# US 2015/0147429 A1 · Mold for forming lens

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147429 A1
- Document ID: US20150147429A1
- Status: Published application
- Kind: A1
- Application number: 14/249,971
- Filed: 2014-04-10
- Published: 2015-05-28
- Earliest claimed: 2013-11-25
- Assignees: Samsung Electro-Mechanics Co., Ltd.
- Applicants: Samsung Electro-Mechanics Co., Ltd.
- Inventors: Yang Ho MOON; Ki Bok KWON; Yong Jin KIM
- Web page: https://patentgrep.com/patent/US20150147429A1

## CPC

- B29D 11/005: {having means for aligning the front and back moulds}
- B29K 2905/10: Copper
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

Embodiments of the invention provide a mold for forming a lens including a first core coupled with a first core hole of a first mold, and a second core coupled with a second core hole of a second mold to face the first core. In accordance with at least one embodiment, the first core and the second core are made of a material having a coefficient of thermal expansion larger than that of the first mold and the second mold, and outer diameters of the first core and the second core are each formed to be smaller than diameters of the first core hole and the second core hole.

## Claims

### Claim 1

A mold for forming a lens, the mold comprising:
a first core coupled with a first core hole of a first mold; and
a second core coupled with a second core hole of a second mold to face the first core,
wherein the first core and the second core are each made of a material having a coefficient of thermal expansion larger than that of the first mold and the second mold, and
wherein outer diameters of the first core and the second core are each formed to be smaller than diameters of the first core hole and the second core hole.

### Claim 2 (depends on 1)

The mold as set forth in claim 1, wherein the outer diameters of the first core and the second core are each formed to be 1 to 2 μm smaller than diameters of the first core hole and the second core hole.

### Claim 3 (depends on 1)

The mold as set forth in claim 1, wherein, when an expansion of the first core is ΔP1 and an expansion of the first core hole is ΔH1, a conditional equation of 2 μm<ΔP1−ΔH1 is satisfied.

### Claim 4 (depends on 1)

The mold as set forth in claim 1, wherein, when an expansion of the second core is ΔP2 and an expansion of the second core hole is ΔH2, a conditional equation of 2 μm<ΔP2−ΔH2 is satisfied.

### Claim 5 (depends on 1)

The mold as set forth in claim 1, wherein the first core or the second core is made of a material having a coefficient of thermal expansion of 17×10−6 or more.

### Claim 6 (depends on 1)

The mold as set forth in claim 1, wherein, when the coefficient of thermal expansion of the first core is α1 and the coefficient of thermal expansion of the first mold is β1, a conditional equation of 5×10−6<α1−β1<10×10−6 is satisfied.

### Claim 7 (depends on 1)

The mold as set forth in claim 1, wherein, when the coefficient of thermal expansion of the second core is α2 and the coefficient of thermal expansion of the second mold is β2, a conditional equation of 5×10−6<α2−β2<10×10−6 is satisfied.

### Claim 8 (depends on 1)

The mold as set forth in claim 1, wherein the first core and the second core are made of a material having heat conductivity of 50 W/m ° C. or more.

### Claim 9 (depends on 1)

The mold as set forth in claim 1, wherein the first core and the second core are made of a moldmax material.

### Claim 10 (depends on 1)

The mold as set forth in claim 1, wherein outer surfaces of the first core and the second core are plated with nickel (Ni).

### Claim 11

A mold for forming a lens, the mold comprising:
a first mold formed with a first core hole;
a second mold disposed in a direction in which the second mold faces the first mold and formed with a second core hole;
a first core coupled with the first core hole of the first mold; and
a second core coupled with the second core hole of the second mold to face the first core,
wherein the first core and the second core are made of a material having heat conductivity of 50 W/m ° C. or more.

### Claim 12 (depends on 11)

The mold as set forth in claim 11, wherein the first core and the second core are each made of a material having a coefficient of thermal expansion larger than that of the first mold and the second mold, and
an outer diameter of the first core and the second core is formed to be smaller than a diameter of the first core hole and the second core hole.

### Claim 13 (depends on 12)

The mold as set forth in claim 12, wherein the outer diameters of the first core and the second core are each formed to be 1 to 2 μm smaller than diameters of the first core hole and the second core hole.

### Claim 14 (depends on 11)

The mold as set forth in claim 11, wherein, when an expansion of the first core is ΔP1 and an expansion of the first core hole is ΔH1, a conditional equation of 2 μm<ΔP1−ΔH1 is satisfied.

### Claim 15 (depends on 11)

The mold as set forth in claim 11, wherein, when an expansion of the second core is ΔP2 and an expansion of the second core hole is ΔH2, a conditional equation of 2 μm<ΔP2−ΔH2 is satisfied.

### Claim 16 (depends on 11)

The mold as set forth in claim 11, wherein the first core and the second core are made of a material having a coefficient of thermal expansion of 17×10−6 or more.

### Claim 17 (depends on 11)

The mold as set forth in claim 11, wherein, when the coefficient of thermal expansion of the first core is α1 and the coefficient of thermal expansion of the first mold is β1, a conditional equation of 5×10−6<α1−β1<10−10−6 is satisfied.

### Claim 18 (depends on 11)

The mold as set forth in claim 11, wherein when the coefficient of thermal expansion of the second core is α2 and the coefficient of thermal expansion of the second mold is β2, a conditional equation of 5×10−6<α2−β2<10×10−6 is satisfied.

### Claim 19 (depends on 11)

The mold as set forth in claim 11, wherein the first core and the second core are made of a moldmax material.

### Claim 20 (depends on 11)

The mold as set forth in claim 11, wherein outer surfaces of the first core and the second core are plated with nickel (Ni).