# US 2015/0147557 A1 · Processes for enhancing flame retardance and chemical resistance of polymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147557 A1
- Document ID: US20150147557A1
- Status: Published application
- Kind: A1
- Application number: 14/607,399
- Filed: 2015-01-28
- Published: 2015-05-28
- Earliest claimed: 2012-12-20
- Assignees: Sabic Global Technologies B.V.
- Applicants: SABIC Global Technologies B.V.
- Inventors: Jean-Francois Morizur; Paul Dean Sybert; Amanda Marie Flores; Peter Johnson; Andrew Frazee; Thomas L. Evans
- Web page: https://patentgrep.com/patent/US20150147557A1

## CPC

- C08G 64/14: containing a chain-terminating or -crosslinking agent
- B05D 3/067: {Curing or cross-linking the coating}
- B29C 35/08: by wave energy or particle radiation {(B29C64/00, B29C71/04 take precedence)}
- B29C 35/0805: {using electromagnetic radiation}
- B29C 45/0001: {characterised by the choice of material}
- C08G 64/045: {containing aliphatic unsaturation}
- C08G 64/24: and phenols
- C08G 67/00: Macromolecular compounds obtained by reactions forming in the main chain of the macromolecule a linkage containing oxygen or oxygen and carbon, not provided for in groups C08G2/00 - C08G65/00
- C08J 3/28: Treatment by wave energy or particle radiation
- C08J 7/123: {Treatment by wave energy or particle radiation (C08J7/18 takes precedence)}
- C08K 5/3475: condensed with carbocyclic rings
- C08K 5/42: Sulfonic acids; Derivatives thereof
- C08K 5/52: Phosphorus bound to oxygen only
- C08K 5/5393: Phosphonous compounds, e.g. R—P(OR')2
- C08K 5/549: containing silicon in a ring
- C08L 69/00: Compositions of polycarbonates; Compositions of derivatives of polycarbonates
- B29C 2035/0827: {using UV radiation}
- B29K 2069/00: Use of PC, i.e. polycarbonates {or derivatives thereof}, as moulding material
- B29K 2105/0026: {Flame proofing or flame retarding agents}
- B29K 2105/24: crosslinked or vulcanised
- B29K 2269/00: Use of {PC, i.e.} polycarbonates {or derivatives thereof} as reinforcement
- C08J 2369/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- C08J 2469/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- C08L 2201/02: Flame or fire retardant/resistant
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2312/06: by radiation
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

Processes for increasing the chemical resistance of a surface of a formed article are disclosed. The formed article is produced from a polymeric composition comprising a photoactive additive containing photoactive groups derived from a monofunctional benzophenone. The surface of the formed article is then exposed to ultraviolet light to cause crosslinking of the photoactive additive and produce a crosslinked surface. The crosslinking enhances the chemical resistance of the surface. Various means for controlling the depth of the crosslinking are also discussed.

## Claims

### Claim 1

A method for forming a cross-linked polycarbonate article, comprising:
providing a composition that comprises:
a cross-linkable polycarbonate resin having endcaps derived from a monohydroxybenzophenone, a weight average molecular weight (Mw) from 15,000 to 30,000 and a PDI from 3.0 to 4.0 as measured by GPC using a UV detector and polycarbonate standards, and a monohydroxybenzophenone-derived endcap content from 3.0 to 4.5 wt %;
optionally one or more additional polycarbonate base resins different from the cross-linkable polycarbonate resin; and
a flame retardant;
wherein the monohydroxybenzophenone-derived endcap content of the composition is between 1.2 wt % and 4 wt %, and wherein the composition has a melt flow rate (MFR) of 7 to 20 g/10 min measured at 300° C./1.2 kg/360 sec dwell;
forming an article from the composition; and
exposing the formed article to UV radiation from a UV radiation source for a time sufficient to form the cross-linked polycarbonate article;
wherein the cross-linked polycarbonate article has a gel layer of at least 5 microns thickness as measured by optical microscopy, and wherein the molded article after exposure to UV radiation has a pFTP(V1) of at least 0.95 at 1.2 mm thickness after aging for 7 days at 70° C.

### Claim 2 (depends on 1)

The method of claim 1, wherein the UV radiation source is a metal halide doped mercury lamp, an electrodeless D-bulb, an electrodeless H-bulb, an electrodeless V-bulb, a Xenon Arc lamp, or a UVA (320-390 nm) light emitting diode (LED).

### Claim 3 (depends on 1)

The method of claim 1, wherein the UV radiation source is a metal halide doped mercury lamp or an electrodeless D-bulb.

### Claim 4 (depends on 3)

The method of claim 3, wherein the molded article is exposed to UV radiation from a metal halide doped mercury lamp providing at least 12 J/cm2 of UVA as measured using an EIT PowerPuck.

### Claim 5 (depends on 3)

The method of claim 3, wherein the molded article is exposed to UV radiation from a metal halide doped mercury lamp providing at least 35.9 J/cm2 of UVA as measured using an EIT PowerPuck.

### Claim 6 (depends on 3)

The method of claim 3, wherein the molded article is exposed to UV radiation from a metal halide doped mercury lamp providing at least 59.9 J/cm2 of UVA as measured using an EIT PowerPuck.

### Claim 7 (depends on 1)

The method of claim 1, wherein the molded article is exposed to filtered UV radiation using a 280 nm long pass filter.

### Claim 8 (depends on 1)

The method of claim 1, wherein the molded article is exposed to filtered UV radiation using a 320 nm long pass filter.

