

The method of claim 6, wherein the first compressive stress is at least about 350 MPa.

### Claim 8 (depends on 6)

The method of claim 6, wherein the alkali aluminosilicate glass has a retained strength of at least about 200 MPa.

### Claim 9 (depends on 6)

The method of claim 6, wherein ion exchanging the alkali aluminosilicate glass comprises ion exchanging the alkali aluminosilicate glass for a period ranging from about 0.5 hours to about 8 hours.

### Claim 10 (depends on 1)

The method of claim 1, wherein the alkali aluminosilicate glass comprises at least about 50 mol % SiO2 and at least about 11 mol % Na2O, and wherein the compressive stress at the surface is at least about 900 MPa.

### Claim 11 (depends on 10)

The method of claim 10, wherein the alkali aluminosilicate glass further comprises Al2O3 and at least one of B2O3, K2O, MgO and ZnO, and wherein −340+27.1·Al2O3−28.7·B2O3+15.6·Na2O−61.4·K2O+8.1·(MgO+ZnO)≧0 mol %.

### Claim 12 (depends on 1)

The method of claim 1, wherein the alkali aluminosilicate glass comprises at least about 50 mol % SiO2; from about 9 mol % to about 22 mol % Al2O3; from about 3 mol % to about 10 mol % B2O3; from about 9 mol % to about 20 mol % Na2O; from 0 mol % to about 5 mol % K2O; and at least about 0.1 mol % MgO, ZnO, or combinations thereof, wherein 0≦MgO≦6 and 0≦ZnO≦6 mol %; and, optionally, at least one of CaO, BaO, and SrO, wherein 0 mol %≦CaO+SrO+BaO≦2 mol %.

### Claim 13 (depends on 1)

The method of claim 1, wherein the alkali aluminosilicate glass comprises: at least about 50 mol % SiO2; at least about 10 mol % R2O, wherein R2O comprises Na2O; Al2O3, wherein −0.5 mol %≦Al2O3(mol %)−R2O(mol %)≦2 mol %; and B2O3, and wherein B2O3(mol %)−(R2O(mol %)−Al2O3(mol %))≧4.5 mol %.

### Claim 14 (depends on 13)

The method of claim 13, wherein the alkali aluminosilicate glass has a zircon breakdown temperature that is equal to the temperature at which the glass has a viscosity of greater than about 40 kPoise and comprises: at least about 50 mol % SiO2; at least about 10 mol % R2O, wherein R2O comprises Na2O; Al2O3; and B2O3, wherein B2O3(mol %)−(R2O(mol %)−Al2O3(mol %))≧4.5 mol %.

### Claim 15 (depends on 1)

The method of claim 1, wherein the alkali aluminosilicate glass comprises at least about 4 mol % P2O5, wherein (M2O3(mol %)/RxO (mol %))<1, wherein M2O3=Al2O3+B2O3, and wherein RxO is the sum of monovalent and divalent cation oxides present in the alkali aluminosilicate glass.

### Claim 16 (depends on 1)

The method of claim 1, wherein the glass has a thickness of up to about 1.5 mm.

### Claim 17 (depends on 1)

The method of claim 1, further comprising:
a. immersing the alkali aluminosilicate glass in a second molten salt bath, the second molten salt bath comprising at least one salt of a third metal, wherein cations of the third metal are larger than the first metal cations and the cations of the second metal; and
b. ion exchanging the cations of the third metal from the second molten salt bath for at least one of the first metal cations and the cations of the second metal in the alkali aluminosilicate glass at a temperature of greater than about 420° C. and at least about 30° C. less than the anneal point, wherein ion exchanging in the second molten salt bath forms a surface region comprising the cations of the third metal.

### Claim 18 (depends on 17)

The method of claim 17, wherein the second molten salt bath is substantially free of the first metal cations.

### Claim 19 (depends on 17)

The method of claim 17, wherein the third metal is cesium or rubidium.

### Claim 20 (depends on 1)

The method of claim 1, further comprising:
a. immersing the alkali aluminosilicate glass in a second molten salt bath, the second molten salt bath comprising at least one salt of the second metal; and
b. ion exchanging the cations of the second metal from the second molten salt bath for the first metal cations in the alkali aluminosilicate glass at a temperature of less than or equal to about 420° C., wherein the surface compressive stress is formed by ion exchanging in the second molten salt bath creates a maximum compressive stress at the surface.

### Claim 21 (depends on 20)

The method of claim 20, wherein the second molten salt bath is substantially free of the first metal cations.

### Claim 22 (depends on 21)

The method of claim 21, wherein the first metal cations are sodium cations.

### Claim 23

An alkali aluminosilicate glass article, the alkali aluminosilicate glass article having a region under a compressive stress, the region extending from a surface of the alkali aluminosilicate glass article to a depth of layer of at least about 40 μm within the alkali aluminosilicate glass article, wherein the alkali aluminosilicate glass article has a compressive stress at the surface and a first compressive stress at a first depth, the first depth being between about 30% and about 70% of the depth of layer, wherein the first compressive stress is at least about 50% of the compressive stress at the surface.

### Claim 24 (depends on 23)

The alkali aluminosilicate glass article of claim 23, wherein the compressive stress at the surface is at least about 100 MPa.

### Claim 25 (depends on 23)

The alkali aluminosilicate glass article of claim 23, wherein the first depth is about 25 μm.

### Claim 26 (depends on 25)

The alkali aluminosilicate glass article of claim 25, wherein the first compressive stress is at least about 350 MPa.

### Claim 27 (depends on 25)

The alkali aluminosilicate glass article of claim 25, wherein the alkali aluminosilicate glass article has a retained strength of at least about 200 MPa.

### Claim 28 (depends on 23)

The alkali aluminosilicate glass article of claim 23, wherein the alkali aluminosilicate glass article comprises at least about 50 mol % SiO2 and at least about 11 mol % Na2O, and wherein the compressive stress at the surface is at least about 900 MPa.

### Claim 29 (depends on 28)

The alkali aluminosilicate glass article of claim 28, wherein the alkali aluminosilicate glass article further comprises Al2O3 and at least one of B2O3, K2O, MgO and ZnO, and wherein −340+27.1·Al2O3−28.7·B2O3+15.6·Na2O−61.4·K2O+8.1·(MgO+ZnO)≧0 mol %.