# US 2015/0147465 A1 · Non-Tracking Tack Coat

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147465 A1
- Document ID: US20150147465A1
- Status: Published application
- Kind: A1
- Application number: 14/550,221
- Filed: 2014-11-21
- Published: 2015-05-28
- Earliest claimed: 2013-11-22
- Assignees: Russell Standard Corp.
- Applicants: Russell Standard Corporation
- Inventors: Matthew Shaffer; Logan Norman
- Web page: https://patentgrep.com/patent/US20150147465A1

## CPC

- C09D 195/005: {Aqueous compositions, e.g. emulsions}
- C08L 33/04: Homopolymers or copolymers of esters {(C08L43/04 takes precedence)}
- C08L 35/06: Copolymers with vinyl aromatic monomers
- C09J 195/005: {Aqueous compositions, e.g. emulsions}
- E01C 7/185: {Isolating, separating or connecting intermediate layers, e.g. adhesive layers; Transmission of shearing force in horizontal intermediate planes, e.g. by protrusions (E01C7/187 takes precedence; adhesive layers for materials E01C7/35)}
- C08L 2555/80: Macromolecular constituents
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- E01C: CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE; MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR (forming roads or like surfaces by compacting or grading snow or ice E01H)

## Abstract

Provided herein is a tack coat for use with paving applications and a method of making the same. The tack coat is substantially non-tracking, and includes asphalt, a pH adjustor, an emulsifier, acrylic, and water. In certain embodiments, the tack coat may also include a stabilizer to prevent settling of the emulsion during storage. The method of producing the tack coat involves heating the asphalt in one tank, and heating the water and emulsifier in a second, separate tank. This mixture of the water and emulsifier is referred to as soap, and is then mixed with asphalt, and the acrylic may be added to the mixture immediately thereafter, with a stabilizer, or later, just prior to shipment of the product, in which case a stabilizer may not be required. The tack coat exhibits moderate softness, with a penetration value above 40 dmm.

## Claims

### Claim 1

An asphalt emulsion for bonding layers comprising asphalt, an acrylic, an emulsifier, and water, wherein the emulsion is configured to provide a hardened layer of acrylic superficial to the asphalt, emulsifier, and water when cured.

### Claim 2 (depends on 1)

The asphalt emulsion according to claim 1, wherein the asphalt has a penetration value of between about 45 dmm and about 55 dmm.

### Claim 3 (depends on 1)

The asphalt emulsion according to claim 1, wherein the asphalt is a mixture of at least two different asphalts forming a blended asphalt, each of the different asphalts having a different penetration value, wherein the blended asphalt has a penetration value between about 45 dmm and about 55 dmm.

### Claim 4 (depends on 1)

The asphalt emulsion according to claim 1, further comprising a pH adjustor, and wherein the pH adjustor is an acid.

### Claim 5 (depends on 4)

The asphalt emulsion according to claim 4, wherein the acid is hydrochloric acid.

### Claim 6 (depends on 1)

The asphalt emulsion according to claim 1, further comprising a pH adjustor, and wherein the pH adjustor is sodium hydroxide or potassium hydroxide.

### Claim 7 (depends on 1)

The asphalt emulsion according to claim 1, wherein the emulsion comprises, by weight, between about 40% and about 60% asphalt, between about 1% and about 10% acrylic, and between about 0.1% and about 3% emulsifier.

### Claim 8 (depends on 1)

The asphalt emulsion according to claim 1 wherein the emulsion comprises, by weight, between about 45% and about 55% asphalt, between about 1% and about 5% acrylic, and between about 0.5% and about 2% emulsifier.

### Claim 9 (depends on 1)

The asphalt emulsion according to claim 1, wherein the emulsion has a penetration value of about 40 to about 60 dmm when cured.

### Claim 10 (depends on 9)

The asphalt emulsion according to claim 9, wherein the emulsion has a penetration value of about 45 dmm to about 55 dmm when cured.

### Claim 11 (depends on 1)

The asphalt emulsion according to claim 1, wherein the emulsion is non-tracking.

### Claim 12

A method of producing a tack coat for bonding pavement layers comprising: combining an asphalt, an emulsifier, and water to form an asphalt emulsion; and
adding acrylic to the asphalt emulsion to form a non-tracking tack coat, wherein the tack coat is configured to provide a hardened layer of acrylic superficial to the asphalt, emulsifier, and water when the tack coat is dried.

### Claim 13 (depends on 12)

The method according to claim 12, further comprising heating the asphalt to a temperature of at least about 250 degrees Fahrenheit heating and the emulsifier and water to a temperature of at least about 75 degrees Fahrenheit.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the non-tracking tack coat comprises, by weight, between about 40% and about 60% asphalt, between about 1% and about 10% acrylic, between about 0.1% and about 3% emulsifier, and water up to 100%.

### Claim 15 (depends on 12)

The method according to claim 12, wherein the asphalt has a penetration value of between about 45 dmm and about 55 dmm.

### Claim 16 (depends on 12)

The method according to claim 12, wherein the asphalt is a mixture of at least two different asphalts forming a blended asphalt, each of the different asphalts having a different penetration value, wherein the blended asphalt has a penetration value between about 45 dmm and about 55 dmm.

### Claim 17 (depends on 12)

The method according to claim 12, further comprising a pH adjustor in the asphalt emulsion, wherein the pH adjustor is an acid.

### Claim 18 (depends on 12)

The method according to claim 12, further comprising a pH adjustor in the asphalt emulsion, wherein the pH adjustor is a base.

### Claim 19 (depends on 12)

The method according to claim 12, wherein the non-tracking tack coat has a penetration value of 40 to 60 dmm when cured.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the non-tracking tack coat has a penetration value of 45 to 55 dmm when cured.

### Claim 21

A method of bonding a layer of asphalt to a substrate layer comprising:
applying to the substrate layer a layer of a tack coat comprising asphalt, an acrylic, an emulsifier, and water, wherein the tack coat is configured to provide a hardened layer of acrylic superficial to the asphalt, emulsifier, and water of the tack coat upon application of the tack coat to the substrate layer and curing of the tack coat;
allowing the tack coat to cure;
hardening the acrylic thereby forming the hardened acrylic layer; and
applying a layer of heated asphalt to the tack coat layer, wherein the heated asphalt softens the tack coat layer and the softened tack coat layer forms a bond between the substrate layer and the asphalt layer.

### Claim 22 (depends on 21)

The method according to claim 21, wherein the tack coat has a penetration value of at least 40 dmm when cured.

### Claim 23 (depends on 21)

The method according to claim 21, wherein the tack coat is non-tracking.

### Claim 24

A method of providing a fog seal to a remediated surface, comprising applying to the surface a layer of a fog seal comprising asphalt, an acrylic, an emulsifier, and water, wherein the fog seal is configured to provide a hardened layer of acrylic superficial to the asphalt, emulsifier, and water of the fog seal upon application of the fog seal to the surface curing of the fog seal; and hardening the acrylic thereby forming the hardened layer of acrylic.