# US 2015/0147569 A1 · Thermo-regulated fiber and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147569 A1
- Document ID: US20150147569A1
- Status: Published application
- Kind: A1
- Application number: 14/412,184
- Filed: 2013-03-21
- Published: 2015-05-28
- Earliest claimed: 2012-07-03
- Applicants: Tianjin Polytechnic University
- Inventors: Xing Xiang Zhang; Jie Yun Meng; Xiao Fen Tang; Hai Feng Shi
- Web page: https://patentgrep.com/patent/US20150147569A1

## CPC

- D01F 8/16: with at least one other macromolecular compound obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds as constituent
- B29C 48/05: Filamentary, e.g. strands
- D01D 5/003: {the material being a polymer solution or dispersion (D01D5/0053 takes precedence)}
- D01D 5/06: Wet spinning methods {(D01D5/0046 takes precedence)}
- D01D 5/08: Melt spinning methods {(D01D5/0023 takes precedence)}
- D01D 5/34: Core-skin structure; Spinnerette packs therefor
- D01D 5/36: Matrix structure; Spinnerette packs therefor
- D01F 8/06: with at least one polyolefin as constituent
- D01F 8/08: with at least one polyacrylonitrile as constituent
- D01F 8/12: with at least one polyamide as constituent
- D01F 8/14: with at least one polyester as constituent
- B29K 2067/04: {Polyesters derived from hydroxycarboxylic acids}
- B29L 2031/731: {Filamentary material, i.e. comprised of a single element, e.g. filaments, strands, threads, fibres (cables B29L2031/707)}
- D10B 2321/021: polyethylene
- D10B 2321/041: polyvinyl chloride or polyvinylidene chloride
- D10B 2321/10: polymers of unsaturated nitriles, e.g. polyacrylonitrile, polyvinylidene cyanide
- D10B 2331/02: polyamides (D10B2331/08 takes precedence)
- D10B 2331/04: polyesters, e.g. polyethylene terephthalate [PET]
- Y10T 428/2929: Bicomponent, conjugate, composite or collateral fibers or filaments [i.e., coextruded sheath-core or side-by-side type]
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention provides a thermo-regulated fiber and a preparation method thereof by using a new polymeric phase-change material and adopting a new fiber preparation method, and the resulting thermo-regulated fiber has good thermo-regulating properties and a good thermal stability. The thermo-regulated fiber has a composite structure, and the cross-sectional structure is an sea-island type or a concentric sheath/core type, characterised in that the polymeric phase-change material is a polyethylene glycol n-alkyl ether (structural formula: H(OCH2CH2)mOCnH2n+1), where the repeating unit number m of the ethylene glycol is 1 to 100, the number n of carbon atoms in the n-alkyl is 11 to 30. The present invention further relates to a preparation method of a thermo-regulated fiber which includes one of the following processes: (1) A melt composite spinning process; (2) Solution composite spinning process; (3) Electrostatic solution composite spinning process. Further, the present invention is characterised as follows: (1) a new polymeric phase-change material polyethylene glycol n-alkyl ether is used; (2) Component A of the thermo-regulated fiber may form a continuous crystallization region; (3) The thermo-regulated fiber can be prepared in various forms by many preparation methods such as melt composite spinning, solution composite spinning and solution static composite spinning.

## Claims

### Claim 1

A thermo-regulated fiber, comprising a polymeric phase-change material as an ingredient A and a fiber-forming polymer as an ingredient B, wherein the mass fraction of the ingredient A in the fiber is 20% to 60%, the mass fraction of the ingredient B in the fiber is 80% to 40%, and the fiber is prepared by a melt composite spinning, solution composite spinning or solution static composite spinning process, the thermo-regulated fiber has a composite structure, the cross-sectional structure is a sea-island type or a concentric sheath/core type, characterized in that the polymeric phase-change material is a polyethylene glycol n-alkyl ether, wherein the number m of the ethylene glycol repeating unit is 1 to 100, the number n of carbon atoms in the n-alkyl is 11 to 30; when the thermo-regulated fiber is prepared by adopting a melt composite spinning process, the fiber-forming polymer comprises at least one of a copolyester, a copolyamide, polyethylene, polypropylene, poly-4-methylpentene-1, acrylonitrile-methyl acrylate copolymer, acrylonitrile-crotononitrile copolymer and polycaprolactam; when the thermo-regulated fiber is prepared by adopting a solution composite spinning or solution static composite spinning process, the fiber-forming polymer comprises at least one of acrylonitrile, acrylonitrile-vinylidene chloride copolymer, and acrylonitrile-vinyl chloride copolymer; the heat absorption temperature and the heat release temperature of fiber are in the range of 11.9° C. to 53.8° C., the heat storage capacity is 18 to 55 J/g, and the 5% weight-loss temperature is 203° C. and more.

