# US 2015/0147538 A1 · Chemically strengthened glass plate, cover glass, chemically strengthened glass with touch sensor, and display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147538 A1
- Document ID: US20150147538A1
- Status: Published application
- Kind: A1
- Application number: 14/552,998
- Filed: 2014-11-25
- Published: 2015-05-28
- Earliest claimed: 2012-05-25
- Assignees: Asahi Glass Company, Limited
- Applicants: Asahi Glass Company, Limited
- Inventors: Masayuki ISHIMARU; Hiroyuki OKAWA; Syusaku AKIBA; Shigeki SAWAMURA; Kazutaka ONO; Tetsuya NAKASHIMA; Izuru KASHIMA; Yusuke KOBAYASHI; Suguru MURAYAMA; Aya YAMAMOTO
- Web page: https://patentgrep.com/patent/US20150147538A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 3/085: containing an oxide of a divalent metal
- Y10T 428/24777: Edge feature
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A chemically strengthened glass sheet, which has front and back main surfaces and an edge surface between the front and back main surfaces, has undergone a chemical strengthening treatment and has an approximately rectangular shape, in which the chemically strengthened glass sheet has a surface compressive stress of 800 MPa or more, and an internal tensile stress of 42 MPa or less.

## Claims

### Claim 1

A chemically strengthened glass sheet, which has front and back main surfaces and an edge surface between the front and back main surfaces,
wherein the chemically strengthened glass sheet has a surface compressive stress of 800 MPa or more, and an internal tensile stress of 42 MPa or less,
the edge surface has a chamfered part, and a part of the chamfered part where a distance from the main surface adjacent to the chamfered part toward a sheet thickness direction is ⅕ or less of a sheet thickness has no latent flaw deeper than 20 μm, and
the chemically strengthened glass sheet contains, in terms of mol % on the basis of oxides, from 56 to 75% of SiO2, from 5 to 20% of Al2O3, from 8 to 22% of Na2O, from 0 to 10% of K2O, from 0 to 14% of MgO, from 0 to 5% of ZrO2 and from 0 to 5% of CaO.

### Claim 2 (depends on 1)

The chemically strengthened glass sheet according to claim 1, which has the surface compressive stress of 850 MPa or more.

### Claim 3 (depends on 1)

The chemically strengthened glass sheet according to claim 1, which has the internal tensile stress of 35 MPa or less.

### Claim 4 (depends on 3)

The chemically strengthened glass sheet according to claim 3, which has the internal tensile stress of 30 MPa or less.

### Claim 5 (depends on 1)

The chemically strengthened glass sheet according to claim 1, which has a thickness of a surface compressive stress layer of from 15 to 40 μm.

### Claim 6 (depends on 5)

The chemically strengthened glass sheet according to claim 5, which has the thickness of the surface compressive stress layer of from 20 to 35 μm.

### Claim 7 (depends on 1)

The chemically strengthened glass sheet according to claim 1, which has a sheet thickness of 0.8 mm or less.

### Claim 8 (depends on 1)

The chemically strengthened glass sheet according to claim 1, wherein a total content of SiO2, Al2O3, Na2O, MgO and B2O3 is 98% or more.

### Claim 9 (depends on 1)

The chemically strengthened glass sheet according to claim 1, wherein a total content of SiO2, Al2O3, Na2O and MgO is 98% or more.

### Claim 10 (depends on 1)

The chemically strengthened glass sheet according to claim 1, wherein a difference resulting from subtracting an Al2O3 content from a Na2O content is less than 5%.

### Claim 11 (depends on 1)

The chemically strengthened glass sheet according to claim 1, wherein the part of the chamfered part where the distance from the main surface adjacent to the chamfered part toward the sheet thickness direction is ⅕ or less of the sheet thickness has no latent flaw of 10 μm or deeper.

### Claim 12 (depends on 1)

The chemically strengthened glass sheet according to claim 1, wherein a touch sensor is provided on the main surface.

### Claim 13

A chemically strengthened glass sheet, which has front and back main surfaces and an edge surface between the front and back main surfaces,
wherein the chemically strengthened glass sheet has a surface compressive stress of 800 MPa or more, and an internal tensile stress of 42 MPa or less,
the edge surface has a chamfered part, and a part of the chamfered part where a distance from the main surface adjacent to the chamfered part toward a sheet thickness direction is ⅕ or less of a sheet thickness has no latent flaw deeper than 20 μm, and
the chemically strengthened glass sheet contains, in terms of mol % on the basis of oxides, from 60 to 75% of SiO2, from 11 to 15% of Al2O3, from 11 to 16% of Na2O, from 0 to 5% of K2O, from 0 to 10% of MgO, from 0 to 1% of ZrO2 and from 0 to 5% of CaO.

### Claim 14 (depends on 13)

The chemically strengthened glass sheet according to claim 13, which has the surface compressive stress of 850 MPa or more.

### Claim 15 (depends on 13)

The chemically strengthened glass sheet according to claim 13, which has the internal tensile stress of 35 MPa or less.

### Claim 16 (depends on 15)

The chemically strengthened glass sheet according to claim 15, which has the internal tensile stress of 30 MPa or less.

### Claim 17 (depends on 13)

The chemically strengthened glass sheet according to claim 13, which has a thickness of a surface compressive stress layer of from 15 to 40 μm.

### Claim 18 (depends on 17)

The chemically strengthened glass sheet according to claim 17, which has the thickness of the surface compressive stress layer of from 20 to 35 μm.

### Claim 19 (depends on 13)

The chemically strengthened glass sheet according to claim 13, which has a sheet thickness of 0.8 mm or less.

### Claim 20 (depends on 13)

The chemically strengthened glass sheet according to claim 13, wherein a total content of SiO2, Al2O3, Na2O, MgO and B2O3 is 98% or more.