# US 2015/0147269 A1 · Metal silicoaluminophosphate molecular sieve with rho framework structure, and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0147269 A1
- Document ID: US20150147269A1
- Status: Published application
- Kind: A1
- Application number: 14/405,957
- Filed: 2012-06-08
- Published: 2015-05-28
- Earliest claimed: 2012-06-08
- Assignees: Dalian Institute of Chemical Physics, Chinese Academy of Sciences
- Inventors: Peng Tian; Xiong Su; Zhongmin Liu; Dong Fan; Ying Zhang; Yue Yang
- Web page: https://patentgrep.com/patent/US20150147269A1

## CPC

- C01B 39/54: Phosphates, e.g. APO or SAPO compounds
- B01J 20/18: Synthetic zeolitic molecular sieves
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- B01J 29/85: Silicoaluminophosphates [SAPO compounds]
- B01J 37/082: {Decomposition and pyrolysis}
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

The present invention relates to a metal silicoaluminophosphate molecular sieve MeAPSO with a RHO framework structure and a preparation method thereof. The metal silicoaluminophosphate molecular sieve is characterized in that: the metal atoms are at least one of vanadium, copper, molybdenum, zirconium, cobalt, manganese, magnesium, iron, nickel and zinc. The chemical composition of said metal silicoaluminophosphate molecular sieve in anhydrous state is expressed as: mR.nMe.(SixAlyPz)O2, where R represents template existed in molecular sieve micropores, m is the molar number of said template per one molar of (SixAlyPz)O2, m=0.1˜0.5; Me represents metal atom entering into said metal silicoaluminophosphate molecular sieve framework, n is the molar number of Me per one molar of (SixAlyPz)O2, n=0.001˜0.30. Said metal silicoaluminophosphate molecular sieve has ion exchange performance and adsorption performance. The catalyst prepared from said metal silicoaluminophosphate molecular sieve can be applicable to multiple hydrocarbon reactions, such as catalytic cracking, reforming, polymerization, alkylation, transalkylation, isomerization, dehydrogenation, hydrogenation and the like.

## Claims

### Claim 1

A metal silicoaluminophosphate molecular sieve with RHO framework structure whose chemical composition in the anhydrous state is expressed as:
mR.nMe.(SixAlyPz)O2,
where,
R represents template existing in micropores of said metal silicoaluminophosphate molecular sieve;
m is the molar number of said template per one mole of (SixAlyPz)O2, m=0.1˜0.5;
Me represents metal atom entering into said metal silicoaluminophosphate molecular sieve framework, n is the molar number of Me per one molar of (SixAlyPz)O2, n=0.001˜0.30;
x, y, z respectively represents the molar number of Si, Al, P, wherein x=0.01˜0.60, y=0.2˜0.60, z=0.2˜0.60, and x+y+z=1.

### Claim 2 (depends on 1)

A metal silicoaluminophosphate molecular sieve according to claim 1, characterized in that said template R is diethylamine, a mixture of diethylamine and triethylamine, a mixture of diethylamine and morpholine or a mixture of diethylamine and tetraethylammonium hydroxide.

### Claim 3 (depends on 1)

A metal silicoaluminophosphate molecular sieve according to claim 1, characterized in that said template R is a mixture of diethylamine and triethylamine, a mixture of diethylamine and morpholine or a mixture of diethylamine and tetraethyl ammonium hydroxide; wherein the molar ratio of said diethylamine in the mixture is more than 70%.

### Claim 4 (depends on 1)

A metal silicoaluminophosphate molecular sieve according to claim 1, characterized in that said metal atom Me entering into said metal silicoaluminophosphate molecular sieve framework is one or more metal atoms selected from the group consisting of vanadium, copper, molybdenum, zirconium, cobalt, manganese, magnesium, iron, nickel and zinc; and preferably said metal atom Me is one or more metal atoms selected from the group consisting of copper, cobalt, manganese, magnesium, iron, nickel and zinc; and further preferably said metal atom Me is one or more metal atoms selected from the group consisting of copper, cobalt, manganese, magnesium and zinc.

