# US 2015/0147486 A1 · Photosintering of micron-sized copper particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147486 A1
- Document ID: US20150147486A1
- Status: Published application
- Kind: A1
- Application number: 14/413,294
- Filed: 2013-07-09
- Published: 2015-05-28
- Earliest claimed: 2012-07-09
- Assignees: PEN Inc.
- Applicants: Pen Inc.
- Inventors: Ovadia Abed; Valerie Kaye Ginsberg; James P. Novak
- Web page: https://patentgrep.com/patent/US20150147486A1

## CPC

- C23C 24/106: {Coating with metal alloys or metal elements only}
- C09D 11/52: Electrically conductive inks
- H01B 1/22: the conductive material comprising metals or alloys
- H05K 1/097: {Inks comprising nanoparticles and specially adapted for being sintered at low temperature (H05K1/095 takes precedence)}
- H05K 3/1283: {After-treatment of the printed patterns, e.g. sintering or curing methods}
- H05K 2203/1545: Continuous processing, i.e. involving rolls moving a band-like or solid carrier along a continuous production path
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

Micron-sized metal particles in an ink or paste composition are deposited onto a substrate and then photosimered. The substrate may comprise a polymeric material. The polymeric substrate may have a coefficient of thermal expansion greater than two times the coefficient of thermal expansion of the photosimered ink or paste composition.

## Claims

### Claim 1

A method for making a conductive film comprising:
depositing an ink or paste composition comprising micron-sized metal particles onto a polymeric substrate having a melting point less than 200° C., wherein the micron-sized metal particles in the ink or paste composition have an average particle size greater than one micron;
and
photosintering the ink or paste composition after being deposited onto the substrate.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein the polymeric substrate has a thermal conductivity greater than 0.1 W/mK.

### Claim 3 (depends on 1)

The method as recited in claim 1, wherein the average particle size of the micron-sized metal particles in the ink or paste composition is less than three microns.

### Claim 4 (depends on 1)

The method as recited in claim 1, wherein the photosintering is performed with a broad spectrum light source.

### Claim 5 (depends on 1)

The method as recited in claim 1, wherein the melting point is less than 150° C.

### Claim 6 (depends on 1)

The method as recited in claim 1, wherein the metal particles comprise copper.

### Claim 7 (depends on 1)

The method as recited in claim 1, wherein the metal particles are selected from the group consisting of Ag, Ni, Al, and Fe.

### Claim 8 (depends on 1)

The method as recited in claim 1, wherein the polymeric substrate is comprised of PET.

### Claim 9 (depends on 1)

The method as recited in claim 1, wherein the photosintered metal particles are connected to each other with necks.

### Claim 10 (depends on 1)

The method as recited in claim 1, wherein the polymeric substrate has a coefficient of thermal expansion greater than two times the coefficient of thermal expansion of the photosintered ink or paste composition.

### Claim 11 (depends on 1)

The method as recited in claim 1, wherein the photosintering causes some of the metal particles to become physically embedded into a surface of the polymeric substrate.

### Claim 12 (depends on 1)

The method as recited in claim 1, wherein the photosintered ink or paste composition has a resulting resistivity less than 10−4 ohm-cm.

### Claim 13 (depends on 1)

The method as recited in claim 1, wherein the melting point is less than 150° C.

### Claim 14 (depends on 1)

The method as recited in claim 1, wherein the micron-sized metal particles in the ink or paste composition have an average particle size greater than two microns.

### Claim 15 (depends on 1)

The method as recited in claim 1, wherein during the photosintering of the ink or paste composition, some heat generated in the micron-sized metal particles as a result of the photosintering is transferred from the particles into the substrate to reduce ramping up of the heat within the particles, which also results in a partial melting of a surface of the substrate so that some of the particles physically embed into the substrate surface.

### Claim 16 (depends on 6)

The method as recited in claim 6, wherein the ink or paste composition has a formulation comprising about 50 wt. % concentration of the micron-sized copper particles, about 48 wt. % concentration of a binder solution, and about 2 wt. % concentration of a dispersant.

### Claim 17 (depends on 1)

The method as recited in claim 1, wherein the photosintered ink or paste composition has a resulting resistivity of at least about 6×10−5 ohm-cm.

### Claim 18 (depends on 1)

The method as recited in claim 1, wherein the polymeric substrate is selected from the group consisting of polyvinyl chloride, polycarbonate, polystyrene, polyethylene, and polypropylene.

### Claim 19

A method for making a conductive film, comprising:
depositing an ink or paste composition comprising micron-sized metal particles onto a polymeric substrate having a melting point less than 200° C. and a thermal conductivity greater than 0.1 W/mK, wherein the micron-sized metal particles in the ink or paste composition have an average particle size greater than two microns; and
photosintering the ink or paste composition after being deposited onto the substrate, wherein during the photosintering of the ink or paste composition, some heat generated in the micron-sized metal particles as a result of the photosintering is transferred from the micron-sized metal particles into the polymeric substrate to reduce ramping up of the heat within the micron-sized metal particles, which also results in a partial melting of a surface of the polymeric substrate so that some of the micron-sized metal particles physically embed into the polymeric substrate surface.

### Claim 20 (depends on 19)

The method as recited in claim 19, wherein the melting point of the polymeric substrate is less than 150° C.