# US 2015/0147462 A1 · Resin composition, filler-containing resin film for non-aqueous electrolyte secondary battery, and method for producing filler-containing resin film for non-aqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147462 A1
- Document ID: US20150147462A1
- Status: Published application
- Kind: A1
- Application number: 14/409,014
- Filed: 2013-06-24
- Published: 2015-05-28
- Earliest claimed: 2012-06-28
- Assignees: Kureha Corporation
- Applicants: Kureha Corporation
- Inventors: Yusaku Inaba; Tamito Igarashi; Yuki Sakai; Aya Takeuchi
- Web page: https://patentgrep.com/patent/US20150147462A1

## CPC

- C09D 127/16: Homopolymers or copolymers of vinylidene fluoride
- C08K 3/22: of metals
- C09D 7/61: inorganic
- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 50/417: Polyolefins
- H01M 50/426: Fluorocarbon polymers
- H01M 50/434: Ceramics
- H01M 50/443: Particulate material
- H01M 50/446: Composite material consisting of a mixture of organic and inorganic materials
- H01M 50/451: comprising layers of only organic material and layers containing inorganic material
- H01M 50/457: comprising three or more layers
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- C08K 2003/2227: {of aluminium}
- H01M 10/052: Li-accumulators
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An object of the present invention is to provide a filler-containing resin film in which shedding of inorganic materials or the like is suppressed, a resin composition that can be used in production of the filler-containing resin film, and a method for producing the filler-containing resin film. The filler-containing resin film of the present invention is a filler-containing resin film comprising: a vinylidene fluoride copolymer obtained by copolymerizing vinylidene fluoride and a compound represented by formula (1) (in formula (1), R1, R2, and R3 are each independently hydrogen atoms, chlorine atoms, or alkyl groups having from 1 to 5 carbons; and X′ is an atomic group having a molecular weight of 472 or less and having a main chain configured from 1 to 19 atoms); and an insulating inorganic filler. The resin film is produced by applying onto a substrate and then drying a resin composition containing the vinylidene fluoride copolymer, the insulating inorganic filler, and an organic solvent.

## Claims

### Claim 1

A resin composition comprising: a vinylidene fluoride copolymer obtained by copolymerizing vinylidene fluoride and a compound represented by formula (1) below; an insulating inorganic filler; and an organic solvent:
wherein R1, R2, and R3 are each independently hydrogen atoms, chlorine atoms, or alkyl groups having from 1 to 5 carbons; and X′ is an atomic group having a molecular weight of 472 or less and having a main chain configured from 1 to 19 atoms.

### Claim 2 (depends on 1)

The resin composition according to claim 1, wherein the compound represented by formula (1) is a compound represented by formula (2) below:
wherein R1, R2, and R3 are each independently hydrogen atoms, chlorine atoms, or alkyl groups having from 1 to 5 carbons; and X′″ is an atomic group having a molecular weight of 456 or less and having a main chain configured from 1 to 18 atoms.

### Claim 3

A filler-containing resin film for a non-aqueous electrolyte secondary battery comprising: a vinylidene fluoride copolymer obtained by copolymerizing vinylidene fluoride and a compound represented by formula (1) below; and an insulating inorganic filler:
wherein R1, R2, and R3 are each independently hydrogen atoms, chlorine atoms, or alkyl groups having from 1 to 5 carbons; and X′ is an atomic group having a molecular weight of 472 or less and having a main chain configured from 1 to 19 atoms.

### Claim 4 (depends on 3)

The filler-containing resin film for a non-aqueous electrolyte secondary battery according to claim 3, wherein the compound represented by formula (1) is a compound represented by formula (2) below:
wherein R1, R2, and R3 are each independently hydrogen atoms, chlorine atoms, or alkyl groups having from 1 to 5 carbons; and X′″ is an atomic group having a molecular weight of 456 or less and having a main chain configured from 1 to 18 atoms.

### Claim 5

A method for producing a filler-containing resin film for a non-aqueous electrolyte secondary battery, the method comprising the steps of: applying a resin composition containing: a vinylidene fluoride copolymer obtained by copolymerizing vinylidene fluoride and a compound represented by formula (1) below, an insulating inorganic filler, and an organic solvent on a substrate; and drying the resin composition:
wherein R1, R2, and R3 are each independently hydrogen atoms, chlorine atoms, or alkyl groups having from 1 to 5 carbons; and X′ is an atomic group having a molecular weight of 472 or less and having a main chain configured from 1 to 19 atoms.

### Claim 6 (depends on 5)

The method for producing a filler-containing resin film for a non-aqueous electrolyte secondary battery according to claim 5, wherein the compound represented by formula (1) is a compound represented by formula (2) below:
wherein R1, R2, and R3 are each independently hydrogen atoms, chlorine atoms, or alkyl groups having from 1 to 5 carbons; and X′″ is an atomic group having a molecular weight of 456 or less and having a main chain configured from 1 to 18 atoms.

### Claim 7 (depends on 5)

The method for producing a filler-containing resin film for a non-aqueous electrolyte secondary battery according to claim 5, wherein the substrate is an electrode or a separator.