### Claim 2 (depends on 1)

The thermo-regulated fiber according to claim 1, wherein the number m of the ethylene glycol repeating unit is 2 to 20, the number n of carbon atoms in the n-alkyl is 12 to 25.

### Claim 3 (depends on 1)

A method for preparing the thermo-regulated fiber according to claim 1 by adopting a melt composite spinning process, comprising:
respectively extruding a polymeric phase-change material component A and a fiber-forming polymer component B having a moisture content of 50 to 150 ppm by a single screw extruder or twin screw extruder at 180° C. to 250° C. after being melted, and entering a metering pump; sending the polymeric phase-change material component A and the fiber-forming polymer component B into a composite spinning assembly of which the temperature is set at 180° C. to 250° C. through a connecting conduit; compounding after passing through a filter screen and a distributing plate respectively; forming spinning threads by a spinneret, cooling by the air, and collecting after being wound or directly collecting without being wound, to obtain an as-spun fiber; processing the as-spun fiber by process such as drawing, molding, curling or twisting, to obtain a thermo-regulated filament, or further processing the as-spun fiber, to obtain a thermo-regulated staple fiber, wherein the spinneret is a sea-island type or a concentric sheath/core type.

### Claim 4 (depends on 1)

A method for preparing the thermo-regulated fiber according to claim 1 by adopting a solution composite spinning process, comprising:
melting and degassing a polymeric phase-change material ingredient A having a moisture content of 50 to 150 ppm in a polymerizer, and dissolving a fiber-forming polymer ingredient B having a moisture content of 50 to 150 ppm in a solvent in a polymerizer, to obtain a solution in which the mass fraction of the polymer is 10% to 30%, and degassing the solution; respectively sending the melted polymeric phase-change material ingredient A and the solution into a metering pump, and then sending into a composite spinning assembly of which the temperature is set at 50° C. to 80° C. through a connecting conduit; compounding after passing through a filter screen and a distributing plate respectively, and forming spinning threads by a spinneret; coagulating the spinning threads in a coagulation bath or spinning tunnel, and drawing, drying and molding, to obtain a thermo-regulated staple fiber or filament; the solvent is dimethyl sulfoxide, N,N-dimethylformamide or N,N-dimethylacetamide; and the spinneret is a sea-island type or a concentric sheath/core type.

### Claim 5 (depends on 1)

A method for preparing the thermo-regulated fiber according to claim 1 by adopting a solution static composite spinning process, comprising:
melting and degassing a polymeric phase-change material ingredient A having a moisture content of 50 to 150 ppm in a polymerizer, and dissolving a fiber-forming polymer ingredient B having a moisture content of 50 to 150 ppm in a solvent in a polymerizer, to obtain a solution in which the mass fraction of the polymer is 10% to 30%, and degassing the solution; respectively sending the melted polymeric phase-change material ingredient A and the solution into a metering pump, and then sending into a composite spinning assembly of which the temperature is set at 50° C. to 80° C. through a connecting duct, and compounding after passing through a filter screen and a distributing plate respectively, and forming spinning threads by a spinneret, and drawing the threads in the presence of a high-voltage electric field of 10 to 60 kV, to form a fiber net on a collecting plate or fiber bundles on a collecting wheel; the solvent is dimethyl sulfoxide, N,N-dimethylformamide or N,N-dimethylacetamide; and the spinneret is a sea-island type or a concentric sheath/core type.