### Claim 9 (depends on 1)

The method of claim 1, wherein the article is formed by injection molding.

### Claim 10

A method for preparing an injection-molded article having low yellowness and high chemical resistance, comprising:
receiving a composition that comprises:
a cross-linkable polycarbonate resin having endcaps derived from a monohydroxybenzophenone, a weight average molecular weight (Mw) from 15,000 to 30,000 and a PDI from 3.0 to 4.0 as measured by GPC using a UV detector and polycarbonate standards, and a monohydroxybenzophenone-derived endcap content from 3.0 to 4.5 wt %;
optionally one or more additional polycarbonate base resins different from the cross-linkable polycarbonate resin; and
optionally a flame retardant;
wherein the composition has a melt flow rate (MFR) of 7 g/10 min or higher, measured at 300° C./1.2 kg/360 sec dwell;
injection-molding the composition to a molded article; and
exposing the molded article to a selected UV light range and a selected dosage of UV radiation to obtain the injection-molded article, wherein the injection molded article has a YI of 15 or less at 3.2 mm thickness when measured at least 48 hours after UV exposure, and has a % retention of 85% or greater at 3.2 mm thickness in a tensile elongation at break test using the ASTM D638 Type I method at 50 mm/min after exposure to acetone under 1.0% strain at 23° C.

### Claim 11 (depends on 10)

The method of claim 10, wherein the injection molded article has a pFTP(V1) of at least 0.70 at 1.2 mm thickness after aging for 7 days at 70° C.

### Claim 12 (depends on 10)

The method of claim 10, wherein the injection molded article has a YI of 8 or less.

### Claim 13 (depends on 10)

The method of claim 10, wherein the composition has a melt flow rate (MFR) of 7 to 20 g/10 min.

### Claim 14 (depends on 10)

The method of claim 10, wherein the composition comprises Rimar salt flame retardant, and the injection molded article has a pFTP(V1) of at least 0.70 at 1.2 mm thickness after aging for 7 days at 70° C.

### Claim 15 (depends on 10)

The method of claim 10, wherein the composition comprises Rimar salt flame retardant, and the injection molded article has a pFTP(V1) of at least 0.90 at 1.2 mm thickness after aging for 7 days at 70° C.

### Claim 16 (depends on 10)

The method of claim 10, wherein the composition comprises Rimar salt flame retardant, and the injection molded article has a pFTP(V0) of at least 0.60 at 1.2 mm thickness after aging for 7 days at 70° C.

### Claim 17

A composition, comprising:
a cross-linkable polycarbonate resin having endcaps derived from a monohydroxybenzophenone and a weight average molecular weight (Mw) from 15,000 to 30,000 and a PDI from 3.0 to 4.0 as measured by GPC using a UV detector and polycarbonate standards;
optionally one or more additional polycarbonate base resins different from the cross-linkable polycarbonate resin; and
a flame retardant;
wherein the composition comprises at least 45 wt % of the cross-linkable polycarbonate resin, wherein the monohydroxybenzophenone-derived endcap content of the composition is between 1.2 wt % and 4 wt %, wherein the composition has a melt flow rate (MFR) of 7 to 20 g/10 min measured at 300° C./1.2 kg/360 sec dwell, and wherein an article formed from the composition has a % T of 85% or greater at 3.2 mm thickness.

### Claim 18 (depends on 17)

A molded article formed from the composition of claim 17, wherein after irradiation with UV light, the article has (a) a % T of 75% or greater at 3.2 mm thickness, and (b) either:
(i) a gel layer of at least 8 microns thickness as measured by optical microscopy; or
(ii) an increase in Mw of at least 30% as measured by GPC using a UV detector and polycarbonate standards.

### Claim 19 (depends on 18)

The molded article of claim 18, wherein the article has a pFTP(V1) of at least 0.95 at 1.2 mm thickness after aging for 7 days at 70° C.

### Claim 20 (depends on 18)

The molded article of claim 18, wherein the article has a delta YI value of 12 or less at 3.2 mm thickness measured at least 48 hours after UV exposure.

### Claim 21 (depends on 18)

The molded article of claim 18, wherein the article has a pFTP(V0) of at least 0.6 at 1.2 mm thickness.

### Claim 22 (depends on 18)

The molded article of claim 18, wherein the article has a % retention of 85% or greater at 3.2 mm thickness in a tensile elongation at break test using the ASTM D638 Type I method at 50 mm/min after exposure to acetone under 1% strain at 23° C.

### Claim 23 (depends on 22)

The molded article of claim 22, wherein the article has a delta YI of less than 12 at 3.2 mm thickness measured at least 48 hours after UV exposure.

### Claim 24 (depends on 22)

The molded article of claim 22, wherein the article has a pFTP(V1) of at least 0.95 at 1.2 mm thickness after aging for 7 days at 70° C.

### Claim 25 (depends on 18)

The molded article of claim 18, wherein the article has a % retention of 90% or greater at 3.2 mm thickness in a tensile elongation at break test using the ASTM D638 Type I method at 50 mm/min after exposure to acetone under 1% strain at 23° C.

### Claim 26 (depends on 25)

The molded article of claim 25, wherein the article has a delta YI of less than 12 at 3.2 mm thickness measured at least 48 hours after UV exposure.

### Claim 27 (depends on 25)

The molded article of claim 25, wherein the article has a pFTP(V1) of at least 0.95 at 1.2 mm thickness after aging for 7 days at 70° C.