# US 2015/0147466 A1 · Method for depositing photoluminescent material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147466 A1
- Document ID: US20150147466A1
- Status: Published application
- Kind: A1
- Application number: 14/614,996
- Filed: 2015-02-05
- Published: 2015-05-28
- Earliest claimed: 2013-11-21
- Assignees: Ford Global Technologies, LLC
- Applicants: Ford Global Technologies, LLC
- Inventors: Paul Kenneth Dellock; Stuart C. Salter; Cornel Lewis Gardner; Talat Karmo; Arsen Terjimanian
- Web page: https://patentgrep.com/patent/US20150147466A1

## CPC

- C09K 11/00: Luminescent materials, e.g. electroluminescent or chemiluminescent
- B60Q 3/68: using ultraviolet light
- C09K 2211/00: Chemical nature of organic luminescent or tenebrescent compounds
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- B60Q: ARRANGEMENT OF SIGNALLING OR LIGHTING DEVICES, THE MOUNTING OR SUPPORTING THEREOF OR CIRCUITS THEREFOR, FOR VEHICLES IN GENERAL

## Abstract

A method of depositing a photoluminescent material into a surface of the polymeric material is disclosed. The method comprises dissolving the photoluminescent material in water to create a solution. The temperature of the solution is then controlled at a predetermined temperature. The surface is contacted by the solution at the predetermined temperature for a predetermined time, thereby infusing the surface with the photoluminescent material. Following the predetermined time, the solution is removed from the surface by rinsing the surface with water.

## Claims

### Claim 1

A method of depositing a photoluminescent material into a surface of a polymeric material comprising the steps of:
dissolving the photoluminescent material in water to create a solution;
controlling a temperature of the solution at a predetermined temperature;
contacting the surface with the solution for a predetermined time to infuse the surface with the photoluminescent material; and
rinsing the solution from the surface.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the polymeric material corresponds to a molded part.

### Claim 3 (depends on 1)

The method according to claim 1, wherein contacting the surface with the solution comprises submerging the molded part in the solution.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the predetermined temperature is approximately between 25 degrees Celsius to 100 degrees Celsius.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the predetermined time is approximately less than one second to approximately 20 minutes.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the predetermined time is approximately 30 second to 3 minutes.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the predetermined time decreases in response to the predetermined temperature being increased.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the solution comprises a percentage of photoluminescent material of approximately 0.001% to 15% by weight.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the solution comprises a percentage of photoluminescent material of approximately 0.01 to 0.5% by weight.

### Claim 10

A method for infusing a molded polymeric part with a photoluminescent material comprising:
dissolving the photoluminescent material in a fluid to create a solution;
controlling a temperature of the solution at a predetermined temperature;
submerging a surface of the part in the solution for a predetermined time to infuse the surface with the photoluminescent material; and
rinsing the solution from the surface with a rinse fluid.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the predetermined time is approximately 30 seconds to 3 minutes.

### Claim 12 (depends on 10)

The method according to claim 10, wherein the photoluminescent material corresponds to at least one of a rylene or phosphor luminescent material.

### Claim 13 (depends on 10)

The method according to claim 10, wherein the solution comprises a percentage of photoluminescent material of approximately 0.001 to 15% by weight.

### Claim 14 (depends on 10)

The method according to claim 10, wherein the solution comprises a percentage of photoluminescent material of approximately 0.01 to 0.5% by weight.

### Claim 15 (depends on 10)

The method according to claim 10, wherein the solution further comprises at least one of a surfactant and an emulsifier.

### Claim 16 (depends on 10)

The method according to claim 10, wherein the surfactant comprises at least one of an anionic surfactant, an amphoteric surfactant, and a non-ionic surfactant.

### Claim 17 (depends on 10)

The method according to claim 10, wherein the surfactant comprises at least one of an unsaturated fatty acid, a polyphenol and a polyalkyl substituted phenol.

### Claim 18 (depends on 10)

The method according to claim 10, further comprising contacting the surface of the part with a second solution comprising at least one of a UV stabilizers, an optical brightener, an antistatic agent, a thermal stabilizer, IR absorbers, and antimicrobial agents.

### Claim 19

A method of depositing a photoluminescent material into a polymeric part comprising the steps of:
dissolving the photoluminescent material in liquid to create a solution;
controlling a temperature of the solution at a predetermined temperature;
submerging the surface in the solution for a predetermined time to infuse the surface with the photoluminescent material; and
rinsing the solution from the surface with rinse liquid wherein the predetermined time decreases in response to the predetermined temperature being increased.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the photoluminescent material corresponds to at least one of a rylene and phosphor luminescent material.