# US 2015/0147483 A1 · Method for Forming Conformal Nitrided, Oxidized, or Carbonized Dielectric Film by Atomic Layer Deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147483 A1
- Document ID: US20150147483A1
- Status: Published application
- Kind: A1
- Application number: 14/090,750
- Filed: 2013-11-26
- Published: 2015-05-28
- Earliest claimed: 2013-11-26
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Atsuki Fukazawa
- Web page: https://patentgrep.com/patent/US20150147483A1

## CPC

- C23C 16/345: {Silicon nitride}
- C23C 16/4554: {Plasma being used non-continuously in between ALD reactions (C23C16/56 takes precedence)}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method for forming a film on a patterned surface of a substrate by atomic layer deposition (ALD) processing includes: adsorbing onto a patterned surface a first precursor containing silicon or metal in its molecule; adsorbing onto the first-precursor-adsorbed surface a second precursor containing no silicon or metal in its molecule; exposing the second-precursor-adsorbed surface to an excited reactant to oxidize, nitride, or carbonize the precursors adsorbed on the surface of the substrate; and repeating the above cycle to form a film on the patterned surface of the substrate.

## Claims

### Claim 1

A method for forming a film on a patterned surface of a substrate by atomic layer deposition (ALD) processing, said surface being patterned with a recess having side walls and a bottom, said method comprising:
(i) adsorbing a non-excited gas of a first precursor onto a patterned surface of a substrate in a reaction space, said first precursor containing silicon or metal in its molecule;
(ii) adsorbing a non-excited gas of a second precursor onto the first-precursor-adsorbed surface of the substrate in the reaction space, said second precursor containing no silicon or metal in its molecule;
(iii) exposing the second-precursor-adsorbed surface of the substrate to an excited gas of a reactant in the reaction space to oxidize, nitride, or carbonize the precursors adsorbed on the surface of the substrate, said reactant having a smaller molecular size than the second precursor; and
(iv) repeating steps (i) to (iii) to form a film on the patterned surface of the substrate.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the second precursor is at least one compound selected from the group consisting of CxHyOz, CxOy, and NxCyOz (x, y, and z are integers), and the reactant is selected from the group consisting of O2, O3, CO2, H2O, and N2O, whereby the excited reactant oxidizes the precursors adsorbed on the surface of the substrate.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the second precursor is at least one compound selected from the group consisting of CxNyHz and NxHy (x, y, and z are integers), and the reactant is selected from the group consisting of N2, N2 and H2, NH3, NxHy, and NxHyCz (x, y, and z are integers), whereby the excited reactant nitrides the precursors adsorbed on the surface of the substrate.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the second precursor is at least one compound selected from the group consisting of CxHy and CxNyHz (x, y, and z are integers), and the reactant is selected from the group consisting of H2, N2, Ar, and He, whereby the excited reactant carbonizes the precursors adsorbed on the surface of the substrate.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the first precursor is a halide compound.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the first precursor is at least one selected from the group consisting of dichlorodiethylsilane, dichlorodimethylsilane, dichlorotetramethyldisilazane, dichlorotetraethyldisilazane, dichloroethylsilane, dichloromethylsilane, diiodomethylsilane, diiodoethylsilane.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the first precursor is an aminosilane compound.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the first precursor is at least one selected from the group consisting of bis(diethylamino)silane and bis(dimethylamino)silane.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the first precursor contains a metal selected from the group consisting of Ti, Zr, Al, and Mn.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the first and second precursors are organic compounds which are liquid at room temperature.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the adsorbed weight of the second precursor in step (ii) is equivalent to or higher than the adsorbed weight of the first precursor in step (i).

### Claim 12 (depends on 1)

The method according to claim 1, wherein the reactant is excited by heat and/or a plasma in step (iii).

### Claim 13 (depends on 12)

The method according to claim 12, wherein the reactant is excited by a plasma generated by applying RF power to the reaction space.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the reactant is continuously supplied to the reaction space throughout steps (i) to (iii), and RF power is applied in step (iii).

### Claim 15 (depends on 14)

The method according to claim 14, further comprising applying RF power to the reaction space between steps (i) and (ii).

### Claim 16 (depends on 13)

The method according to claim 13, wherein the reactant is supplied only during step (iii), and RF power is applied in step (iii).

### Claim 17 (depends on 16)

The method according to claim 16, further comprising applying RF power to the reaction space between steps (i) and (ii).

### Claim 18 (depends on 1)

The method according to claim 1, further comprising, after step (iv), (v) exposing the film on the substrate to a plasma of an inert gas, a hydrogen-containing gas, ammonium-containing gas, and/or oxidizing gas.

### Claim 19 (depends on 1)

The method according to claim 1, wherein a rare gas is continuously supplied to the reaction space throughout steps (i) to (iii).

### Claim 20 (depends on 1)

The method according to claim 1, further comprising purging the reaction space between steps (i) and (ii), between steps (ii) and (iii), and between steps (iii) and (i).