### Claim 5 (depends on 1)

A method for preparing said metal silicoaluminophosphate molecular sieve according to claim 1, including the steps as following:
(1) a metal source, a silicon source, an aluminum source, a phosphorus source, a surfactant, a template and deionized water are mixed homogeneously by stirring, and an initial gel mixture with following molar ratio is obtained:
Me/Al2O3=0.01˜1.0;
SiO2/Al2O3=0.01˜2.0;
P2O5/Al2O3=0.5˜2.0;
H2O/Al2O3=21˜200;
S/Al2O3=0.01˜0.5; S represents at least one surfactant;
R/Al2O3=0.5˜5.5; R is diethylamine, a mixture of diethylamine and triethylamine, a mixture of diethylamine and morpholine or a mixture of diethylamine and tetraethylammonium hydroxide;
(2) said initial gel mixture is transferred into a synthetic kettle, then sealed and heated to crystallization temperature, and crystallized in the rotating conditions; wherein the crystallization temperature is 155˜230° C., and the crystallization time is 1˜72 h;
(3) after finishing the crystallization, the solid crystal product is washed and dried to obtain said metal silicoaluminophosphate molecular sieve with RHO framework structure.

### Claim 6 (depends on 5)

A method according to claim 5, characterized in that said silicon source is one or more silicon sources selected from the group consisting of silica sol, silica gel, active silica, and orthosilicates;
said aluminum source is one or more aluminum sources selected from the group consisting of aluminum salts, activated alumina, aluminum alkoxide and pseudoboehmite;
said phosphorus source is one or more phosphorus sources selected from the group consisting of phosphoric acid, phosphate, organophosphorous compounds, and phosphorus oxides;
said surfactant is one or more surfactants selected from the group consisting of dodecyl trimethyl ammonium chloride, dodecyl trimethyl ammonium bromide, tridecyl trimethyl ammonium chloride, tridecyl trimethyl ammonium bromide, tetradecyl trimethyl ammonium chloride, tetradecyl trimethyl ammonium bromide, pentadecyl trimethyl ammonium chloride, pentadecyl trimethyl ammonium bromide, hexadecyl trimethyl ammonium bromide, hexadecyl trimethyl ammonium chloride, dimethylhexadecyl[3-trimethylsilylpropyl]ammonium chloride, dimethyloctadecyl[3-trimethylsilylpropyl]ammonium chloride and hexadecyl(trimethoxy)silane.

### Claim 7 (depends on 5)

A method according to claim 5, characterized in that said metal source is one or more metal sources selected from the group consisting of oxides, inorganic salts and organic salts of vanadium, copper, molybdenum, zirconium, cobalt, manganese, magnesium, iron, nickel or zinc; and preferably said metal source is one or more metal sources selected from the group consisting of oxides, inorganic salts and organic salts of copper, cobalt, manganese, magnesium, iron, nickel or zinc; and further preferably said metal source is one or more metal sources selected from the group consisting of oxides, inorganic salts and organic salts of copper, cobalt, manganese, magnesium or zinc.

### Claim 8 (depends on 5)

A method according to claim 5, characterized in that the molar ratio of Me to Al2O3 in the step (1) is 0.01˜0.5, and preferably the molar ratio of Me to Al2O3 in the step (1) is 0.01˜0.35.

### Claim 9 (depends on 5)

A method according to claim 5, characterized in that the molar ratio of S to Al2O3 in the step (1) is 0.05˜0.35.

### Claim 10 (depends on 5)

A method according to claim 5, characterized in that the molar ratio of R to Al2O3 in the step (1) is 1.0˜4.0.

### Claim 11 (depends on 5)

A method according to claim 5, characterized in that R in the step (1) is a mixture of diethylamine and triethylamine, a mixture of diethylamine and morpholine or a mixture of diethylamine and tetraethyl ammonium hydroxide; wherein, the molar ratio of said diethylamine in the mixture is more than 70%.

### Claim 12 (depends on 5)

A method according to claim 5, characterized in that in the step (1), said initial gel mixture is obtained as the following steps of: mixing 2/3 of said deionized water with phosphoric acid; adding said metal source and stirring to mix homogeneously; adding aluminum source and stirring to mix homogeneously; adding said silicon source; adding the solution of said surfactant in the rest 1/3 of said deionized water and stirring for at least 1 h; adding organic amine template and stirring for at least 1 hour to obtain said initial gel mixture.

### Claim 13 (depends on 5)

A method according to claim 5, characterized in that the crystallization temperature in step (2) is 170˜215° C., and the crystallization time is 2˜48 hours.

### Claim 14 (depends on 1)

A catalyst for acid-catalyzed reaction, which is obtained by calcining at least one of said metal silicoaluminophosphate molecular sieves according to claim 1 at 400˜700° C. in the air.

### Claim 15 (depends on 1)

A gas absorbent, which is obtained by calcining at least one of said metal silicoaluminophosphate molecular sieves according to claim 1 at 400˜700° C. in the air.

### Claim 16 (depends on 1)

A catalyst for selective oxidation reaction, which is obtained by calcining at least one of said metal silicoaluminophosphate molecular sieves according to claim 1 at 400˜700° C. in the air.